scholarly journals A method to estimate the temperature coefficient for shear modulus

2005 ◽  
Vol 54 (1) ◽  
pp. 246
Author(s):  
Hua Jing-Song ◽  
Jing Fu-Qian ◽  
Tan Hua ◽  
Zhuo Xian-Ming
1998 ◽  
Vol 554 ◽  
Author(s):  
A. S. Bains ◽  
C. A. Gordon ◽  
A. V. Granato ◽  
R. B. Schwarz

AbstractWe have measured the shear modulus and its temperature dependence of Pd40Ni40P20 using an EMAT technique. The room temperature value of 3.92(1011) d/cm2 is in fair agreement with that of 3.66(1011) d/cm2 given earlier by He and Schwarz, using a resonant ultrasound spectroscopy technique. The relative change with temperature coefficient for T << Tg is 3.4(10−4) K−1. For the heating rate of ∼1 K/min used here, Tg = 565 K compared with a value of 575 K reported earlier. The shear modulus is continuous at Tg , but its temperature coefficient is larger by a factor of 6.5 for T >> Tg. During temperature cycling near but below Tg , irreversible aging effects are found showing that the amorphous state is not an equilibrium state. Near but above Tg, the cycling effects are reversible for time scales of the order of hours but not for time scales of the order of days, showing that metastable equilibrium states have not yet been fully attained. The results are in overall agreement with the predictions of the Interstitialcy Theory.


Alloy Digest ◽  
1960 ◽  
Vol 9 (4) ◽  

Abstract EVANOHM is a nickel-base alloy having low temperature coefficient of resistance and high electrical resistivity. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on joining. Filing Code: Ni-57. Producer or source: Wilbur B. Driver Company.


Alloy Digest ◽  
1989 ◽  
Vol 38 (7) ◽  

Abstract EVANOHM alloy S offers optimum stability and flexibility with regard to both size and required temperature coefficient of resistance. Its extremely low electromotive force vs copper together with its high electrical resistivity are highly desirable properties in a precision resistance wire. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-373. Producer or source: Wilbur B. Driver Company.


Alloy Digest ◽  
1957 ◽  
Vol 6 (8) ◽  

Abstract ISO-ELASTIC is an iron-nickel alloy having low temperature coefficient of the modulus of elasticity. It is suitable for precision instrument springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Fe-14. Producer or source: John Chatillon & Sons.


Alloy Digest ◽  
1970 ◽  
Vol 19 (6) ◽  

Abstract MONEL alloy 401 is a copper-nickel alloy with high electrical resistance and is used primarily in specialized electrical and electronic applications. It has a negligible temperature coefficient of electrical resistance and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: Cu-216. Producer or source: Huntington Alloy Products Division.


Author(s):  
Mark Kimball

Abstract Silicon’s index of refraction has a strong temperature coefficient. This temperature dependence can be used to aid sample thinning procedures used for backside analysis, by providing a noncontact method of measuring absolute sample thickness. It also can remove slope ambiguity while counting interference fringes (used to determine the direction and magnitude of thickness variations across a sample).


Sign in / Sign up

Export Citation Format

Share Document