scholarly journals Experimental Study on the Mechanical Properties of Amorphous Alloy Fiber-Reinforced Concrete

2018 ◽  
Vol 2018 ◽  
pp. 1-9 ◽  
Author(s):  
Chaohua Jiang ◽  
Yizhi Wang ◽  
Wenwen Guo ◽  
Chen Jin ◽  
Min Wei

With great mechanical properties and corrosion resistance, amorphous alloy fiber (AAF) is a highly anticipated material in the fiber-reinforced concrete (FRC) field. In this study, the mechanical properties of AAFRC such as compressive strength, tensile strength, and flexural strength were examined. The comparison and analysis between AAFRC and steel fiber-reinforced concrete (SFRC) were also carried out. The results show that adding fibers significantly improves the concrete strength and toughness index. Compared with plain concrete, the compressive strength, splitting tensile strength, and flexural strength of AAFRC increase by 8.21–16.72%, 10.4–32.8%, and 18.12–45.21%, respectively. Meanwhile, the addition of AAF with a greater tensile strength and larger unit volume quantity improves the splitting tensile strength and flexural strength of concrete more noticeably than that of SF. Adding AAF improves the ductility of concrete more significantly in comparison to the SF. AAFRC shows great interfacial bonding performance as well. A prediction equation for the strength of AAFRC was proposed, which verified good accuracy calibrated based on the test results.

2018 ◽  
Vol 80 (5) ◽  
Author(s):  
Agustinus Agus Setiawan ◽  
Fredy Jhon Philip ◽  
Eka Permanasari

The objective of this research is to determine the mechanical properties of the waste-plastic-banner-fiber reinforced concrete: compressive strength, splitting tensile strength, rupture modulus and modulus of elasticity. Concrete mixtures with different proportions of waste plastic banner fiber were produced and tested: 0%, 0.25%, 0.5%, 1.0%, 2.0% of waste plastic banner fiber. The tests showed that the addition of fiber by 0.5% from the total concrete volume will increase the splitting tensile strength by 14.28% and produce the modulus of elasticity as high as 23,025 MPa (up to 12% from the normal mix)  and yield the concrete compressive strength of 35.56 MPa (up to 4.95% of the normal mixture). The rupture modulus will increase by 4.11% as the addition of 0.25% of waste plastic banner fiber. 


2020 ◽  
Vol 14 (2) ◽  
pp. 6734-6742
Author(s):  
A. Syamsir ◽  
S. M. Mubin ◽  
N. M. Nor ◽  
V. Anggraini ◽  
S. Nagappan ◽  
...  

This study investigated the combine effect of 0.2 % drink cans and steel fibers with volume fractions of 0%, 0.5%, 1%, 1.5%, 2%, 2.5% and 3% to the mechanical properties and impact resistance of concrete. Hooked-end steel fiber with 30 mm and 0.75 mm length and diameter, respectively was selected for this study.  The drinks cans fiber were twisted manually in order to increase friction between fiber and concrete. The results of the experiment showed that the combination of steel fibers and drink cans fibers improved the strength performance of concrete, especially the compressive strength, flexural strength and indirect tensile strength. The results of the experiment showed that the combination of steel fibers and drink cans fibers improved the compressive strength, flexural strength and indirect tensile strength by 2.3, 7, and 2 times as compare to batch 1, respectively. Moreover, the impact resistance of fiber reinforced concrete has increase by 7 times as compared to non-fiber concretes. Moreover, the impact resistance of fiber reinforced concrete consistently gave better results as compared to non-fiber concretes. The fiber reinforced concrete turned more ductile as the dosage of fibers was increased and ductility started to decrease slightly after optimum fiber dosage was reached. It was found that concrete with combination of 2% steel and 0.2% drink cans fibers showed the highest compressive, split tensile, flexural as well as impact strength.    


