scholarly journals Supplementation with 45S5 Bioactive Glass Reduces In Vivo Resorption of the β-Tricalcium-Phosphate-Based Bone Substitute Material Vitoss

2019 ◽  
Vol 20 (17) ◽  
pp. 4253 ◽  
Author(s):  
Fabian Westhauser ◽  
Christopher Essers ◽  
Maria Karadjian ◽  
Bruno Reible ◽  
Gerhard Schmidmaier ◽  
...  

Compared to other materials such as 45S5 bioactive glass (BG), β-tricalcium phosphate (β-TCP)-based bone substitutes such as Vitoss show limited material-driven stimulation of osteogenesis and/or angiogenesis. The unfavorable degradation kinetics of β-TCP-based bone substitutes may result in an imbalance between resorption and osseous regeneration. Composite materials like Vitoss BA (Vitoss supplemented with 20 wt % 45S5-BG particles) might help to overcome these limitations. However, the influence of BG particles in Vitoss BA compared to unsupplemented Vitoss on osteogenesis, resorption behavior, and angiogenesis is not yet described. In this study, Vitoss and Vitoss BA scaffolds were seeded with human mesenchymal stromal cells before subcutaneous implantation in immunodeficient mice for 10 weeks. Scaffold resorption was monitored by micro-computed tomography, while osteoid formation and vascularization were assessed by histomorphometry and gene expression analysis. Whilst slightly more osteoid and improved angiogenesis were found in Vitoss BA, maturation of the osteoid was more advanced in Vitoss scaffolds. The volume of Vitoss implants decreased significantly, combined with a significantly increased presence of resorbing cells, whilst the volume remained stable in Vitoss BA scaffolds. Future studies should evaluate the interaction of 45S5-BG with resorbing cells and bone precursor cells in greater detail to improve the understanding and application of β-TCP/45S5-BG composite bone substitute materials.

2015 ◽  
Vol 27 (03) ◽  
pp. 1550028 ◽  
Author(s):  
Kam-Kong Chan ◽  
Chia-Hsien Chen ◽  
Lien-Chen Wu ◽  
Yi-Jie Kuo ◽  
Chun-Jen Liao ◽  
...  

Calcium phosphate ceramics, of a similar composition to that of mineral bone, and which possess the properties of bioactivity and osteoconductivity, have been widely used as substitutes for bone graft in orthopedic, plastic and craniofacial surgeries. A synthetic β-tricalcium phosphate, Osteocera™, a recently developed bone graft substitute, has been used in this study. To evaluate the affinity and efficacy of Osteocera™ as bone defect implant, we used a New Zealand white rabbit femur defect model to test the osteoconductivity of this new bone substitute. Alternative commercially available bone substitutes, Triosite® and ProOsteon500, were used as the control materials. These three bone substitutes show good biocompatibility, and no abnormal inflammation either infection was seen at the implantation sites. In the histological and histomorphometric images, newly formed bone grew into the peripheral pores in the bone substitutes. After six months implantation, the volume of bone formation was found to be 20.5 ± 5.2%, 29.8 ± 6.5% and 75.5 ± 4.9% of the potential total cavity offered by ProOsteon500, Triosite® and Osteocera™, respectively. The newly formed bone area within the femur defect section for Osteocera™ was significantly larger than ProOsteon500 and Triosite®. We concluded that Osteocera™ shows better bioresorbability, biocompatibility and osteoconductivity in the rabbit femur defect model.


2018 ◽  
Vol 69 (2) ◽  
pp. 429-433
Author(s):  
Solyom Arpad ◽  
Cristian Trambitas ◽  
Ecaterina Matei ◽  
Eugeniu Vasile ◽  
Fodor Pal ◽  
...  

