scholarly journals Effects of the addition of fluoride to a 4-META/MMA-TBB-based resin adhesive on fluoride release, acid resistance of enamel and shear bond strength in vitro

2013 ◽  
Vol 32 (1) ◽  
pp. 156-164 ◽  
Author(s):  
Masahiro IIJIMA ◽  
Shuichi ITO ◽  
Susumu NAKAGAKI ◽  
Takeshi MUGURUMA ◽  
Naohisa KOHDA ◽  
...  
Author(s):  
Sílvia Fontes Do Amaral Pereira

O objetivo do presente estudo in vitro foi verificar, através de teste de cisalhamento, a resistência de união da liga Wironia®light, à base de níquel-cromo sem berílio, sujeita a diferentes tratamentos de superfície, às cerâmicas Vita VM13 e Noritake. Foram confeccionados oitenta espécimes cilíndricos metálicos, com o auxílio de uma matriz de aço, nas dimensões de 4 mm de diâmetro por 4 mm de altura. Os espécimes foram divididos em oito grupos (n=10), de acordo com o tipo de tratamento superficial aplicado à liga metálica e com o tipo de cerâmica testada. Estes foram avaliados de acordo com os critérios de resistência ao cisalhamento e, com o auxílio de microscopia óptica, foi avaliada a área de cerâmica remanescente aderida ao metal após a fratura. Os corpos-de-prova do G6 (fabricados em Cerâmica Noritake com jateamento-26,401 ± 11,637 MPa) apresentaram maior resistência ao cisalhamento (p> 0,05) enquanto que os menores valores foram registrados no G4 (Cerâmica Vita com utilização de broca-13,440 ± 7,766 MPa). G6 (19425,4 μm2) apresentou a maior área de cerâmica aderida ao metal (p> 0,05) enquanto que o G4 (2310,2 μm2) apresentou a menor área. Concluiu-se que G6 obteve os valores mais altos de resistência ao cisalhamento e de remanescente cerâmico aderido à superfície metálica enquanto que o G4 obteve os valores mais baixos. Descritores: Restaurações metalo-cerâmicas; ligas de níquel-cromo;porcelana dentária.


2012 ◽  
Vol 83 (1) ◽  
pp. 152-157 ◽  
Author(s):  
Erika L. Silva-Benítez ◽  
Veronica Zavala-Alonso ◽  
Gabriel A. Martinez-Castanon ◽  
Juan P. Loyola-Rodriguez ◽  
Nuria Patiño-Marin ◽  
...  

Abstract Objective: To study the shear bond strength (SBS), sites of failure, and micromorphology of bonded molar tubes used on teeth affected by dental fluorosis. Materials and Methods: This in vitro study included 140 first molars classified according to Dean's index for dental fluorosis. Samples were divided into seven groups: (1) healthy teeth etched for 15 seconds, (2) teeth with moderate fluorosis (MOF) etched for 15 seconds, (3) teeth with MOF etched for 150 seconds, (4) teeth with MOF microabrasion etched for 15 seconds, (5) teeth with severe fluorosis (SEF) etched for 15 seconds, (6) teeth with SEF etched for 150 seconds, and (7) teeth with SEF microabrasion etched for 15 seconds. All samples were incubated and were then submitted to the SBS test and evaluated with the modified adhesive remnant index (ARI) and analyzed by using a scanning electronic microscope. Results: The SBS mean value for healthy enamel was 20 ± 10.2 MPa. For the group with MOF, the etched 150-second mean value was the highest (19 ± 7.6 MPa); for the group with SEF treated with microabrasion and etched for 15 seconds, the mean value was (13 ± 4.1 MPa). Significant differences (P ≤ .05) were found in the ARI between healthy and fluorosed groups. Conclusions: Fluorotic enamel affects the adhesion of bonded molar tubes. The use of overetching in cases of MOF and the combination of microabrasion and etching in SEF provides a suitable adhesion for fixed appliance therapy.


2010 ◽  
Vol 29 (2) ◽  
pp. 138-146 ◽  
Author(s):  
Zeynep ÖZKURT ◽  
Ender KAZAZOGLU ◽  
Ahmet ÜNAL

2013 ◽  
Vol 18 (3) ◽  
pp. 101-106 ◽  
Author(s):  
Sissy Maria Mendes Machado ◽  
Diego Bruno Pinho do Nascimento ◽  
Robson Costa Silva ◽  
Sandro Cordeiro Loretto ◽  
David Normando

OBJECTIVE: To evaluate in vitro the effects of tooth whitening using gel with Amorphous Calcium Phosphate (ACP) on the bond strength of metal brackets. METHODS: Thirty-six bovine incisors were sectioned at the crown-root interface, and the crowns were then placed in PVC cylinders. The specimens were divided into 3 groups (n = 12) according to whitening treatment and type of gel used, as follows: G1 (control) = no whitening; G2 = whitening with gel not containing ACP (Whiteness Perfect - FGM), G3 = whitening with gel containing ACP (Nite White ACP - Discus Dental). Groups G2 and G3 were subjected to 14 cycles of whitening followed by an interval of 15 days before the bonding of metal brackets. Shear bond strength testing was performed on a Kratos universal test machine at a speed of 0.5 mm/min. After the mechanical test, the specimens were assessed to determine the adhesive remnant index (ARI). The results were subjected to ANOVA, Tukey's test and Kruskal-Wallis test (5%). RESULTS: Significant differences were noted between the groups. Control group (G1 = 11.10 MPa) showed a statistically higher shear bond strength than the groups that underwent whitening (G2 = 5.40 Mpa, G3 = 3.73 MPa), which did not differ from each other. There were no significant differences between the groups in terms of ARI. CONCLUSION: Tooth whitening reduces the bond strength of metal brackets, whereas the presence of ACP in the whitening gel has no bearing on the results.


2012 ◽  
Vol 17 (4) ◽  
pp. 1-7 ◽  
Author(s):  
Roberto Hideo Shimizu ◽  
Karlos Giovani Grando ◽  
Isabela Almeida Shimizu ◽  
Augusto Ricardo Andriguetto ◽  
Ana Cláudia Moreira Melo ◽  
...  

OBJECTIVE: This in vitro study was designed to evaluate the shear bond strength (SBS) of orthodontic metal brackets bonded by direct and indirect techniques. METHODS: Thirty healthy human maxillary premolar teeth were used. The teeth were divided into three groups of 10 teeth each: Group I - indirect bonding with SondhiTM Rapid-Set system (3M/Unitek), Group II - indirect bonding with TransbondTM XT adhesive system (3M/Unitek) and Group III - direct bonding with TransbondTM XT adhesive system (3M/Unitek). After bonding and obtaining the specimens for the study, the specimens were subjected to SBS testing in a universal testing machine (Emic, model DL-500). The Kolmogorov-Smirnov test was applied to ascertain that the data had a normal distribution and the Bartlett test to check whether there was homogeneity of variance. One-factor analysis of variance was performed and, subsequently, Tukey's test for paired means. A 5% significance level was adopted. RESULTS: The results of Group I were 67.6 (N) and 5.9 (MPa); Group II, 68.9 (N) and 6.1 (MPa) and Group III (control), 92.5 (N) and 8.1 (MPa). CONCLUSION: It can therefore be concluded that the means for Group III were significantly higher compared with Groups I and II in both Newton (N) and Megapascal (MPa) values. The means attained by the indirect bonding technique used in Groups I and II, however, exhibited no statistically significant differences.