2021 ◽  
Vol 11 (17) ◽  
pp. 7926
Author(s):  
Qian Zhang ◽  
Wenqing Zhang ◽  
Yu Fang ◽  
Yongjie Xu ◽  
Xianwen Huang

In order to solve the problem of highly brittle shaft lining under dynamic loading, a combination of hybrid fiber concrete mixed with steel and polypropylene fiber is proposed to make shaft lining. C60, the concrete commonly used in shaft lining, was selected as the reference group. The static mechanical properties, dynamic mechanical properties, and crack failure characteristics of the hybrid fiber concrete were experimentally studied. The test results showed that compared to the reference group concrete, the compressive strength of the hybrid fiber-reinforced concrete did not significantly increase, but the splitting tensile strength increased by 60.4%. The split Hopkinson compression bar results showed that the optimal group peak stress and peak strain of the hybrid fiber concrete increased by 58.2% and 79.2%, respectively, and the dynamic toughness increased by 68.1%. The strain distribution before visible cracks was analyzed by the DIC technology. The results showed that the strain dispersion phenomenon of the fiber-reinforced concrete specimen was stronger than that of the reference group concrete. By comparing the crack failure forms of the specimens, it was found that compared to the reference group concrete, the fiber-reinforced concrete specimens showed the characteristics of continuous and slow ductile failure. The above results suggest that HFRC has significantly high dynamic splitting tensile strength and compressive deformation capacity, as well as a certain anti-disturbance effect. It is an excellent construction material for deep mines under complex working conditions.


2009 ◽  
Vol 610-613 ◽  
pp. 69-75
Author(s):  
Yuan Hua ◽  
Tai Quan Zhou

Different kinds of fiber are used to reinforce the concrete to improve the concrete mechanical properties. The high modulus and high flexibility fibers are often used to reinforce in the cement base, which leads to the higher performance compound cement based materials. In the paper, the carbon fiber and glass fiber material are used as flexibility reinforced materials. The polypropylene fiber and the polyethylene fiber are used as strength reinforced materials. The combinations of the flexibility reinforced fiber and strength reinforced fiber are chosen as C-P HF (Carbon and Polypropylene Hybrid Fiber) and G-Pe HF (Glass and Polyethylene Hybrid Fiber). The concrete mixture ratio and the fiber-reinforced amount are determined to the author’s previous study. The relationship between compressive strength, flexural strength and length/diameter aspect ratio of fiber for the carbon and polypropylene hybrid fiber reinforced concrete (C-P HFRC), and for the glass and polyethylene hybrid fiber reinforced concrete (G--Pe HFRC) was tested and discussed. The testing results show that length/diameter aspect ratio of fiber obviously affects the flexural strength of C-P HFRC and G-Pe HFRC, though the compressive strength is slightly affected by the length-diameter aspect ratio.


2018 ◽  
Vol 875 ◽  
pp. 174-178
Author(s):  
Bhawat Chaichannawatik ◽  
Athasit Sirisonthi ◽  
Qudeer Hussain ◽  
Panuwat Joyklad

This study presents results of an experimental investigation conducted to investigate the mechanical properties of sisal and glass fiber reinforced concrete. Four basic concrete mixes were considered: 1) Plain concrete (PC) containing ordinary natural aggregates without any fibers, 2) sisal fiber reinforced concrete (SFRC), 3) sisal and glass fiber reinforced concrete (SGFRC), 4, glass fiber reinforced concrete (GFRC). Investigated properties were compressive strength, splitting tensile strength, flexural tensile strength and workability. The results of fiber reinforced concrete mixes were compared with plain concrete to investigate the effect of fibers on the mechanical properties of fiber reinforced concrete. It was determined that addition of different kinds of fibers (natural and synthetic) is very useful to produce concrete. The addition of fibers was resulted into higher compressive strength, splitting and tensile strength. However, the workability of the fiber reinforced concrete was found lower than the plain concrete due to the addition of fibers in the concrete.