Osteoplasty, is a procedure mostly applied in complicated bone fractures. Nowadays this method is widely used in primary fracture treatment while the native bone graft is progressively replaced with various synthetic bone substitutes. From the numerous bone grafts we�d like to mention a representative of ceramics, the S53P4 bioactive glass. (BonAlive�). The aim of this study was to investigate the healing process of different fracture types generated on rabbit femurs. During this experiment we used seven common European rabbits. We separated these animals into two groups; in the first group we surgically generated a total fracture in the middle 1/3 of the femur, while in the second group, we produced only a bone defect on the femur. The osteoplasty was carried out with bioactive glass and autologous bone grafts. The radiographic follow-up was immediate after the operation and after 3, 6 and 7 weeks. The animals were euthanized after 19, 20 and 21 weeks, for histomorphometric examination of the femur. It was also studied the ionic release from the used bioactive glass at physiological pH and the etching of the glass was studied by Scanning Electron Microscopy.


2020 ◽  
Author(s):  
Isabel Pereira ◽  
José Eduardo Pereira ◽  
Luís Maltez ◽  
Alexandra Rodrigues ◽  
Catarina Rodrigues ◽  
...  

Abstract The development of injectable bone substitutes (IBS) have obtained great importance in the bone regeneration field, as a strategy to reach hardly accessible defects using minimally invasive techniques and able to fit to irregular topographies. In this scenario, the association of injectable hydrogels and bone graft granules is emerging as a well-established trend. Particularly, in situ forming hydrogels have arisen as a new IBS generation. An in situ forming and injectable dextrin-based hydrogel (HG) was developed, aiming to act as a carrier of granular bone substitutes and bioactive agents. In this work, the HG was associated to a granular bone substitute (Bonelike®) and implanted in goat critical-sized calvarial defects (14 mm) for 3, 6 and 12 weeks. The results showed that HG improved the handling properties of the Bonelike® granules and did not affect its osteoconductive features, neither impairing the bone regeneration process. Human multipotent mesenchymal stromal cells from the umbilical cord, extracellular matrix hydrolysates and the pro-angiogenic peptide LLKKK18 were also combined with the IBS. These bioactive agents did not enhance the new bone formation significantly under the conditions tested, according to micro-computed tomography and histological analysis.


Materials ◽  
2021 ◽  
Vol 14 (4) ◽  
pp. 946
Author(s):  
Katharina Kowalewicz ◽  
Elke Vorndran ◽  
Franziska Feichtner ◽  
Anja-Christina Waselau ◽  
Manuel Brueckner ◽  
...  

Calcium magnesium phosphate cements (CMPCs) are promising bone substitutes and experience great interest in research. Therefore, in-vivo degradation behavior, osseointegration and biocompatibility of three-dimensional (3D) powder-printed CMPC scaffolds were investigated in the present study. The materials Mg225 (Ca0.75Mg2.25(PO4)2) and Mg225d (Mg225 treated with diammonium hydrogen phosphate (DAHP)) were implanted as cylindrical scaffolds (h = 5 mm, Ø = 3.8 mm) in both lateral femoral condyles in rabbits and compared with tricalcium phosphate (TCP). Treatment with DAHP results in the precipitation of struvite, thus reducing pore size and overall porosity and increasing pressure stability. Over 6 weeks, the scaffolds were evaluated clinically, radiologically, with Micro-Computed Tomography (µCT) and histological examinations. All scaffolds showed excellent biocompatibility. X-ray and in-vivo µCT examinations showed a volume decrease and increasing osseointegration over time. Structure loss and volume decrease were most evident in Mg225. Histologically, all scaffolds degraded centripetally and were completely traversed by new bone, in which the remaining scaffold material was embedded. While after 6 weeks, Mg225d and TCP were still visible as a network, only individual particles of Mg225 were present. Based on these results, Mg225 and Mg225d appear to be promising bone substitutes for various loading situations that should be investigated further.


