Corrosion Resistance of Low-Temperature and Conventional Plasma-Nitrided 410S Ferritic-Martensitic Stainless Steels

2021 ◽  
Vol 10 (1) ◽  
pp. 20200099
Author(s):  
L. B. Varela ◽  
M. T. Umemura ◽  
J. W. Calderón-Hernández ◽  
C. E. Pinedo ◽  
F. O. Kolawole ◽  
...  
2011 ◽  
Vol 312-315 ◽  
pp. 994-999 ◽  
Author(s):  
Riza Karadas ◽  
Ozgur Celik ◽  
Huseyin Cimenoglu

Nitriding is as an effective technique applied for many years to improve the surface hardness and wear resistance of low carbon and tool steels [1]. In the case of stainless steels, increase of surface hardness and wear resistance accompany by a drop in corrosion resistance due to the precipitation of CrN. In this respect, many attempts have been made to modify the surfaces of austenitic stainless steels to increase their surface hardness and wear resistance without scarifying the corrosion resistance [2-6]. It is finally concluded that, nitriding at temperatures lower than conventional nitriding process (which is generally about 550°C) has potentiality to produce a nitrogen expanded austenite (also known as S-phase), on the surface without formation of CrN. Due to the superb properties of the S-phase, the low temperature nitrided austenitic stainless steels exhibit very high surface hardness, a good wear resistance, and more importantly, an excellent corrosion resistance. Recently some attempts have been made to apply low temperature nitriding to martensitic stainless steels, which are widely used in the industries of medicine, food, mold and other civil areas [7-9]. In these works, where nitriding has been conducted by plasma processes, superior surface hardness, along with excellent wear and corrosion resistances have been reported for AISI 410 and AISI 420 grade martensitic stainless steels. This work focuses on low temperature gas nitriding of AISI 420 grade martensitic stainless steel in a fluidized bed reactor. In this respect the microstructures, phase compositions, hardness, wear and corrosion behaviours of the original and nitrided martensitic stainless steels have been compared.


Alloy Digest ◽  
2009 ◽  
Vol 58 (5) ◽  

Abstract Crucible 174 SXR is a premium-quality precipitation-hardening stainless steel designed for use as rifle barrels. It is a modification of Crucible’s 17Cr-4Ni that offers substantially improved machinability without sacrificing toughness. Its excellent corrosion resistance approaches that of a 300 series austenitic stainless steel, while its high strength is characteristic of 400 series martensitic stainless steels. At similar hardness levels, Crucible 174 SXR offers greater toughness than either the 410 or 416 stainless steels which are commonly used for rifle barrels. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming and heat treating. Filing Code: SS-1034. Producer or source: Crucible Service Centers.


Metals ◽  
2021 ◽  
Vol 11 (11) ◽  
pp. 1845
Author(s):  
Francesca Borgioli ◽  
Emanuele Galvanetto ◽  
Tiberio Bacci

Low-temperature nitriding allows to improve surface hardening of austenitic stainless steels, maintaining or even increasing their corrosion resistance. The treatment conditions to be used in order to avoid the precipitation of large amounts of nitrides are strictly related to alloy composition. When nickel is substituted by manganese as an austenite forming element, the production of nitride-free modified surface layers becomes a challenge, since manganese is a nitride forming element while nickel is not. In this study, the effects of nitriding conditions on the characteristics of the modified surface layers obtained on an austenitic stainless steel having a high manganese content and a negligible nickel one, a so-called nickel-free austenitic stainless steel, were investigated. Microstructure, phase composition, surface microhardness, and corrosion behavior in 5% NaCl were evaluated. The obtained results suggest that the precipitation of a large volume fraction of nitrides can be avoided using treatment temperatures lower than those usually employed for nickel-containing austenitic stainless steels. Nitriding at 360 and 380 °C for duration up to 5 h allows to produce modified surface layers, consisting mainly of the so-called expanded austenite or gN, which increase surface hardness in comparison with the untreated steel. Using selected conditions, corrosion resistance can also be significantly improved.


2006 ◽  
pp. 115-124

Abstract Martensitic stainless steels are essentially iron-chromium-carbon alloys that possess a body-centered tetragonal crystal structure (martensitic) in the hardened condition. Martensitic stainless steels are similar to plain carbon or low-alloy steels that are austenitized, hardened by quenching, and then tempered for increased ductility and toughness. This chapter provides a basic understanding of grade designations, properties, corrosion resistance, and general welding considerations of martensitic stainless steels. It also discusses the causes for hydrogen-induced cracking in martensitic stainless steels and describes sulfide stress corrosion resistance of type 410 weldments.