scholarly journals Plasticization of Polylactide with Myrcene and Limonene as Bio-Based Plasticizers: Conventional vs. Reactive Extrusion

Polymers ◽  
2019 ◽  
Vol 11 (8) ◽  
pp. 1363 ◽  
Author(s):  
Berit Brüster ◽  
Yann-Olivier Adjoua ◽  
Reiner Dieden ◽  
Patrick Grysan ◽  
Carlos Eloy Federico ◽  
...  

Polylactide (PLA) was blended by conventional and reactive extrusion with limonene (LM) or myrcene (My) as bio-based plasticizers. As-processed blends were carefully analyzed by a multiscale and multidisciplinary approach to tentatively determine their chemical structure, microstructure, thermal properties, tensile and impact behaviors, and hydrothermal stability. The main results indicated that LM and My were efficient plasticizers for PLA, since compared to neat PLA, the glass transition temperature was reduced, the ultimate tensile strain was increased, and the impact strength was increased, independently of the type of extrusion. The addition of a free radical initiator during the extrusion of PLA/LM was beneficial for the mechanical properties. Indeed, the probable formation of local branched/crosslinked regions in the PLA matrix enhanced the matrix crystallinity, the tensile yield stress, and the tensile ultimate stress compared to the non-reactive blend PLA/LM, while the other properties were retained. For PLA/My blends, reactive extrusion was detrimental for the mechanical properties since My polymerization was accelerated resulting in a drop of the tensile ultimate strain and impact strength, and an increase of the glass transition temperature. Indeed, large inclusions of polymerized My were formed, decreasing the available content of My for the plasticization and enhancing cavitation from inclusion-matrix debonding.

2007 ◽  
Vol 15 (5) ◽  
pp. 343-355 ◽  
Author(s):  
S. Lipponen ◽  
P. Pietikäinen ◽  
U. Vainio ◽  
R. Serimaa ◽  
J.V. Seppälä

Ethylene/1,7-octadiene copolymer was polymerised with metallocene catalyst and hydrosilylated to form silane functionalised polyethylenes (PE-co-SiX, X=Cl, OEt, Ph). The functionalised species were tested as modifiers in composites of rubber toughened polypropylene (heterophasic PP, hPP) and microsilica filler (μSi). A metallocene-based functionalised PE (PE-co-SiF) produced earlier in our laboratory and three commercial grades of functionalised polyolefins (one PE- and two PP-based) were used as reference modifiers. Major differences were seen in the toughness of the composites both above and below the glass transition temperature (Tg) of PP. In addition to increasing the stiffness, the microsilica filler enhanced the toughness of the heterophasic polypropylene by over 200% at ambient temperature. Below the Tg of PP (at −20 °C), the influence of μSi was the opposite and the impact strength of the hPP/μSi composite was below that of unfilled hPP. With the addition of just 2 wt% of functionalised polyethylene, the poor cold toughness of hPP/μSi composite was improved by nearly 100%. With the same addition, the toughness of the composites at ambient temperature was improved by 50 to 100% compared with the unfilled hPP. This behaviour was explained by significant changes in the fracture mechanism. Addition of functionalised PE increased the concentration of microsilica in the rubbery phase, allowing the crack to enter that phase. The rubbery phase was also able to absorb a large amount of impact energy below the glass transition temperature of PP.


Author(s):  
Galina S. Bozhenkova ◽  
Alexandra N. Tarakanovskaya ◽  
Oksana D. Tarnovskaya ◽  
Roman V. Ashirov

The article is devoted to the production of polymer by metathesis ring-opening polymerization under the influence of ruthenium initiator of type of Hoveyda-Grubbs II generation. The monomer used the mixture of dimethyl ether norbornene-2;3-dicarboxylic acid. The monomer was prepared by the Diels-Alder reaction of dicyclopentadiene and dimethyl maleate. The polymer was prepared in bulk of the monomer mixture. In this paper we have studied the physical and mechanical properties polydimethyl ether of norbornene-2;3-dicarboxylic acid; and assessed the impact of environmental factors on the change in properties of the polymer. As environmental factors; light; UV radiation; water; 0.1 M hydrochloric acid were applied; and accelerated aging conditions; which were held in a climate chamber. During performance we found that maintaining the polymer samples in the UV light chamber led to the slight increase in flexural modulus. In contrast; the polymer storage in water and in a hydrochloric acid solution for two months resulted in a slight decrease in the modulus of elasticity in bending index. These factors did not affect the change in the glass transition temperature of the polymer. Under the conditions of accelerated aging conducted for 1; 2 and 6 days after two cycles we observed the drop in modulus for bending of 8.5%; after 6 cycles of 13%. The glass transition temperature of polydimethyl ether of norbornene-2;3-dicarboxylic acid after 6 cycles decreased by only 3.4% in the climatic chamber. Studies have shown that the resulting polymer is resistant to water; hydrochloric acid; light and UV radiation; as well as it saves properties at a sufficient level for operation at conditions of accelerated aging. It should be noted that the tested polymer was prepared without additives; stabilizers and antioxidants. The proposed polymer can be used as a structural material for machine parts; including bulky.For citation:Bozhenkova G.S.; Tarakanovskaya A.N.; Tarnovskaya O.D.; Ashirov R.V. Influence of environmental factors on physical-mechanical properties of polydimethyl ether of norborene -2;3-dicarboxylic acid. Izv. Vyssh. Uchebn. Zaved. Khim. Khim. Tekhnol. 2017. V. 60. N 5. P. 68-73


Adhesive strength of «epoxy binder-steel wire» joints and the mechanical behavior of the binder during multiple repeated curing have been investigated. It is shown that when the curing temperature is considerably higher than the glass transition temperature of the binder, the adhesive strength decreases monotonically with an increase in the number of curing cycles. In this case the mechanical properties of the matrix also decrease. Possible mechanisms of the observed changes are discussed.