2016 ◽  
Vol 721 ◽  
pp. 229-233 ◽  
Author(s):  
Sandris Petronis ◽  
Janis Locs ◽  
Vita Zalite ◽  
Mara Pilmane ◽  
Andrejs Skagers ◽  
...  

Calcium bone substitutes are successfully used for local recovery of osteoporotic bone and filling of bone defects. Previous studies revieled that biphasic calcium phosphate (BCP) show better bioactivity in compare to pure β-tricalcium phosphate or hydroxyapatite. Also increased porosity of material promotes better bone tissue response. Aim of this experiment was to evaluate immunohistologically response of osteoporotic bone of experimental animal to implantation of granules with hydroxyapatite/β-tricalcium phosphate (HAp/β-TCP) ratio of 90/10. Calcium phosphate (CaP) was synthesized by aqueous precipitation technique from calcium hydroxide and phosphoric acid. Bioceramic granules in size range from 1.0 to 1.4 mm were prepared with nanopore sizes around 200 nm. We used nine female rabbits with induced osteoporosis in this experiment. Six animals in study group underwent implantation of BCP in hip bone defect and three animals in control group left without BCP implantation. After 6 months animals were euthanized, bone samples collected and proceeded for detection of bone activity and repair markers: osteocalcin (OC), osteopontin (OP) and osteoprotegerin (OPG). Controls showed the presence of experimental bone osteoporosis. In experimental group bone showed partially resorbed bioceramic granules and in some samples new bone formation near the granuli was observed. Increase of OC and OPG up to twice as to compare to control group were detected as well. Implantation of BCP granules in osteoporotic rabbit bone increases expression of OC and OPG indicating the activation of osteoblastogenesis and bone mineralization in vivo.


2005 ◽  
Vol 284-286 ◽  
pp. 281-284 ◽  
Author(s):  
Masanobu Kamitakahara ◽  
Chikara Ohtsuki ◽  
M. Oishi ◽  
Shinichi Ogata ◽  
Toshiki Miyazaki ◽  
...  

Biphasic ceramic consisting of tricalcium phosphate with α- and β -phases (αβ-TCP) is a candidate as biodegradable bone substitutes since its biodegradability may be controlled by the ratio of the phases. In the present study, preparation of porous αβ-TCP body with continuous pores of 10-50 µm in diameter was attempted using additives of Mg, and its in vivo behavior was examined. Powder of β-TCP was mixed with Mg and potato starch to form slurry, followed by loading in polyurethane foam. The sample was fired at 1400°C for 12 hours for sintering process. α-TCP content of the sample decreased with increasing the Mg content, while β-TCP increased. Ceramic body consisting of β-TCP phase was obtained when 1.0 mass% of Mg was added. Porosity of the body decreased with increasing the content of Mg. The αβ-TCP body with 80% porosity was obtained when the content of Mg was 0.1 mass%. The in vivo experiments showed that the rate of degradation of the obtained αβ-TCP was almost same as α-TCP, and much higher than β-TCP.


2013 ◽  
Vol 541 ◽  
pp. 97-113 ◽  
Author(s):  
Rossella Bedini ◽  
Deborah Meleo ◽  
Raffaella Pecci

After a short introduction to bone substitute biomaterials and X-ray microtomography, this article describes a research work carried out for in-vitro characterization of bone substitute biomaterials as well as for in-vivo investigation of human bone grafted with biomaterials. Three different bone substitute biomaterials have been analyzed in-vitro by means of 3D microtomographic technique, while human bone samples grafted with bone substitute biomaterials are investigated by 3D microtomography and histological techniques. 3D images of bone substitutes and human bone samples with biomaterials have been obtained, together with morphometric parameters, by microtomography . 2D histological images have also been obtained by traditional technique only for human bone samples with biomaterials. Compared to traditional histological analysis, 3D microtomography shows better results for investigating bone tissue and bone substitute biomaterial, and in a short time. Nevertheless, histological analysis remains the best technique for the observation of soft tissue and blood vessels.