Abstract Objective The study aimed to evaluate the shear bond strength (SBS) of lithium disilicate glass-ceramic (LDGC) and resin cement (RC) using different surface treatments. Materials and Methods LDGC blocks (Vintage LD Press) were prepared, etched with 4.5% hydrofluoric acid, and randomly divided into seven groups (n = 10), depending on the surface treatments. The groups were divided as follows: 1) no surface treatment (control), 2) Silane Primer (KS), 3) Signum Ceramic Bond I (SGI), 4) Signum Ceramic Bond I/Signum Ceramic Bond II (SGI/SGII), 5) experimental silane (EXP), 6) experimental silane/Signum Ceramic Bond II (EXP/SGII), and 7) Experimental/Adper Scotchbond Multi-purpose Adhesive (EXP/ADP). The specimens were cemented to resin composite blocks with resin cement and stored in water at 37 °C for 24 hours. The specimens underwent 5,000 thermal cycles and were subjected to the SBS test. Mode of failure was evaluated under the stereo microscope. Statistical Analysis Data were analyzed with Welch ANOVA and Games-Howell post hoc tests (α = 0.05). Results The highest mean SBS showed in group EXP/ADP (45.49 ± 3.37 MPa); however, this was not significantly different from group EXP/SGII (41.38 ± 2.17 MPa) (p ≥ 0.05). The lowest SBS was shown in the control group (18.36 ± 0.69 MPa). This was not significantly different from group KS (20.17 ± 1.10 MPa) (p ≥ 0.05). Conclusions The different surface treatments significantly affected the SBS value between LDGC and RC. The application of pure silane coupling agent with or without the application of an adhesive improved the SBS value and bond quality.


2019 ◽  
Vol 5 (2) ◽  
pp. 23-27
Author(s):  
K Premnath ◽  
◽  
Nagaranjani Prakash ◽  
Mohammed Ajmal B ◽  
Syed Ahmed Raheel ◽  
...  

2021 ◽  
Vol 24 (3) ◽  
Author(s):  
Amr El-Etreby ◽  
Osama AlShanti ◽  
Gihan El-Nagar

Objective: The present study aimed to evaluate the effect of repressing and different surface treatment protocols on the shear bond strength of lithium disilicate glass-ceramics. Material and Methods: A total of 52 lithium disilicate glass-ceramic discs (IPS emax Press, Ivoclar Vivadent) were fabricated using the heat-press technique. The discs were divided into two groups; group (P): discs fabricated from new e.max ingots (n=26), group (R): discs fabricated from reused e.max buttons (n=26). Each group was subdivided into subgroup (E): discs were etched with hydrofluoric acid (9.5%) (n=13), subgroup (S): discs were air-abraded with 110 µm alumina particles. All specimens were subjected to X-ray Diffraction analysis, Scanning Electron Microscope, Energy Dispersive X-Ray, Thermo-Cycling, and Shear Bond Strength Testing. Results: Repressed Etched subgroup (RE) recorded the statistically highest shear bond strength value, followed by the Pressed Etched subgroup (PE), while the statistically lowest shear bond strength value was recorded for the Pressed Air-Abraded subgroup (PS) and Repressed Air-Abraded subgroup (RS). Conclusion: Repressing the leftover buttons for the construction of new lithium disilicate glass-ceramic restorations has no adverse effect on the bond strength of the resin cement to the ceramic. Hydrofluoric acid surface treatment improves the shear bond strength and durability of resin cement bond to both pressed and repressed lithium disilicate glass-ceramic. Air-abrasion cannot be considered as a reliable surface treatment when bonding to lithium disilicate glass-ceramics. Keywords Heat pressed; Lithium disilicate glass-ceramics; Repressing; Shear bond strength; Surface treatment.


2020 ◽  
Vol 49 ◽  
Author(s):  
Marcos Daniel Septímio LANZA ◽  
Walisson Arthuso VASCONCELLOS ◽  
Giovani Lana Peixoto de MIRANDA ◽  
Rogéli Tibúrcio Ribeiro da Cunha PEIXOTO ◽  
Lincoln Dias LANZA

Abstract Introduction The silanization of the ceramic surface prior to applying the adhesive and/or resinous materials plays an important role in bond strength. Nowadays, a new family of adhesive systems has been introduced into the market, aiming to simplify the technique of adhesive procedures during cementation. Objective To investigate the effectiveness of different bonding agents containing silane and primer on Lithium Disilicate Glass Ceramic (LD) surface by shear bond strength tests. Material and method 130 LD ceramic blocks were included in acrylic resin, polished and washed in ultrasound for 10 minutes. The specimens were divided into 2 groups according to surface treatment: Polished Surface (PS); Hydrofluoric Acid 9.5% - 20s (HF). Each group was divided into 5 subgroups (n = 13) according to bonding agent type: metallic primer containing MDP (ZPrimePlus, Bisco Inc); two traditional silanes (MonobondPlus, IvoclarVivadent / Porcelain Prime, Bisco Inc.); mixture of silane and resin (Kerr Silane, Kerr); mixture of silane and universal adhesive (Single-bond Universal, 3M Espe). The specimens were mounted in a standard device for shear testing (UltradentBonding Assembly), cemented with dual resin cement (RelyX UltimateTM, 3M Espe.) and photo-polymerized for 20s. The samples were tested after 24 hours and 3 months of storage in distilled water at ±36 °C. The data were analyzed by 3-Way Anova and Tukey's test (α = 5%). Result Shear bond strength (SBS) was significantly influenced by surface treatment, bonding agent used and storage (p <0.001). Conclusion Adequate adhesive bond strength to Lithium Disilicate Glass Ceramic can be obtained with traditional silanes, combined with HF acid pretreatment surface.


2019 ◽  
Vol 53 (1) ◽  
pp. 17-27 ◽  
Author(s):  
Blerim Mehmeti ◽  
Jeta Kelmendi ◽  
Donika Iiljazi-Shahiqi ◽  
Bleron Azizi ◽  
Suzana Jakovljevic ◽  
...  

2021 ◽  
Vol 2021 ◽  
pp. 1-7
Author(s):  
Amjad Abu Hasna ◽  
Stephanie Semmelmann ◽  
Fernanda Alves Feitosa ◽  
Danilo De Souza Andrade ◽  
Franklin R Tay ◽  
...  

This study evaluated the effect of different surface treatments on the tensile bond strength between lithium disilicate glass-ceramics, resin cement, and dentin. Fifty truncated cone-shape glass-ceramics were divided into five groups (n = 10): G1, control: 10% hydrofluoric acid (HF); G2, Nd:YAG laser + silane; G3, Sil + Nd:YAG laser; G4, graphite + Nd:YAG laser + Sil; and G5, graphite + Sil + Nd:YAG laser. Fifty human third-molars were cut to cylindrical shape and polished to standardize the bonding surfaces. The glass-ceramic specimens were bonded to dentin with a dual-cured resin cement and stored in distilled water for 24 h at 37ºC. Tensile testing was performed on a universal testing machine (10 Kgf load cell at 1 mm/min) until failure. The bond strength values (mean ± SD) in MPa were G1 (9.4 ± 2.3), G2 (9.7 ± 2.0), G3 (6.7 ± 1.9), G4 (4.6 ± 1.1), and G5 (1.2 ± 0.3). Nd:YAG laser and HF improve the bond strength between lithium disilicate glass-ceramics, resin cement, and dentin. The application of a graphite layer prior to Nd:YAG laser irradiation negatively affects this bonding and presented inferior results.