Co-substitution in Ca1−xYxAl12−xMgxO19phosphors: local structure evolution, photoluminescence tuning and application for plant growth LEDs

2018 ◽  
Vol 6 (15) ◽  
pp. 4217-4224 ◽  
Author(s):  
Yinjian Zheng ◽  
Haiming Zhang ◽  
Haoran Zhang ◽  
Zhiguo Xia ◽  
Yingliang Liu ◽  
...  

Compounds prepared using a high-temperature solid-state reaction method exhibit red to far-red emission under UV excitation. Therefore, these compounds have potential as supplemental or sole-source lighting systems for plant growth.

2015 ◽  
Vol 3 (27) ◽  
pp. 7096-7104 ◽  
Author(s):  
Kai Li ◽  
Mengmeng Shang ◽  
Yang Zhang ◽  
Jian Fan ◽  
Hongzhou Lian ◽  
...  

A series of Ca9Bi(PO4)7:Ce3+,Tb3+,Mn2+phosphors synthesizedviathe high-temperature solid-state reaction method can emit intense tunable color from purple-blue to red including white under UV excitation, which shows their potential application in UV-pumped white-light-emitting diodes.


2015 ◽  
Vol 3 (24) ◽  
pp. 6341-6349 ◽  
Author(s):  
Kai Li ◽  
Ju Xu ◽  
Xuechao Cai ◽  
Jian Fan ◽  
Yang Zhang ◽  
...  

A series of Eu2+-doped α-Ca1.65Sr0.35SiO4 phosphors synthesized via the high-temperature solid-state reaction method can emit intense green light under UV/n-UV excitation, which show potential application in UV/n-UV-pumped white-light-emitting diodes.


2010 ◽  
Vol 105-106 ◽  
pp. 827-829
Author(s):  
Da Wei He ◽  
Xin Rong Zhou ◽  
Yong Sheng Wang

A series of phosphor of (MxMg1-x)2SiO4: Dy3+, Eu3+ (M=Ca, Sr, Ba) were synthesized by high temperature solid-state reaction method and studied. The structure and emission spectrum excited by near violet light were investigated. The excitation spectra of single-doped (MxMg1-x)2SiO4: Dy3+ show strong absorption near 322nm, 347nm, 362nm and 391nm due to 6H15/2→4I9/2, 6H15/2→6P5/2, 6H15/2→4F7/2, 6H15/2→4G11/2 transition of Dy3+. The emission light is at about 469nm, 474nm, 483nm and 494nm under 391nm UV excitation. In order to obtain white light emission, (MxMg1-x)2SiO4: Dy3+, Eu3+ (M=Ca, Sr, Ba) were prepared to enhance the red light emission.


2018 ◽  
Vol 781 ◽  
pp. 36-40
Author(s):  
Olga Dotsenko ◽  
Kirill Frolov ◽  
Dmitry Wagner ◽  
Veronika Dotsenko ◽  
Dmitry Aksentev

In this study, Co0,7Zn1,3W powders were synthesized and investigated at the microwave region. The solid-state reaction method and self-propagating high-temperature synthesis were used to production of the two kinds of hexaferrite powders. The high-frequency magnetic properties under temperature effect have been studied. It is show, that there is a nonlinear dependence on temperature within the 0 – +40 °C temperature range.


2018 ◽  
Vol 6 (41) ◽  
pp. 19967-19973 ◽  
Author(s):  
Zhenyong Cen ◽  
Yu Huan ◽  
Wei Feng ◽  
Yan Yu ◽  
Peiyao Zhao ◽  
...  

Lead-free (1 − x)(0.96K0.46Na0.54Nb0.98Ta0.02O3–0.04Bi0.5(Na0.82K0.18)0.5ZrO3)–xCaZrO3 ((1 − x)(0.96KNNT–0.04BNKZ)–xCZ) piezoelectric ceramics were prepared by the conventional solid-state reaction method.


2020 ◽  
Vol 18 (11) ◽  
pp. 14-18
Author(s):  
Abbas K. Saadon ◽  
Kareem A. Jasim ◽  
Auday H. Shaban

The high temperature superconductor’s compounds are one of the hot spot field of science, due to their applications in industries. Hg0.8Sb0.2Ba2Ca2Cu3O8+δ and Hg0.8Sb0.2Ba2Ca1Cu2O6+δ, were manufactured using a doable-step of solid state reaction method. The samples were sintered at 800 ° C. The transition temperatures Tc are found from electrically resistively by using four probe techniques. The resistivity become zero when the transition temperature Tc(offset) have 131 and 119 K, and the onset temperature Tc(onset) have 139 K for Hg0.8Sb0.2Ba2Ca2Cu3O8+δ and 132 K for Hg0.8Sb0.2Ba2Ca1Cu2O6+δ. Analysis of X-ray diffraction showed a tetragonal structure with lattice parameters changes for all samples.


RSC Advances ◽  
2014 ◽  
Vol 4 (22) ◽  
pp. 11360-11366 ◽  
Author(s):  
Yahong Jin ◽  
Yihua Hu ◽  
He Duan ◽  
Li Chen ◽  
Xiaojuan Wang

The blue emitting long persistent phosphor (LPP) Li2ZnGeO4 and green emitting LPP Li2ZnGeO4:Mn2+ were newly prepared by a high temperature solid-state reaction method.


RSC Advances ◽  
2017 ◽  
Vol 7 (60) ◽  
pp. 37765-37770 ◽  
Author(s):  
Huanhuan Liu ◽  
Long Yuan ◽  
Hui Qi ◽  
Yanyan Du ◽  
Shan Wang ◽  
...  

Reversible thermochromic inorganic materials of Sm3Fe5O12with different particle sizes have been synthesized by a conventional high temperature solid state reaction method (2.51 μm) and sol–gel method (0.16 μm).


2013 ◽  
Vol 683 ◽  
pp. 3-6
Author(s):  
Jia Yue Sun ◽  
Bing Xue ◽  
Guang Chao Sun ◽  
Dian Peng Cui ◽  
Hai Yan Du

The upconversion (UC) luminescence properties of phosphor Tm3+/Yb3+co-doped Gd2Mo3O9were investigated in detail. Tm3+/Yb3+co-doped Gd2Mo3O9was prepared by solid-state reaction method using Na2CO3as flux and characterized by powder X-ray diffractometry. Under 980nm excitation, Tm3+/Yb3+co-doped Gd2Mo3O9has exhibited a weak red emission near 651nm and strong blue emission at 476nm. Tm3+/Yb3+co-doped Gd2Mo3O9phosphor has been considered as a better candidate in solid-state lighting applications.


RSC Advances ◽  
2016 ◽  
Vol 6 (40) ◽  
pp. 33387-33392 ◽  
Author(s):  
Zhongran Yao ◽  
Ruiqing Chu ◽  
Zhijun Xu ◽  
Jigong Hao ◽  
Guorong Li

Lead-free piezoelectric ceramics with the formula of Sr1−x(Li,Ce)x/2(Na0.5Bi0.5)Bi4Ti5O18 (LCSNBT-x, x = 0.0, 0.1, 0.2, 0.3, 0.4), were prepared by a conventional solid-state reaction method.