Ozone Resistance of Natural Rubber Vulcanizates. Part I. Apparatus for Exposure at Low Ozone Concentration

1958 ◽  
Vol 31 (4) ◽  
pp. 866-873
Author(s):  
B. I. C. F. van Pul

Abstract An apparatus is described for evaluating the cracking resistance of rubber specimens exposed under static or dynamic conditions to ozone concentrations between 5 and 50×10−8 ml/ml of air. Ozone concentration is kept constant automatically however much is destroyed at the walls of the cabinet or at the surfaces of the rubber testpieces. Temperature can be regulated between 20° and 100° C.

1958 ◽  
Vol 31 (4) ◽  
pp. 882-895 ◽  
Author(s):  
B. I. C. F. van Pul

Abstract An investigation of the ozone protection given to natural rubber vulcanizates by different accelerators and antioxidants has shown that, of the accelerators investigated, the thiuram derivatives appear to be the best antioxidants, when they are used as vulcanizing agents; of the large number of antioxidants examined. NN′-di-sec-octyl p-phenylene diamine appears to be the best antiozonant. Vulcanizates containing this material showed no cracks after being exposed for 400 hours to an ozone concentration of 25×10−8 ml/ml under static conditions; it was far superior to all other materials examined.


1958 ◽  
Vol 31 (4) ◽  
pp. 874-881 ◽  
Author(s):  
B. I. C. F. van Pul

Abstract Commerical waxes whose melting points, refractive indexes and numbers of side chains are within the ranges described seem likely to give good ozone protection under static conditions. All waxes lead to worse cracking under dynamic conditions than if none had been included and it is clearly better to use no wax if the rubber is likely to be submitted to intermittent stretching.


Author(s):  
An Zhang ◽  
Jinhuang Lin ◽  
Wenhui Chen ◽  
Mingshui Lin ◽  
Chengcheng Lei

Long-term exposure to ozone pollution will cause severe threats to residents’ physical and mental health. Ground-level ozone is the most severe air pollutant in China’s Pearl River Delta Metropolitan Region (PRD). It is of great significance to accurately reveal the spatial–temporal distribution characteristics of ozone pollution exposure patterns. We used the daily maximum 8-h ozone concentration data from PRD’s 55 air quality monitoring stations in 2015 as input data. We used six models of STK and ordinary kriging (OK) for the simulation of ozone concentration. Then we chose a better ozone pollution prediction model to reveal the ozone exposure characteristics of the PRD in 2015. The results show that the Bilonick model (BM) model had the highest simulation precision for ozone in the six models for spatial–temporal kriging (STK) interpolation, and the STK model’s simulation prediction results are significantly better than the OK model. The annual average ozone concentrations in the PRD during 2015 showed a high spatial variation in the north and east and low in the south and west. Ozone concentrations were relatively high in summer and autumn and low in winter and spring. The center of gravity of ozone concentrations tended to migrate to the north and west before moving to the south and then finally migrating to the east. The ozone’s spatial autocorrelation was significant and showed a significant positive correlation, mainly showing high-high clustering and low-low clustering. The type of clustering undergoes temporal migration and conversion over the four seasons, with spatial autocorrelation during winter the most significant.


1959 ◽  
Vol 32 (3) ◽  
pp. 739-747 ◽  
Author(s):  
J. R. Dunn ◽  
J. Scanlan

Abstract The thermal and photochemical aging of extracted dicumyl peroxide-, TMTD (sulfurless)- and santocure-vulcanized rubber, in presence of a number of metal and alkylammonium dithiocarbamates, has been investigated by measurements of stress relaxation. The dithiocarbamates have a considerable protective action upon the degradation of peroxide- and TMTD-vulcanizates, but they accelerate stress decay in santocure-accelerated vulcanizates. The reasons for this behavior are discussed. It is suggested that the excellent aging properties of unextracted TMTD vulcanizates are due to the presence of zinc dimethyldithiocarbamate formed during vulcanization.


