Microtensile Bond Strength of Resin Composite Bonded to Caries-affected Dentin with Three Adhesives

10.2341/06-2 ◽  
2007 ◽  
Vol 32 (1) ◽  
pp. 24-30 ◽  
Author(s):  
H. Omar ◽  
W. El-Badrawy ◽  
O. El-Mowafy ◽  
O. Atta ◽  
B. Saleem

Clinical Relevance Compared to two other adhesives, a self-etch adhesive resulted in higher microtensile bond strength values when used to bond a resin composite to both sound and caries-affected dentin.

2016 ◽  
Vol 27 (4) ◽  
pp. 446-451 ◽  
Author(s):  
João Luiz Bittencourt de Abreu ◽  
Maíra Prado ◽  
Renata Antoun Simão ◽  
Eduardo Moreira da Silva ◽  
Katia Regina Hostilio Cervantes Dias

Abstract Studies have been showing a decrease of bond strength in dentin treated with sodium hypochlorite (NaOCl). The aim of this study was to evaluate the effect of non-thermal argon plasma on the bond strength of a self-etch adhesive system to dentin exposed to NaOCl. Thirty-two flat dentin surfaces of bovine incisors were immersed in 2.5% NaOCl for 30 min to simulate the irrigation step during endodontic treatment. The specimens were divided into four groups (n=8), according to the surface treatment: Control (without plasma treatment), AR15 (argon plasma for 15 s), AR30 (argon plasma for 30 s) and AR45 (argon plasma for 45 s). For microtensile bond strength test, 5 specimens were used per group. In each group, the specimens were hybridized with a self-etch adhesive system (Clearfil SE Bond) and resin composite buildups were constructed. After 48 h of water storage, specimens were sectioned into sticks (5 per tooth, 25 per group) and subjected to microtensile bond strength test (μTBS) until failure, evaluating failure mode. Three specimens per group were analyzed under FTIR spectroscopy to verify the chemical modifications produced in dentin. μTBS data were analyzed using ANOVA and Tamhane tests (p<0.05). AR30 showed the highest μTBS (20.86±9.0). AR15 (13.81±6.4) and AR45 (11.51±6.8) were statistically similar to control (13.67±8.1). FTIR spectroscopy showed that argon plasma treatment produced chemical modifications in dentin. In conclusion, non-thermal argon plasma treatment for 30 s produced chemical changes in dentin and improved the μTBs of Clearfil SE Bond to NaOCl-treated dentin.


2010 ◽  
Vol 35 (1) ◽  
pp. 94-104 ◽  
Author(s):  
M. Sarr ◽  
A. W. Kane ◽  
J. Vreven ◽  
A. Mine ◽  
K. L. Van Landuyt ◽  
...  

Clinical Relevance In the current study, contemporary adhesives are assessed mechanically and ultra-morphologically to predict clinical effectiveness. Adhesives with simplified application procedures (in particular, one-step self-etch adhesives) still underperform as compared to conventional “gold-standard” multi-step adhesives. “Mild” two-step self-etch adhesives that provide additional chemical bonding appear to most optimally combine bonding effectiveness with a simplified application protocol.


2010 ◽  
Vol 35 (4) ◽  
pp. 428-435 ◽  
Author(s):  
A. Reis ◽  
C. Zander-Grande ◽  
S. Kossatz ◽  
R. Stanislawczuk ◽  
A. Manso ◽  
...  

Clinical Relevance All Bond 3 and All Bond Self-Etch are versatile systems, capable of being used either in the full or simplified version. Both showed adequate microtensile bond strength results in enamel and dentin after 24 hours of water storage.


