Copper-Base Alloys Processed by Rapid Solidification and Ion Implantation

1985 ◽  
Vol 58 ◽  
Author(s):  
J.V. Wood ◽  
C.J. Elvidge ◽  
E. Johnson ◽  
A. Johansen ◽  
L. Sarholt-Kristensen ◽  
...  

ABSTRACTAlloys of Cu-Sn and Cu-B have been processed by both melt spinning and ion implantation. In some instances (eg Cu-Sn alloys) rapidly solidified ribbons have been subjected to further implantation. This paper describes the similarities and differences in structure of materials subjected to a dynamic and contained process. For example in Cu-B alloys (up to 2wt% Boron) extended solubility is found in implanted alloys which is not present to the same degree in rapidly solidified alloys of the same composition. Likewise the range and nature of the reversible martensitic transformation is different in both cases as examined by electron microscopy and differential scanning calorimetry.

2012 ◽  
Vol 1373 ◽  
Author(s):  
G. C. S. Anselmo ◽  
W. B. de Castro ◽  
C. J. de Araújo

ABSTRACTRibbons of the Ni-44.8wt%Ti shape memory alloy are prepared through the melt spinning technique. The study is focused on investigating the effect of the rapid solidification and grain size at characteristic start martensitic (Ms), final martensitic (Mf), start austenite (As) and final austenite (Af) transformation temperatures. Changes on martensitic transformation temperatures in Ti45Ni55 melt spun ribbons are observed as grain size is reduced. Results of optical microscopy and differential scanning calorimetry (DSC) are used to associate grain size with transformation temperatures.


1996 ◽  
Vol 455 ◽  
Author(s):  
J. J. Suñol ◽  
M. T. Clavaguera-Mora ◽  
N. Clavaguera ◽  
T. Pradell

ABSTRACTMechanical alloying and rapid solidification are two important routes to obtain glassy alloys. New Fe-Ni based metal-metalloid (P-Si) alloys prepared by these two different processing routes were studied by differential scanning calorimetry and transmission Mössbauer spectroscopy. Mechanical alloyed samples were prepared with elemental precursors, and different nominal compositions. Rapidly solidified alloys were obtained by melt-spinning. The structural analyses show that, independent of the composition, the materials obtained by mechanical alloying are not completely disordered whereas fully amorphous alloys were obtained by rapid solidification. Consequently, the thermal stability of mechanically alloyed samples is lower than that of the analogous material prepared by rapid solidification. The P/Si ratio controls the magnetic interaction of the glassy ribbons obtained by rapid solidification. The experimental results are discussed in terms of the degree of amorphization and crystallization versus processing route and P/Si ratio content.


2018 ◽  
Vol 930 ◽  
pp. 345-348
Author(s):  
R.L. Soares ◽  
Walman Benicio Castro

Solidification structures and shape memory characteristics of Ni50Ti36Hf14(at.%) alloy ribbons prepared by melt spinning were investigated by means of differential scanning calorimetry and X-ray diffraction. In these experiments particular attention has been paid to change the velocity of cooling wheel from 20 to 40 m/s. Then the cooling rates of ribbons were controlled. The effect of this cooling rate on solidification structures and martensitic transformation behaviors is discussed. When the ribbon is produced at a wheel velocity of 40 m/s in melt spinning, the degree of supercooling becomes high because of its thinner thickness.


2021 ◽  
pp. 095400832110055
Author(s):  
Yang Wang ◽  
Yuhui Zhang ◽  
Yuhan Xu ◽  
Xiucai Liu ◽  
Weihong Guo

The super-tough bio-based nylon was prepared by melt extrusion. In order to improve the compatibility between bio-based nylon and elastomer, the elastomer POE was grafted with maleic anhydride. Scanning Electron Microscopy (SEM) and Thermogravimetric Analysis (TGA) were used to study the compatibility and micro-distribution between super-tough bio-based nylon and toughened elastomers. The results of mechanical strength experiments show that the 20% content of POE-g-MAH has the best toughening effect. After toughening, the toughness of the super-tough nylon was significantly improved. The notched impact strength was 88 kJ/m2 increasing by 1700%, which was in line with the industrial super-tough nylon. X-ray Diffraction (XRD) and Differential Scanning Calorimetry (DSC) were used to study the crystallization behavior of bio-based PA56, and the effect of bio-based PA56 with high crystallinity on mechanical properties was analyzed from the microstructure.


e-Polymers ◽  
2002 ◽  
Vol 2 (1) ◽  
Author(s):  
Andrea Pucci ◽  
Letizia Moretto ◽  
Giacomo Ruggeri ◽  
Francesco Ciardelli

AbstractA new polyethylene-compatible terthiophene chromophore, 5”-thio-(3- butyl)nonyl-2,2’:5’,2”-terthiophene, with melting point lower than 0°C was prepared and used for linear polarizers based on ultra-high-molecular-weight polyethylene (UHMWPE). Differential scanning calorimetry and scanning electron microscopy indicate that the new chromophore is dispersed uniformly in films of UHMWPE obtained by casting from solution. The films show excellent dichroic properties (dichroic ratio 30) at rather low drawing ratio (≈ 20) . Moreover, qualitative agreement is observed with the Ward pseudo-affine deformation scheme.


