Luminescence Properties of Tb3+, Eu3+, Tm3+ Co-Doped Na5La(MoO4)4 for White Light-Emitting Diode

2014 ◽  
Vol 14 (5) ◽  
pp. 3683-3686 ◽  
Author(s):  
Ye Jin ◽  
Wei Lu ◽  
Jiahua Zhang ◽  
Zhendong Hao ◽  
Xia Zhang
2009 ◽  
Vol 24 (5) ◽  
pp. 1730-1734 ◽  
Author(s):  
Hucheng Yang ◽  
G. Lakshminarayana ◽  
Yu Teng ◽  
Shifeng Zhou ◽  
Jianrong Qiu

Sm3+, Ce3+ codoped Al2O3–La2O3–SiO2 glasses were prepared and their luminescence properties were characterized. Blue-cyan to orange-red tunable luminescence was observed from these glasses with different excitation wavelengths ranging from 385 to 410 nm. White light emission with internal luminescence efficiency 42% has been observed using commercially available purple light-emitting-diode excitation. The energy transfer between Ce3+ and Sm3+ has also been investigated from fluorescence decay curves and spectral properties.


2018 ◽  
Vol 100 ◽  
pp. 26-31 ◽  
Author(s):  
Irish Valerie B. Maggay ◽  
Kai-Yuan Yeh ◽  
Bingfu Lei ◽  
Mikhail G. Brik ◽  
Michal Piasecki ◽  
...  

2021 ◽  
Vol 11 (1) ◽  
pp. 54-62
Author(s):  
Jinpeng Xie ◽  
Bonan Liu ◽  
Qingtao Qong ◽  
Zhicheng Xu ◽  
Zhiqiang Jin ◽  
...  

In this work, we report Eu3+/Tb3+/Eu2+ co-activated Gd2O2 S as novel phosphor materials that can be effectively applied in the white-light emitting diode based on a near-UV chip with sensational performances. The luminescent properties and energy transfer mechanism have been thoroughly investigated. The as-prepared europium/terbium co-doped Gd2O2 S phosphors exhibit strong fluorescence with tunable color output under UV-vis light excitation. Furthermore, a high response to ultraviolet illumination of 398 nm wavelength was observed in the excitation spectra, indicating an excellent match with a light-emitting-diode chip in the dominant emissions. It is found that a tricolor (blue, green and red) emission band which results in a white light emission can be acquired when Eu3+, Eu2+ and Tb3+ ions are all co-doped into the single phase Gd2O2S, and an optimum ion doping level (10 at.% Eu and 0.7 at.% Tb) can effectively emit nearly pure white color photoluminescence with lifetime effectively tuned from 0.55 ms to 1.10 ms. The CIE (Commission International de I'Eclairage 1931 chromaticity) is X = 0.3507, Y = 0.3029. It is therefore expected that the newly found phosphor material with high-performance properties possess great potentials for the future advanced white LED applications.


2015 ◽  
Vol 31 (12) ◽  
pp. 1232-1236 ◽  
Author(s):  
Yongzhang Jiang ◽  
Haiping Xia ◽  
Jiazhong Zhang ◽  
Shuo Yang ◽  
Haochuan Jiang ◽  
...  

2012 ◽  
Vol 522 ◽  
pp. 33-35 ◽  
Author(s):  
J.W. Sun ◽  
V. Jokubavicius ◽  
R. Liljedahl ◽  
R. Yakimova ◽  
S. Juillaguet ◽  
...  

2020 ◽  
Vol 227 ◽  
pp. 117559
Author(s):  
Lei Han ◽  
Jun Song ◽  
Weizhen Liu ◽  
Zongliang Xiao ◽  
Liaolin Zhang ◽  
...  