2012 ◽  
Vol 37 (6) ◽  
pp. 610-616 ◽  
Author(s):  
RL Quock ◽  
JA Barros ◽  
SW Yang ◽  
SA Patel

SUMMARY The aim of this in vitro study was to investigate the effect of the cariostatic and preventive agent silver diamine fluoride (SDF) on the microtensile bond strength of resin composite to dentin. Forty-two caries-free, extracted molars were flattened occlusally and apically using a diamond saw, and the exposed occlusal dentin was polished with a series of silicon carbide papers, all under water irrigation. The teeth were then randomly divided into six groups of seven teeth each that were treated as follows: 1) Peak SE self-etch bonding agent; 2) 12% SDF + Peak SE; 3) 38% SDF + Peak SE; 4) Peak LC etch-and-rinse bonding agent; 5) 12% SDF + Peak LC; and 6) 38% SDF + Peak LC. Four-millimeter buildups of Amelogen Plus were incrementally placed on all teeth; after a 24-hour storage period in distilled water, the specimens were sectioned perpendicular to the adhesive interface to produce beams of cross-sectional surface area measuring approximately 1 mm2. The beams were placed on a microtensile testing machine, which utilized a single-speed pump motor and force gauge at 20 kgf × 0.01 second to record maximum tensile force before failure occurred. Two-way analysis of variance and post hoc Tukey tests were performed to compare the effects of the SDF on microtensile bond strength, with statistical significance set at α = 0.05. None of the experimental groups treated with different concentrations of SDF showed a significant difference in bond strength compared to the control groups, and there was no significant difference in bond strength between self-etch and etch-and-rinse groups. However, the effect of SDF on self-etch bonded teeth compared to etch-and-rinse bonded teeth was statistically significant (p=0.0363), specifically at the 12% concentration. SDF does not adversely affect the bond strength of resin composite to noncarious dentin.


2011 ◽  
Vol 22 (2) ◽  
pp. 122-128 ◽  
Author(s):  
Vinicius Di Hipólito ◽  
Roberta Caroline Bruschi Alonso ◽  
Marcela Rocha de Oliveira Carrilho ◽  
Camillo Anauate Netto ◽  
Mário Alexandre Coelho Sinhoreti ◽  
...  

This study evaluated the bonding characteristics to ground and unground enamel obtained with different strategies. For this purpose, 24 sound third-molars were bisected mesiodistally to obtain tooth halves. A flat enamel area was delimited in the tooth sections, which were randomly distributed into 8 groups (n=6), according to the enamel condition (ground and unground) and adhesive system (Adper Single Bond 2 - SB2; Adper Prompt L-Pop - PLP; Adper Prompt - AD; Clearfil SE Bond - SE). Each system was applied according manufacturers' instructions and a 6-mm-high resin composite "crown" was incrementally built up on bonded surfaces. Hourglass-shaped specimens with 0.8 mm² cross-section were produced. Microtensile bond strength (μTBS) was recorded and the failure patterns were classified. Results were analyzed by two-way ANOVA and Tukey's test (α=0.05). There were no statistically significant differences among the μTBS values of SB2, PLP and AD (p>0.05). SE values were significantly lower (p0.05). There was prevalence of cohesive failure within enamel, adhesive system and resin composite for SB2. The self-etch systems produced higher incidence of cohesive failures in the adhesive system. Enamel condition did not determine significant differences on bonding characteristics for the same bonding system. In conclusion, the bonding systems evaluated in this study resulted in specific μTBS and failure patterns due to the particular interaction with enamel.


2020 ◽  
Vol 23 (2) ◽  
Author(s):  
Amr Mohsen Mohamed ◽  
Sameh Mahoud Nabih ◽  
Mohamed Ahmed Wakwak