2008 ◽  
Vol 584-586 ◽  
pp. 127-132 ◽  
Author(s):  
Anastasia E. Sergeeva ◽  
Daria Setman ◽  
Michael Zehetbauer ◽  
Sergey Prokoshkin ◽  
Vladimir V. Stolyarov

The aim of this paper is the investigation of electroplastic deformation (EPD) and subsequent annealing influence on martensitic transformation in the shape memory Ni50.7Ti49.3 alloy. Using differential scanning calorimetry method it was shown that EPD at the low strain stimulates structure relaxation and recovers martensitic transformation in cooling, which is usually suppressed by cold rolling.


2011 ◽  
Vol 04 (04) ◽  
pp. 415-418 ◽  
Author(s):  
K. VALLAL PERUMAN ◽  
S. VINODH KUMAR ◽  
K. PUSHPANATHAN ◽  
M. MAHENDRAN

Ferromagnetic Ni2MnGa nanoparticles were prepared by post milling and annealing method. Differential scanning calorimetry studies confirm absence of martensitic and Curie transformation in the disordered state. It was found that the bulk alloy was annealed into a well-defined 7 M structure at around 1073 K. The residual stress of nanoparticles induced the disordered phase to transform into a NM tetragonal phase through atomic ordering. Thermo hysteresis curve of the 'disordered' powder was linear and revealed very low moment indicative of paramagnetic nature. It is confirmed that the martensitic transformation in nanosized particles is predominantly dependent on the strain and the particles size.


2012 ◽  
Vol 535-537 ◽  
pp. 950-953
Author(s):  
Li Na Bai ◽  
Gui Xing Zheng ◽  
Zhi Jian Duan ◽  
Jian Jun Zhang

The influences of Gd concentration on martensitic transformation and magnetic properties of NiMnIn alloys were investigated by differential scanning calorimetry (DSC) , vibrating sample magnetometry (VSM), X-ray diffraction (XRD) and etc. It is Observed through the experiment: the addition of Gd enhances martensite transition temperature;X-ray diffraction analysis of experimental alloys is revealed that to the mixture is martensite and austenite at room temperature; content of Gd is not proportional to the improvement of magnetic property.


2016 ◽  
Vol 61 (2) ◽  
pp. 1083-1088
Author(s):  
M. Pastuszak ◽  
G. Cieślak ◽  
A. Dobkowska ◽  
J. Mizera ◽  
K.J. Kurzydłowski

Abstract The aim of the present work was to plan and carry out an experiment consisting of amorphization of industrial magnesium alloy WE 43 (Mg - 4 Y - 3 RE - 0.5 Zr) modified by the copper addition. Investigated alloy modified with 20% of copper was rapidly quenched with the use of melt spinning technique. The effects of cooling rate on the structure and properties of the obtained material were extensively analyzed. The structure and phase analysis of samples were examined using X-ray diffraction method (XRD) while the thermal stability of the samples was determined by differential scanning calorimetry (DSC). Microstructure observations were also conducted. The microhardness tests (HV0.02) and corrosion resistance tests were carried out to investigate the properties of the material. Corrosion resistance measurements were held using a typical three-electrode system. As the result of the research, the effect of cooling rate on microstructure and properties of investigated alloy was determined.


2019 ◽  
Vol 953 ◽  
pp. 209-214
Author(s):  
Yi Teng Zhang ◽  
Lian Zuo ◽  
Jin Chao Yang ◽  
Wei Xia Zhao ◽  
Xiang Xiong Zeng

The main objective of this study is to investigate the effect of cementitious capillary crystalline waterproofing (CCCW) material on the water impermeability and microstructure of concrete. The water impermeability of concrete covered with or without CCCW material was tested according to the Chinese standard GB 18445-2012. The results indicate that concretes coated with CCCW material showed much higher water impermeability than blank ones, and the ratio of water impermeability pressure between them reached 275. The samples obtained in various depths of hardened cement paste specimens with or without CCCW coating were analyzed through scanning electron microscopy (SEM) and thermogravimetry-differential scanning calorimetry (TG-DSC), to study the differences in microstructure and hydration products. The results present that after a 28-day standard curing, there were lots of ettringite crystals and CaCO3 formed in the paste in 1 cm from the coating, but the action depth of the CCCW coating could not reach 3 cm. The ettringite and CaCO3 is precipitated in the pore structure of cement matrix and filling the voids, which leads to the significant enhancement in water impermeability.