Poly(norbornene-co-styrene)s were synthesized by the use of anilinonaphthoquinone-ligated nickel complexes [Ni(C10H5O2NAr)(Ph)(PPh3): 1a, Ar = C6H3-2,6-iPr; 1b, Ar = C6H2-2,4,6-Me; 1c, Ar = C6H5] activated with modified methylaluminoxane (MMAO) or B(C6F5)3 in toluene. The effects of the cocatalysts were more significant than those of the nickel complexes, and MMAO gave higher activity than B(C6F5)3. The structural characterizations of the products indicated the formation of statistical norbornene copolymers. An increase of the styrene ratio in feed led to an increase in the incorporated styrene (S) content of the resulting copolymer. The molecular weight of the copolymer decreased with increasing the S ratio in feed at 70 °C. The copolymerization activity, using MMAO as a cocatalyst, decreased with lowering of the temperature from 70 to 0 °C, accompanied by an increase in the molecular weight of the copolymer. The S incorporation up to 59% with Mn of 78,000 was achieved by the 1b-B(C6F5)3 catalytic system. The glass transition temperatures of the norbornene (N)/S copolymers determined by differential scanning calorimetry, decreased from 329 to 128 °C according to the S content.

1982 ◽  
Vol 55 (1) ◽  
pp. 245-252 ◽  
Author(s):  
C. Kow ◽  
M. Morton ◽  
L. J. Fetters ◽  
N. Hadjichristidis

Abstract The glass transition temperatures for a series of high-1,4 linear and star-branched polyisoprenes have been measured by differential scanning calorimetry. The Fox-Flory relation for the linear polyisoprenes was found to be Tg=Tg∞−1.76×104Mn−1. The influence of hydroxyl groups on Tg was also examined for low molecular weight (<2.2×104) polyisoprenes.


2014 ◽  
Vol 881-883 ◽  
pp. 165-168
Author(s):  
Xiang Wang Cui ◽  
Lin Zhang

Two bis (benzimidazoyl) monomers were synthesized, and Poly (N-arylenebenzimidazole ketone) s were prepared by N-C coupling reaction that replaced the NH sites from the bis (benzimidazolyl) derivatives with activated difluorides monomers in sulfolane at 210 °C. All the resulting polymers showed easy solubility compared with traditional polybenzimidazoles. Differential scanning calorimetry and thermogravimetric measurements showed that the polymers had high glass transition temperatures (>240 °C), good thermostability and high decomposition temperatures (>460 °C).


Sign in / Sign up

Export Citation Format

Share Document