2018 ◽  
Vol 12 (1) ◽  
pp. 368-382 ◽  
Author(s):  
Abass Abayomi Okeola ◽  
Silvester Ochieng Abuodha ◽  
John Mwero

Introduction: Fiber reinforced concrete is becoming popular in improving the quasi-brittle failure of concrete. Natural fibers such as sisal holds great promise in this regard. It has amazing tensile strength and is renewable. This paper presents the result of an investigation carried out on the effect of sisal fiber on the compressive strength, Split tensile strength, failure mode and Poisson ratio of Sisal Fiber-Reinforced Concrete (SFRC). Methods: A mix proportion of 1:1.92:3.68 and w/c ratio of 0.47 for a target compressive strength of 35 MPa was used. Sisal fiber was added at percentages of 0.5%, 1.0%, 1.5%, and 2.0% by weight of cement. The effect of specimen shape on the compressive strength of sisal fiber-reinforced concrete (SFRC) was reported. The compressive strength of cube (150mm X 150mm) and cylinder (150mm diameter and 300mm height) specimen was determined at 7 and 28 days, while Split tensile strength and Poisson ratio were obtained using cylindrical specimen (150mm diameter and 300mm height). Results and Conclusion: The result shows that the addition of sisal fiber slightly reduces the compressive strength of concrete, increases its split tensile strength up to 47.167% of the control specimen, arrests crack propagation and reduces its Poisson ratio. The correlation between the compressive strength of cylindrical and cube specimen was established with a ratio ranging between 0.82 - 0.73. The difference in the compressive strength was found to increase with rise in the percentages of sisal fiber. Based on the ratio and mechanical properties, 1.0% sisal fiber content was recommended as the optimum for reinforcing concrete.


2021 ◽  
Vol 16 (4) ◽  
pp. 169-176
Author(s):  
Xiaohu Luo

In order to improve the application effect of steel fiber reinforced concrete (SFRC) in road bridge construction, the mechanical properties of SFRC with different fiber content were analyzed. The SFRC specimens with 0%, 0.5%, 1%, 1.5% and 2% fiber content were designed, and the mechanical properties were tested. The results showed that the compressive strength first increased and then decreased with the increase of fiber content, and the maximum compressive strength of SFRC1.5 reached 40.86 MPa, increasing by 7.19%; the increase amplitude of tensile strength of SFRC1.5 was 73.04%, which was the most obvious; the flexural strength of SFRC increased with the increase of fiber content, and the flexural strength of SFRC2 was 9.78 MPa, increasing by 94.43%. It is concluded from the experimental results of a case study that SFRC1.5 presents the optimal overall mechanical properties and is more suitable for road bridge construction.


2012 ◽  
Vol 174-177 ◽  
pp. 1219-1222 ◽  
Author(s):  
Xin Zhang ◽  
Jian Yun Pan ◽  
Bo Yang

A series of experiments are carried out to investigate the mechanical performance of bamboo fiber reinforced concrete, including the cubic compressive strength and splitting tensile strength. The experimental results show that bamboo fibers can enhance the cubic compressive strength and remarkably improve the splitting tensile strength of concrete. In addition, the effects of various bamboo fiber content and length on cubic compressive strength and splitting strength are also discussed respectively.


2014 ◽  
Vol 2014 ◽  
pp. 1-14 ◽  
Author(s):  
Tehmina Ayub ◽  
Nasir Shafiq ◽  
M. Fadhil Nuruddin

This paper presents the mechanical properties and the microstructure of the high performance fiber reinforced concrete (HPFRC) containing up to 3% volume fraction of chopped Basalt fibers. Three types of the concrete were prepared, out of which, the first type was prepared by utilizing 100% cement content. The other two types of the concrete were prepared by replacing 10% cement content with silica fume and the locally produced metakaolin. Using each concrete type, four mixes were prepared in which Basalt fibers were added in the range of 0–3%; that is, total twelve mixes of the HPFRC concrete were prepared. From each of the twelve concrete mixes, total twelve specimens were cast to determine the mechanical properties of the HPFRC including compressive strength (cube and cylinder), splitting tensile strength, and the flexural strength. In this way, a total of 108 specimens were cast and tested in this study. Test results showed that the addition of the Basalt fibers significantly increased the tensile splitting strength and the flexural strength of the HPFRC, while there was slight improvement in the compressive strength with the addition of Basalt fibers. The microstructure of HPFRC was examined to determine the interfacial transition zone (ITZ) between the aggregates and the paste by using field emission scanning electron microscope (FESEM), which showed the improvement of the ITZ due to the addition of the Basalt fibers.