2011 ◽  
Vol 239-242 ◽  
pp. 3253-3256 ◽  
Author(s):  
Li Huo ◽  
Jun Gang Gao ◽  
Yong Gang Du

The curing, thermal and mechanical properties of bi-component system for bisphenol A epoxy resin (BPAER) modified by liquid crystalline Sulfonyl bis(4,1-phenylene)bis[4-(2,3-epoxypro pyloxy)benzoate] (p-SBPEPB), with 4,4'-diaminodiphenyl ether (DDE) as a curing agent, were investigated. The effect of the different liquid crystalline contents and the heating rate on curing reaction was discussed. The results show that the curing peak temperature decreases, curing rate increases, the glass transition temperature (Tg)and impact strength all increase with adding of liquid crystalline p-SBPEPB when the content is not over 8wt%.


1990 ◽  
Vol 68 (7) ◽  
pp. 1228-1232 ◽  
Author(s):  
Denis Duchesne ◽  
Adi Eisenberg

The thermal and dynamic mechanical properties of random butyl acrylate- and plasticized ethyl acrylate-based vinylpyridinium ionomers have been investigated. The properties of the ionomers were found to be dependent on the glass transition temperature of the matrix material. Ionomers having a glass transition temperature lower than ca. 25 °C exhibited all the features associated with the presence of phase-separated microdomains or clusters while the materials with higher glass transition temperatures were not. It was also observed that the dispersion associated with the vinylpyridinium clusters for a butyl acrylate-based ionomer with 12 mol% of ionic units occurs at ca. 25 °C. This value is very close to that observed previously by Otocka and Eirich in their study of a butadiene-based vinylpyridinium ionomer with the same ion content. Keywords: ionomers, plasticization, clustering, glass transition, dynamic mechanical properties.


2021 ◽  
Vol 2 (2) ◽  
pp. 419-430
Author(s):  
Ankur Bajpai ◽  
James R. Davidson ◽  
Colin Robert

The tensile fracture mechanics and thermo-mechanical properties of mixtures composed of two kinds of epoxy resins of different chemical structures and functional groups were studied. The base resin was a bi-functional epoxy resin based on diglycidyl ether of bisphenol-A (DGEBA) and the other resins were (a) distilled triglycidylether of meta-amino phenol (b) 1, 6–naphthalene di epoxy and (c) fluorene di epoxy. This research shows that a small number of multifunctional epoxy systems, both di- and tri-functional, can significantly increase tensile strength (14%) over neat DGEBA while having no negative impact on other mechanical properties including glass transition temperature and elastic modulus. In fact, when compared to unmodified DGEBA, the tri-functional epoxy shows a slight increase (5%) in glass transition temperature at 10 wt.% concentration. The enhanced crosslinking of DGEBA (90 wt.%)/distilled triglycidylether of meta-amino phenol (10 wt.%) blends may be the possible reason for the improved glass transition. Finally, the influence of strain rate, temperature and moisture were investigated for both the neat DGEBA and the best performing modified system. The neat DGEBA was steadily outperformed by its modified counterpart in every condition.


Life ◽  
2021 ◽  
Vol 11 (1) ◽  
pp. 43
Author(s):  
Lamya Zahir ◽  
Takumitsu Kida ◽  
Ryo Tanaka ◽  
Yuushou Nakayama ◽  
Takeshi Shiono ◽  
...  

An innovative type of biodegradable thermoplastic elastomers with improved mechanical properties from very common and potentially renewable sources, poly(L-lactide)-b-poly(2-methyl-1,3-propylene glutarate)-b-poly(L-lactide) (PLA-b-PMPG-b-PLA)s, has been developed for the first time. PLA-b-PMPG-b-PLAs were synthesized by polycondensation of 2-methyl-1,3-propanediol and glutaric acid and successive ring-opening polymerization of L-lactide, where PMPG is an amorphous central block with low glass transition temperature and PLA is hard semicrystalline terminal blocks. The copolymers showed glass transition temperature at lower than −40 °C and melting temperature at 130–152 °C. The tensile tests of these copolymers were also performed to evaluate their mechanical properties. The degradation of the copolymers and PMPG by enzymes proteinase K and lipase PS were investigated. Microbial biodegradation in seawater was also performed at 27 °C. The triblock copolymers and PMPG homopolymer were found to show 9–15% biodegradation within 28 days, representing their relatively high biodegradability in seawater. The macromolecular structure of the triblock copolymers of PLA and PMPG can be controlled to tune their mechanical and biodegradation properties, demonstrating their potential use in various applications.


Sign in / Sign up

Export Citation Format

Share Document