scholarly journals Adsorption of Metal Clusters on Graphene and Their Effect on the Electrical Conductivity

Author(s):  
Roxana M. Del Castillo ◽  
Luis E. Sansores Cuevas
1992 ◽  
Vol 272 ◽  
Author(s):  
U. Simon ◽  
G. Schmid ◽  
G. Schön

ABSTRACTAll presently published electrical and optical measurements on concentrated ligand stabilized Au55-cluster samples reveal an inter-cluster tunnel-conductivity and indicate the influence of a “quantum-size-effect” (QSE) [1],[2]. However these data do not show any initials for the separation of inter- and possible intracluster effects. In the present Raper electronic intra-cluster Properties such as the electrical “conductivity” of 1nm chemical auantum dots, their relaxation frequencies and the relevant activation enthalpies as well as the respective Properties of pairs of Au55-clusters have been investigated in comparison to diluted clusters and interpreted by means of Impedance Spectroscopy. Furthermore a method to determine the number and the density of states (DOS) in the metal-core from the measuring data by means of very simple quantum-size assumptions is presented, which is compatible with both the SIMIT[3] and the existing cluster models.


Author(s):  
M. A. Listvan ◽  
R. P. Andres

Knowledge of the function and structure of small metal clusters is one goal of research in catalysis. One important experimental parameter is cluster size. Ideally, one would like to produce metal clusters of regulated size in order to characterize size-dependent cluster properties.A source has been developed which is capable of producing microscopic metal clusters of controllable size (in the range 5-500 atoms) This source, the Multiple Expansion Cluster Source, with a Free Jet Deceleration Filter (MECS/FJDF) operates as follows. The bulk metal is heated in an oven to give controlled concentrations of monomer and dimer which were expanded sonically. These metal species were quenched and condensed in He and filtered to produce areosol particles of a controlled size as verified by mass spectrometer measurements. The clusters were caught on pre-mounted, clean carbon films. The grids were then transferred in air for microscopic examination. MECS/FJDF was used to produce two different sizes of silver clusters for this study: nominally Ag6 and Ag50.


Author(s):  
John C. Russ ◽  
Nicholas C. Barbi

The rapid growth of interest in attaching energy-dispersive x-ray analysis systems to transmission electron microscopes has centered largely on microanalysis of biological specimens. These are frequently either embedded in plastic or supported by an organic film, which is of great importance as regards stability under the beam since it provides thermal and electrical conductivity from the specimen to the grid.Unfortunately, the supporting medium also produces continuum x-radiation or Bremsstrahlung, which is added to the x-ray spectrum from the sample. It is not difficult to separate the characteristic peaks from the elements in the specimen from the total continuum background, but sometimes it is also necessary to separate the continuum due to the sample from that due to the support. For instance, it is possible to compute relative elemental concentrations in the sample, without standards, based on the relative net characteristic elemental intensities without regard to background; but to calculate absolute concentration, it is necessary to use the background signal itself as a measure of the total excited specimen mass.


Author(s):  
Klaus-Ruediger Peters ◽  
Samuel A. Green

High magnification imaging of macromolecules on metal coated biological specimens is limited only by wet preparation procedures since recently obtained instrumental resolution allows visualization of topographic structures as smal l as 1-2 nm. Details of such dimensions may be visualized if continuous metal films with a thickness of 2 nm or less are applied. Such thin films give sufficient contrast in TEM as well as in SEM (SE-I image mode). The requisite increase in electrical conductivity for SEM of biological specimens is achieved through the use of ligand mediated wet osmiuum impregnation of the specimen before critical point (CP) drying. A commonly used ligand is thiocarbohvdrazide (TCH), first introduced to TEM for en block staining of lipids and glvcomacromolecules with osmium black. Now TCH is also used for SEM. However, after ligand mediated osinification nonspecific osmium black precipitates were often found obscuring surface details with large diffuse aggregates or with dense particular deposits, 2-20 nm in size. Thus, only low magnification work was considered possible after TCH appl ication.


Polymer News ◽  
2005 ◽  
Vol 30 (9) ◽  
pp. 296-300
Author(s):  
F. Esposito ◽  
V. Casuscelli ◽  
M. V. Volpe ◽  
G. Carotenuto ◽  
L. Nicolais

1991 ◽  
Vol 18 (3) ◽  
pp. 611-627 ◽  
Author(s):  
Marta L. Fiorotto ◽  
William J. Klish

2020 ◽  
Vol 92 (1) ◽  
pp. 10901
Author(s):  
Saloua El Asri ◽  
Hamid Ahamdane ◽  
Lahoucine Hajji ◽  
Mohamed El Hadri ◽  
Moulay Ahmed El Idrissi Raghni ◽  
...  

Forsterite single phase powder Mg2SiO4 was synthesized by sol–gel method alongside with heat treatment, using two different cation alkaline salts MCl as mineralizers (M = Na, K) with various mass percentages (2.5, 5, 7.5, and 10 wt.%). In this work, we report on the effect of the cation type and the added amount of used mineralizer on microstructure and electrical conductivity of Mg2SiO4. The formation of forsterite started at 680–740  °C and at 630–700  °C with KCl and NaCl respectively, as shown by TG-DTA and confirmed by XRD. Furthermore, the Fourier transform infrared (FTIR) transmission spectra indicated bands corresponding to vibrations of forsterite structure. The morphology and elemental composition of sintered ceramics were examined by SEM-EDX analyses, while their densities, which were measured by Archimedes method, increased with addition of both alkaline salts. The electrical measurements were performed by Complex Impedance Spectroscopy. The results showed that electrical conductivity increased with the addition of both mineralizers, which was higher for samples prepared with NaCl than those prepared with KCl.


1980 ◽  
Vol 41 (C5) ◽  
pp. C5-219-C5-222
Author(s):  
J. P. Desfours ◽  
C. Godart ◽  
J. P. Nadai ◽  
A. Mauger ◽  
G. Weill ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document