Objective: The purpose of this study was to evaluate the effect of chitosan nanoparticles on microtensile bond strength of resin composite to dentin using self etch adhesive after aging. Material and Methods: A total number of 90 freshly extracted, sound human molar teeth. Flat tooth surface was gained after cut of the occlusal surface. Three main groups according to pretreatment of dentin before adhesive application; 0.2 % chitosan, 2.5 % chitosan and no treatment control group. Universal self etch adhesive were applied according to manufacture instruction and 4 mm of Feltik Z250 xt composite. Storage of specimens for 1 day, 3 months and 6 months in 37O C distilled water. After that, the tooth was sectioned to beams of 1 mm x8 mm sticks for microtensile bond strength test using universal testing machine. Scanning electron microscope (SEM) was used to evalute the effect of chitosan nanoparticles on dentin and smear layer. Kruskal-Wallis test was used to compare between the three groups as well as the three aging periods. Dunn’s test was used for pair-wise comparisons. The significance level was set at P ≤ 0.05. Results: chitosan 0.2% is statistically significant increase in bond strength than chitosan 2.5% and control in one day group. Three months chitosan 0.2 % groups have statistically significant increase in bond strength than chitosan 2.5%. It was found in 6 months that control and chitosan 0.2 % have statistically significant increase in bond strength than chitosan 2.5%. There was statistically significant difference found between the three studied groups regarding bond strength at different storage times . Conclusion: Microtensile bond strength was influenced by different chitosan concentration. Different aging periods had no effect on the microtensile bond strength without application of chitosan and with application of 2.5% chitosan concentration.KEYWORDSChitosan nanoparticles; Microtensile bond strength; MMPs.


10.2341/06-32 ◽  
2007 ◽  
Vol 32 (2) ◽  
pp. 133-137 ◽  
Author(s):  
M. Toledano ◽  
J. P. Proença ◽  
M. C. G. Erhardt ◽  
E. Osorio ◽  
F. S. Aguilera ◽  
...  

Clinical Relevance When treating dentin surfaces with Futurabond one-step self-etch bonding agent, in order to obtain higher microtensile bond strength, doubling the application time of the adhesive should be considered.


2009 ◽  
Vol 34 (4) ◽  
pp. 460-466 ◽  
Author(s):  
Z. Ergücü ◽  
E. U. Çelik ◽  
N. Ünlü ◽  
M. Türkün ◽  
F. Özer

Clinical Relevance The microtensile bond strength of a three-step etch-and-rinse and a two-step self-etch adhesive is not negatively affected by Er,Cr:YSGG laser irradiation in sound and caries-affected dentin.


2013 ◽  
Vol 07 (03) ◽  
pp. 315-326 ◽  
Author(s):  
Luciana Andrea Salvio ◽  
Vinicius Di Hipólito ◽  
Adriano Luis Martins ◽  
Mario Fernando de Goes

ABSTRACT Objective: To evaluate the hybridization quality and bond strength of adhesives to dentin. Materials and Methods: Ten human molars were ground to expose the dentin and then sectioned in four tooth-quarters. They were randomly divided into 5 groups according to the adhesive used: Two single-step self-etch adhesives - Adper Prompt (ADP) and Xeno III (XE), two two-step self-etching primer systems - Clearfil SE Bond (SE) and Adhe SE (ADSE), and one one-step etch-and-rinse system - Adper Single Bond (SB). Resin composite (Filtek Z250) crown buildups were made on the bonded surfaces and incrementally light-cured for 20 s. The restored tooth-quarters were stored in water at 37΀C for 24 h and then sectioned into beams (0.8 mm 2 in cross-section). Maximal microtensile bond strength (μ-TBS) was recorded (0.5 mm/min in crosshead speed). The results were submitted to one-way ANOVA and Tukey′s test (α = 0.05). Thirty additional teeth were used to investigate the hybridization quality by SEM using silver methenamine or ammoniacal silver nitrate dyes. Results: SE reached significantly higher μ-TBS (P < 0.05); no significance was found between ADSE and XE (P > 0.05), and between SB and ADP (P > 0.05); ADSE and XE were significantly higher than SB and ADP (P < 0.05). The bonding interface of SB showed the most intense silver uptake. SE and ADSE showed more favorable hybridization quality than that observed for ADP and XE. Conclusions: The bond strength and hybridization quality were affected by the interaction form of the adhesives with dentin. The hybridization quality was essential to improve the immediate μ-TBS to dentin.


Sign in / Sign up

Export Citation Format

Share Document