Magnetic-field Sensitivity for Monomodal Magnetic Elastomers with Various Volume Fractions of Magnetic Particles

2017 ◽  
Vol 46 (11) ◽  
pp. 1628-1630
Author(s):  
Jinta Nanpo ◽  
Shota Abe ◽  
Mika Kawai ◽  
Tetsu Mitsumata
Polymers ◽  
2018 ◽  
Vol 10 (12) ◽  
pp. 1351 ◽  
Author(s):  
Yasuhiro Umehara ◽  
Yusuke Yamanaga ◽  
Shota Akama ◽  
Shunsuke Kato ◽  
Shogo Kamoshita ◽  
...  

We fabricated a mono-link using bimodal magnetic elastomers that demonstrate drastic changes in the elastic modulus by magnetic fields. The magnetic elastomer is bimodal consisting of large magnetic particles and nonmagnetic fine particles. The storage modulus for bimodal magnetic elastomers was altered from 2.2 × 105 to 1.7 × 106 Pa by a magnetic field of 500 mT. Compression tests up to a strain of 20% also revealed that the on-field stress for the bimodal magnetic elastomer was 1.24 times higher than the off-field stress. The bimodal magnetic elastomer was synthesized for the mono-link and was mounted on the bogie of a railway vehicle. A running test exhibited that the wheel lateral force was reduced by 20% by applying a magnetic field of 390 mT.


2016 ◽  
Vol 120 (50) ◽  
pp. 12993-13000 ◽  
Author(s):  
Jinta Nanpo ◽  
Kazushi Nagashima ◽  
Yasuhiro Umehara ◽  
Mika Kawai ◽  
Tetsu Mitsumata

2016 ◽  
Vol 45 (7) ◽  
pp. 785-786 ◽  
Author(s):  
Jinta Nanpo ◽  
Mika Kawai ◽  
Tetsu Mitsumata

Polymers ◽  
2020 ◽  
Vol 12 (2) ◽  
pp. 290
Author(s):  
Shota Akama ◽  
Yusuke Kobayashi ◽  
Mika Kawai ◽  
Tetsu Mitsumata

The magnetic response of the storage modulus for bimodal magnetic elastomers containing magnetic particles with a diameter of 7.0 μm and plastic beads with a diameter of 200 μm were investigated by varying the volume fraction of plastic beads up to 0.60 while keeping the volume fraction of the magnetic particles at 0.10. The storage modulus at 0 mT for monomodal magnetic elastomers was 1.4 × 104 Pa, and it slightly increased with the volume fraction of plastic beads up to 0.6. The storage modulus at 500 mT for bimodal magnetic elastomers at volume fractions below 0.25 was constant, which was equal to that for the monomodal one (=7.9 × 104 Pa). At volume fractions of 0.25–0.40, the storage modulus significantly increased with the volume fraction, showing a percolation behavior. At volume fractions of 0.40-0.60, the storage modulus was constant at 2.0 × 105 Pa, independently of the volume fraction. These results indicate that the enhanced increase in the storage modulus was caused by the chain formation of the magnetic particles in vacancies made of plastic beads.


2019 ◽  
Vol 20 (12) ◽  
pp. 2879 ◽  
Author(s):  
Mayuko Watanabe ◽  
Yoshihiro Takeda ◽  
Takayuki Maruyama ◽  
Junko Ikeda ◽  
Mika Kawai ◽  
...  

The morphology of magnetic particles with a size of 7.0 μm was observed for magnetic elastomers with a concentration of magnetic particles of 70 wt% using an X-ray microscope remolded into high resolution. Computed tomography images revealed that magnetic particles were distributed isotopically in the absence of a magnetic field, but they formed a chain structure in the polyurethane network under a magnetic field of 270 mT. It was also established, by image analysis, that magnetic elastomers had an anisotropic structure under the magnetic field.


2020 ◽  
Vol 64 (1-4) ◽  
pp. 439-446
Author(s):  
Gildas Diguet ◽  
Gael Sebald ◽  
Masami Nakano ◽  
Mickaël Lallart ◽  
Jean-Yves Cavaillé

Magneto Rheological Elastomers (MREs) are composite materials based on an elastomer filled by magnetic particles. Anisotropic MRE can be easily manufactured by curing the material under homogeneous magnetic field which creates column of particles. The magnetic and elastic properties are actually coupled making these MREs suitable for energy conversion. From these remarkable properties, an energy harvesting device is considered through the application of a DC bias magnetic induction on two MREs as a metal piece is applying an AC shear strain on them. Such strain therefore changes the permeabilities of the elastomers, hence generating an AC magnetic induction which can be converted into AC electrical signal with the help of a coil. The device is simulated with a Finite Element Method software to examine the effect of the MRE parameters, the DC bias magnetic induction and applied shear strain (amplitude and frequency) on the resulting electrical signal.


2021 ◽  
Vol 7 (5) ◽  
pp. 82
Author(s):  
River Gassen ◽  
Dennis Thompkins ◽  
Austin Routt ◽  
Philippe Jones ◽  
Meghan Smith ◽  
...  

Magnetic particles have been evaluated for their biomedical applications as a drug delivery system to treat asthma and other lung diseases. In this study, ferromagnetic barium hexaferrite (BaFe12O19) and iron oxide (Fe3O4) particles were suspended in water or glycerol, as glycerol can be 1000 times more viscous than water. The particle concentration was 2.50 mg/mL for BaFe12O19 particle clusters and 1.00 mg/mL for Fe3O4 particle clusters. The magnetic particle cluster cross-sectional area ranged from 15 to 1000 μμm2, and the particle cluster diameter ranged from 5 to 45 μμm. The magnetic particle clusters were exposed to oscillating or rotating magnetic fields and imaged with an optical microscope. The oscillation frequency of the applied magnetic fields, which was created by homemade wire spools inserted into an optical microscope, ranged from 10 to 180 Hz. The magnetic field magnitudes varied from 0.25 to 9 mT. The minimum magnetic field required for particle cluster rotation or oscillation in glycerol was experimentally measured at different frequencies. The results are in qualitative agreement with a simplified model for single-domain magnetic particles, with an average deviation from the model of 1.7 ± 1.3. The observed difference may be accounted for by the fact that our simplified model does not include effects on particle cluster motion caused by randomly oriented domains in multi-domain magnetic particle clusters, irregular particle cluster size, or magnetic anisotropy, among other effects.


2011 ◽  
Vol 378-379 ◽  
pp. 663-667 ◽  
Author(s):  
Toempong Phetchakul ◽  
Wittaya Luanatikomkul ◽  
Chana Leepattarapongpan ◽  
E. Chaowicharat ◽  
Putapon Pengpad ◽  
...  

This paper presents the simulation model of Dual Magnetodiode and Dual Schottky Magnetodiode using Sentaurus TCAD to simulate the virtual structure of magneto device and apply Hall Effect to measure magnetic field response of the device. Firstly, we use the program to simulate the magnetodiode with p-type semiconductor and aluminum anode and measure electrical properties and magnetic field sensitivity. Simulation results show that sensitivity of Dual Schottky magnetodiode is higher than that of Dual magnetodiode.


Sign in / Sign up

Export Citation Format

Share Document