scholarly journals Conducting materials based on nanodispersed titanium monoxide

2007 ◽  
Vol 39 (3) ◽  
pp. 295-299 ◽  
Author(s):  
A.A. Gusev ◽  
E.G. Avvakumov

The possibility of obtaining the TiO compound during mechanical activation of rutile and titanium in a planetary mill was studied depending on ball size and the activation time. The initial substances, TiO2 (rutile) and Ti (metal), were shown to change into TiO almost completely during grinding as early as after ten minutes. In this case the cubic modification of TiO formed, with the lattice parameter a=4.185(7) ? and particles of 1-3 ?m, which consisted of units about 10 nm in size. The other subject of our research was the dependence of the conductivity of the products on the conditions under which they were moulded and sintered under argon. The conductivity of the samples was in the range 300 to 600 S cm-1. Their chemical resistance equaled that of Ti4O7 samples.

2013 ◽  
Vol 333 ◽  
pp. 193-198 ◽  
Author(s):  
O.M. Fedorova ◽  
Anatoly Yakovlevich Fishman ◽  
Tatiana Eugenievna Kurennykh ◽  
Vladimir Borisovich Vykhodets ◽  
V.B. Vykhodets

sotope exchange of oxygen 18О2 with oxides NdMnO3+δ was investigated. The oxide was obtained from oxides Nd2O3 and Mn2O3 using a ceramic technology with annealing in air at 1400°C for 90 hours followed by cooling in a furnace. A planetary mill AGO-2 with a centrifugal factor of g = 60 was used for mechanical treatment of oxides. The study of isotope exchange was carried out by nuclear microanalysis. The concentration of the isotopes 18O and 16O in oxides was determined using a Van de Graaff accelerator and 18O(p, α)15N and 16O(d, p)17O* reactions at the energies of incident beams 762 and 900 keV. Isothermal annealing of powders was carried out in oxygen, enriched to 80% by the isotope 18O. It was established that the concentration of the isotope 18O in mechanically activated powders was several times higher than in the initial micropowder under the same conditions of annealing. The effect increased with increasing of mechanical activation time (30 - 300 s). The isotope exchange parameters connected with the processes at the boundaries of the particles of mechano-activated powder and within their volume were analyzed.


Minerals ◽  
2020 ◽  
Vol 10 (9) ◽  
pp. 827 ◽  
Author(s):  
Alexander M. Kalinkin ◽  
Basya I. Gurevich ◽  
Mikhail S. Myshenkov ◽  
Mikhail V. Chislov ◽  
Elena V. Kalinkina ◽  
...  

Blends of fly ash and natural calcite, mechanically activated for 0–400 s in a planetary mill, were used to synthesize geopolymers at ambient temperature. The calcite content in the blends was 0–10 wt.%. Sodium hydroxide solution was used as an alkaline agent. Mechanical activation of the raw material considerably enhanced its reactivity with respect to the alkaline agent, as was observed using Fourier-transform infrared spectroscopy, isothermal conduction calorimetry, thermogravimetry coupled with mass spectrometry analysis of the evolved gas, and SEM/EDS. The addition of calcite to the fly ash improved the compressive strength of the geopolymers, especially during the early age of curing. For 7 d aged geopolymers based on the 90% fly ash + 10% calcite blend, the strength was 8.0-, 3.5- and 2.9-fold higher than that for the geopolymers based on the unblended fly ash for 30 s, 180 s and 400 s mechanical activation time, respectively. Using Mössbauer spectroscopy, it was revealed that iron present in the fly ash did not play a significant part in the geopolymerization process. The dominant reaction product was sodium containing aluminosilicate hydrogel (N-A-S-H gel). Calcite was found to transform, to a small extent, to vaterite and Ca(OH)2 in the course of the geopolymerization.