Atmosphere ◽  
2021 ◽  
Vol 12 (12) ◽  
pp. 1585
Author(s):  
Xin Zhang ◽  
Chengduo Yuan ◽  
Zibo Zhuang

Aerosols can interact with other meteorological variables in the air via aerosol–radiation or aerosol–cloud interactions (ARIs/ACIs), thus affecting the concentrations of particle pollutants and ozone. The online-coupled model WRF-Chem was applied to simulate the changes in the PM2.5 (particulate matter less than 2.5 μm in aerodynamic diameter) and ozone concentrations that are caused by these mechanisms in China by conducting three parallel sensitivity tests. In each case, availabilities of aerosol–radiation interactions and aerosol–cloud interactions were set differently in order to distinguish each pathway. Partial correlation coefficients were also analyzed using statistical tools. As suggested by the results, the ARIs reduced ground air temperature, wind speed, and planetary boundary height while increasing relative humidity in most places. Consequently, the ozone concentration in the corresponding region declined by 4%, with a rise in the local annual mean PM2.5 concentration by approximately 12 μm/m3. The positive feedback of the PM2.5 concentration via ACIs was also found in some city clusters across China, despite the overall enhancement value via ACIs being merely around a quarter to half that via ARIs. The change in ozone concentration via ACIs exhibited different trends. The ozone concentration level increased via ACIs, which can be attributed to the drier air in the south and the diminished solar radiation that is received in central and northern China. The correlation coefficient suggests that the suppression in the planetary boundary layer is the most significant factor for the increase in PM2.5 followed by the rise in moisture required for hygroscopic growth. Ozone showed a significant correlation with NO2, while oxidation rates and radiation variance were also shown to be vitally important.


2007 ◽  
Vol 80 (5) ◽  
pp. 751-761 ◽  
Author(s):  
Seiichi Kawahara ◽  
Jinta Ukawa ◽  
Junichiro Sakai ◽  
Yoshimasa Yamamoto ◽  
Yoshinobu Isono

Abstract Crosslinking junctions of natural rubber vulcanizates were characterized by high-resolution latex-state 13C-NMR spectroscopy. Vulcanized natural rubber latex was prepared by two methods: i.e., vulcanization of the rubber latex and cryogenic crushing of a rubber sheet vulcanized on a hot press. High-resolution latex-state 13C-NMR spectroscopy was attained even after vulcanization of the rubber latex, as is evident from no background in spectrum and narrow half width of signals independent of vulcanization time. Small signals at 44 ppm and 57 ppm in the aliphatic carbon region were assigned by measurements of both Distortionless Enhancement by Polarization Transfer (DEPT) and Attached Proton Test (APT) to secondary and tertiary carbons of crosslinking points. The assignment was proved by high-resolution solution-state NMR spectroscopy of vulcanized liquid cis-1,4-polyisoprene as a model, in which DEPT, APT, 2-dimensional 1H-1H correlation (H-H COSY), 2-dimensional 1H-13C correlation (H-C COSY) and 2-dimensional heteronuclear multiple bond correlation (HMBC) measurements were applied.


2003 ◽  
Vol 76 (2) ◽  
pp. 334-347 ◽  
Author(s):  
Tarek M. Madkour ◽  
Rasha A. Azzam

Abstract Stress-strain measurements were performed on dry and swollen natural rubber vulcanizates prepared using both sulfur as the crosslinking agent and aromatic-based bound antioxidants acting as a second crosslinking agent. The aromatic-based antioxidants were synthesized and analyzed spectroscopically in order to relate the final behavior of the vulcanizates to the nature of the crosslink characteristics. The anomalous upturn in the modulus values of these networks in response to the imposed stress was shown to persist in the dry as well as the swollen state. Since the swollen elastomeric chains cannot undergo a strain-induced crystallization, the abnormal upturns in the modulus values in an absence of a filler were explained on the basis of the limited extensibility of the short chains of networks prepared using two different crosslinking agents in line with earlier modeling predictions. Remarkably, the swelling experiments revealed the increase in the crosslink density of the networks in the early stages of the thermal oxidative degradation procedure indicating a post-cure of the chemically bound antioxidants to the elastomeric chains, which incidentally corresponds to a maximum in the modulus values of the networks. The rheological and other mechanical properties such as the hardness were shown not to have been affected as a result of the incorporation of the chemically bound antioxidants.