Flexible thermistors: pulsed laser-induced liquid-phase sintering of spinel Mn–Co–Ni oxide films on polyethylene terephthalate sheets

2015 ◽  
Vol 3 (15) ◽  
pp. 3809-3816 ◽  
Author(s):  
Tomohiko Nakajima ◽  
Tetsuo Tsuchiya

Flexible Co and Ni doped Mn3O4 spinel oxide thermistors with a high B constant and quick response.

2018 ◽  
Vol 284 ◽  
pp. 127-132
Author(s):  
Evgeniy Georgiyevich Sokolov

Structure formation of diamond-containing composites with Sn-Cu-Co-W binders has been studied within the range of sintering temperatures of 780–820°C. The specimens were obtained by rolling the paste-like mixtures of metallic powders and diamonds on steel substrates, with sintering performed in vacuum. The structure of the sintered specimens was studied by optical metallography, X-ray diffractometry and electron probe microanalysis. Hardness of the materials was identified by Rockwell method (scale B). It has been found that the process of composites sintering is largely affected by oxide films available on the surface of the powders. In order to obtain composites having less than 10% porosity and up to 96–98 HRB hardness, they have to be sintered at the temperature of 820°C which eliminates the oxide films.


Author(s):  
Michael P. Mallamaci ◽  
James Bentley ◽  
C. Barry Carter

Glass-oxide interfaces play important roles in developing the properties of liquid-phase sintered ceramics and glass-ceramic materials. Deposition of glasses in thin-film form on oxide substrates is a potential way to determine the properties of such interfaces directly. Pulsed-laser deposition (PLD) has been successful in growing stoichiometric thin films of multicomponent oxides. Since traditional glasses are multicomponent oxides, there is the potential for PLD to provide a unique method for growing amorphous coatings on ceramics with precise control of the glass composition. Deposition of an anorthite-based (CaAl2Si2O8) glass on single-crystal α-Al2O3 was chosen as a model system to explore the feasibility of PLD for growing glass layers, since anorthite-based glass films are commonly found in the grain boundaries and triple junctions of liquid-phase sintered α-Al2O3 ceramics.Single-crystal (0001) α-Al2O3 substrates in pre-thinned form were used for film depositions. Prethinned substrates were prepared by polishing the side intended for deposition, then dimpling and polishing the opposite side, and finally ion-milling to perforation.


Author(s):  
J. Drennan ◽  
R.H.J. Hannink ◽  
D.R. Clarke ◽  
T.M. Shaw

Magnesia partially stabilised zirconia (Mg-PSZ) ceramics are renowned for their excellent nechanical properties. These are effected by processing conditions and purity of starting materials. It has been previously shown that small additions of strontia (SrO) have the effect of removing the major contaminant, silica (SiO2).The mechanism by which this occurs is not fully understood but the strontia appears to form a very mobile liquid phase at the grain boundaries. As the sintering reaches the final stages the liquid phase is expelled to the surface of the ceramic. A series of experiments, to examine the behaviour of the liquid grain boundary phase, were designed to produce compositional gradients across the ceramic bodies. To achieve this, changes in both silica content and furnace atmosphere were implemented. Analytical electron microscope techniques were used to monitor the form and composition of the phases developed. This paper describes the results of our investigation and the presentation will discuss the work with reference to liquid phase sintering of ceramics in general.


Author(s):  
Mahesh Chandramouli

Magnetization reversal in sintered Fe-Nd-B, a complex, multiphase material, occurs by nucleation and growth of reverse domains making the isolation of the ferromagnetic Fe14Nd2B grains by other nonmagnetic phases crucial. The magnets used in this study were slightly rich in Nd (in comparison to Fe14Nd2B) to promote the formation of Nd-oxides at multigrain junctions and incorporated Dy80Al20 as a liquid phase sintering addition. Dy has been shown to increase the domain wall energy thus making nucleation more difficult while Al is thought to improve the wettability of the Nd-oxide phases.Bulk polished samples were examined in a JEOL 35CF scanning electron microscope (SEM) operated at 30keV equipped with a Be window energy dispersive spectrometer (EDS) detector in order to determine the phase distribution.


1986 ◽  
Vol 47 (C1) ◽  
pp. C1-441-C1-445
Author(s):  
E. KOSTIĆ ◽  
S. J. KISS ◽  
D. CEROVIĆ

2005 ◽  
Vol 96 (2) ◽  
pp. 141-147 ◽  
Author(s):  
Sung-Min Lee ◽  
Suk-Joong L. Kang

ChemInform ◽  
2010 ◽  
Vol 27 (32) ◽  
pp. no-no
Author(s):  
F. K. VAN DIJEN ◽  
E. MAYER

Materials ◽  
2021 ◽  
Vol 14 (14) ◽  
pp. 3790
Author(s):  
Yongzheng Ji ◽  
Tsuyoshi Honma ◽  
Takayuki Komatsu

Sodium super ionic conductor (NASICON)-type Na3Zr2Si2PO12 (NZSP) with the advantages of the high ionic conductivity, stability and safety is one of the most famous solid-state electrolytes. NZSP, however, requires the high sintering temperature about 1200 °C and long sintering time in the conventional solid-state reaction (SSR) method. In this study, the liquid-phase sintering (LPS) method was applied to synthesize NZSP with the use of NaPO3 glass with a low glass transition temperature of 292 °C. The formation of NZSP was confirmed by X-ray diffraction analyses in the samples obtained by the LPS method for the mixture of Na2ZrSi2O7, ZrO2, and NaPO3 glass. The sample sintered at 1000 °C for 10 h exhibited a higher Na+ ion conductivity of 1.81 mS/cm at 100 °C and a lower activation energy of 0.18 eV compared with the samples prepared by the SSR method. It is proposed that a new LPE method is effective for the synthesis of NZSP and the NaPO3 glass has a great contribution to the Na+ diffusion at the grain boundaries.