2010 ◽  
Vol 63 ◽  
pp. 420-424
Author(s):  
Riva Rivas-Marquez ◽  
Carlos Gomez-Yanez ◽  
Ivan Velasco-Davalos ◽  
Jesus Cruz-Rivera

Using Mechanical Activation it is possible to obtain small grain size and good homogeneity in a ceramic piece. For ZnO varistor devices Mechanical Activation appears to be a good fabrication technique, since good homogeneity and small grain sizes are advantageous microstructural features. The typical formulation is composed by ZnO, Bi2O3, Sb2O3, CoO, MnO2 and Cr2O3 as raw materials, and during sintering, several dissolutions and reactions to form pyrochlore and spinel phases occur. When Mechanical Activation is applied to the entire formulation, it is difficult to know what processes are being mechanically activated due to the complexity of the system. The aim of the present work was to clarify how the mechanical activation is taking place in a typical ZnO varistor formulation. The methodology consisted in the formation of all possible combinations of two out of the five oxides above mentioned and to apply mechanical activation on the mixture of each pair of powders. The results showed that systems containing Bi2O3 are prone to react during mechanical activation. Also, reduction reactions were observed in MnO2. In addition, the powder mixture corresponding to the whole formulation was milled in a planetary mill, pressed and sintered, and varistor devices were fabricated. Improvement in the nonlinearity coefficient and breakdown voltage was observed.


2005 ◽  
Vol 475-479 ◽  
pp. 841-844 ◽  
Author(s):  
Hideki Hosoda ◽  
Yuji Higaki ◽  
Shuichi Miyazaki

The phase constitution, lattice parameter, martensitic and magnetic transformation behavior and hardness of the Ni2MnGa-Cu2MnAl pseudobinary alloys designed as (Ni2MnGa)x(Cu2MnAl)1-x were investigated in order to improve magnetic properties of Ni2MnGa. It was revealed that L21 Ni2MnGa and Cu2MnAl make a continuous solid solution of (Ni,Cu)2Mn(Ga,Al) when heat treated at 1073K, and that the lattice parameter of the L21 phase increases monotonously with increasing the compositional ratio x, that is, the amount of Cu2MnAl. Curie temperature TC also increases with increasing x. On the other hand, the martensitic transformation temperature of Ni2MnGa seems to decrease rapidly by adding Cu2MnAl. Hardness of the alloys heat-treated at 1073K ranges from HV200 to HV370, and solution hardening was recognized by mixing. When heat treated at 773K, a phase decomposition from L21 phase to Cu9Al4 and b-Mn was confirmed in the Cu2MnAl-rich alloys. The phase decomposition causes a decrease in the lattice parameter of L21 phase and TC and a significant increase in hardness.


2016 ◽  
Vol 1 (1) ◽  
pp. 122 ◽  
Author(s):  
A.A. Okhlopkova ◽  
L.A. Nikiforov ◽  
T.A. Okhlopkova ◽  
R.V. Borisova

<p>Several technologies of the preparation of nanocomposites based on ultra-high-molecular-weight polyethylene were developed. The first technology is based on mechanical activation of layered silicates with surfactant before addition into polymer matrix. The second technology represents mixing of ultra-high-molecular-weight polyethylene with nanoparticles by joint mechanical activation in a planetary mill. The third technology is based on mixing of ultra-high-molecular-weight polyethylene with nanoparticles in liquid media under continuous ultrasonic treatment. Common features of these technologies are reaching of filler uniform distribution in a polymer matrix and significant improvement in the mechanical properties. Also, supramolecular structure of the composites was studied.</p>


2019 ◽  
Vol 18 (03n04) ◽  
pp. 1940067
Author(s):  
P. Vitiaz ◽  
N. Lyakhov ◽  
T. Grigoreva ◽  
E. Pavlov

The interaction between a solid inert metal Ir and an active liquid metal Ga during mechanical activation in a high-energy planetary mill is studied by X-ray diffraction and scanning electron microscopy with high-resolution energy dispersive X-ray microanalysis. The effect of mechanical activation on the formation of GaxIry intermetallic compounds and GaxIry/Ir composites and their solubility in acids was investigated. The subsequent extraction of Ga from intermetallic compounds and composites in the mixture of concentrated acids [Formula: see text] makes it possible to produce nanoscale Ir.


2020 ◽  
Vol 49 (1) ◽  
pp. 233-250 ◽  
Author(s):  
Caroline H. Roney ◽  
Rokas Bendikas ◽  
Farhad Pashakhanloo ◽  
Cesare Corrado ◽  
Edward J. Vigmond ◽  
...  

AbstractAtrial anisotropy affects electrical propagation patterns, anchor locations of atrial reentrant drivers, and atrial mechanics. However, patient-specific atrial fibre fields and anisotropy measurements are not currently available, and consequently assigning fibre fields to atrial models is challenging. We aimed to construct an atrial fibre atlas from a high-resolution DTMRI dataset that optimally reproduces electrophysiology simulation predictions corresponding to patient-specific fibre fields, and to develop a methodology for automatically assigning fibres to patient-specific anatomies. We extended an atrial coordinate system to map the pulmonary veins, vena cava and appendages to standardised positions in the coordinate system corresponding to the average location across the anatomies. We then expressed each fibre field in this atrial coordinate system and calculated an average fibre field. To assess the effects of fibre field on patient-specific modelling predictions, we calculated paced activation time maps and electrical driver locations during AF. In total, 756 activation time maps were calculated (7 anatomies with 9 fibre maps and 2 pacing locations, for the endocardial, epicardial and bilayer surface models of the LA and RA). Patient-specific fibre fields had a relatively small effect on average paced activation maps (range of mean local activation time difference for LA fields: 2.67–3.60 ms, and for RA fields: 2.29–3.44 ms), but had a larger effect on maximum LAT differences (range for LA 12.7–16.6%; range for RA 11.9–15.0%). A total of 126 phase singularity density maps were calculated (7 anatomies with 9 fibre maps for the LA and RA bilayer models). The fibre field corresponding to anatomy 1 had the highest median PS density map correlation coefficient for LA bilayer simulations (0.44 compared to the other correlations, ranging from 0.14 to 0.39), while the average fibre field had the highest correlation for the RA bilayer simulations (0.61 compared to the other correlations, ranging from 0.37 to 0.56). For sinus rhythm simulations, average activation time is robust to fibre field direction; however, maximum differences can still be significant. Patient specific fibres are more important for arrhythmia simulations, particularly in the left atrium. We propose using the fibre field corresponding to DTMRI dataset 1 for LA simulations, and the average fibre field for RA simulations as these optimally predicted arrhythmia properties.


2013 ◽  
Vol 690-693 ◽  
pp. 3529-3532
Author(s):  
Yu Xing ◽  
Hong Gao ◽  
Yuan Fang Ying ◽  
De Zheng Qu

The activation effect of ball-to-powder ratio and activation time on phosphorite ore that takes place in mechanochemical activation has been investigated in present paper, which is carried out in a planetary mill AGO-II. The results show that, particle sizes decreased after activation; the leaching rate of water-soluble P2O5 increased 4.6 percentage as ball-to-powder ratio rose from 8:1 to 40:1; the activated particle of samples has been highly dispersed, while the leaching rate of water-soluble P2O5 reached 10.1% after milling 15 minutes during activation, which was 4 times as high as the un-activated samples. The results show a potential utilization of low-medium grade phosphorite ore with mechanochemical activation directly.


1989 ◽  
Vol 158 ◽  
Author(s):  
M. Okoshi ◽  
M. Murahara ◽  
K. Toyoda

ABSTRACTThe fluorocarbon resin (Teflon) which is a very stable material chemically, has chemical resistance. Because of this property, it has no affinity for oil or water. Therefore, we have tried selective area modification of the resin surface b-y using an excimer laser.Fluorocarbon resin is a polymer of C-F bonds. In our experiment, the resin surface was irradiated by an ArF excimer laser, of which the photon energy is higher than that of the C-F bond, to excite the strong C-F bonds. B radicals, the best combination for F atoms, were formed simultaneously. Consequently, F atoms of C-F bonds were pulled out by B radicals. B(CH3 )3 with absorption in agreement with the wavelength of the ArF laser were used as raw materials of the B radicals. By irradiating the gas by the ArF laser beam, the photodecomposed B radicals functioned by pulling out F atoms, and the other methyl radicals ( -CH3 ) substituted for F atoms. As the result, this resin surface turned out to be oleophilic exclusively on the areas exposed to the light.


2014 ◽  
Vol 118 (2) ◽  
pp. 1245-1251 ◽  
Author(s):  
Traian Florin Marinca ◽  
Bogdan Viorel Neamţu ◽  
Ionel Chicinaş ◽  
Petru Pascuta

Sign in / Sign up