Cadmium- and indium-doped zinc oxide by combustion synthesis using dopant chloride precursors

2006 ◽  
Vol 21 (12) ◽  
pp. 3234-3241 ◽  
Author(s):  
G. Yogeeswaran ◽  
C.R. Chenthamarakshan ◽  
N.R. de Tacconi ◽  
K. Rajeshwar

Cadmium-doped ZnO was prepared for the first time by combustion synthesis using CdCl2 as a dopant precursor, with zinc nitrate and urea as the combustion mixture. Unlike previous studies of combustion synthesis of ZnO in the presence of an indium nitrate precursor, which resulted in (ZnO)mIn2O3 (m = 3 or 4) compound formation, In-doped ZnO was prepared by combustion synthesis in this study using an InCl3 precursor. The doped samples were compared and contrasted with undoped ZnO using scanning electron microscopy, x-ray powder diffraction, energy-dispersive x-ray analyses, and x-ray photoelectron spectroscopy. Diffuse reflectance spectroscopy showed the optical band gap of ZnO to shrink from 3.14 to 3.07 eV and 3.02 eV on Cd and In doping, respectively. Finally, the doped samples showed an improved photoelectrochemical response relative to undoped ZnO over the wavelength range from ∼300 to ∼450 nm.

2019 ◽  
Vol 3 (1) ◽  
pp. 18 ◽  
Author(s):  
Md. Molla ◽  
Mai Furukawa ◽  
Ikki Tateishi ◽  
Hideyuki Katsumata ◽  
Satoshi Kaneco

Ag-doped ZnO nanocomposites are successfully synthesized at different calcination temperatures and times through a simple, effective, high-yield and low-cost mechanochemical combustion technique. Effects of calcination temperature on the crystallinity and optical properties of Ag/ZnO nanocomposites have been studied by X-ray diffraction (XRD), UV−visible diffuse reflectance spectroscopy (UV-DRS), photoluminescence spectroscopy (PL) and X-ray photoelectron spectroscopy (XPS). The XRD patterns of the synthesized Ag/ZnO exhibit a well-crystalline wurtzite ZnO crystal structure. The grain size of Ag/ZnO nanocomposites is found to be 19 and 46 nm at calcination temperatures of 400 °C and 700 °C, respectively. The maximum absorption in the UV region is obtained for Ag/ZnO nanocomposites synthesized at a calcination temperature of 500 °C for 3 h. The peak position of blue emissions is almost the same for the nanocomposites obtained at 300–700 °C calcination temperatures. The usual band edge emission in the UV is not obtained at 330 nm excitation. Band edge and blue band emissions are observed for the use of low excitation energy at 335–345 nm.


2014 ◽  
Vol 2014 ◽  
pp. 1-8 ◽  
Author(s):  
Xiaowen Zou ◽  
Xiaoli Dong ◽  
Limei Wang ◽  
Hongchao Ma ◽  
Xinxin Zhang ◽  
...  

Herein, Ni doped ZnO-TiO2composites were prepared by facile sol-gel approach and were characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM), UV-visible diffuse reflectance spectroscopy (UV-Vis DRS), X-ray photoelectron spectroscopy (XPS), and photoluminescence spectroscopy (PL). The results indicated that the Ni ions can be incorporated into the lattice of TiO2structure and replace Ti. The introduction of Ni expanded light absorption of TiO2to visible region, increased amount of surface hydroxyl groups and physically adsorbed oxygen (as the electronic scavenges), and then enhanced separation rate of photogenerated carriers. The photodegradation test of reactive brilliant blue (KN-R) under simulated solar light indicated that Ni doped ZnO-TiO2composites have better photocatalytic activities, as compared to those of TiO2and ZnO-TiO2.


Materials ◽  
2021 ◽  
Vol 14 (21) ◽  
pp. 6441
Author(s):  
P. J. Navarro-Gázquez ◽  
M. J. Muñoz-Portero ◽  
E. Blasco-Tamarit ◽  
R. Sánchez-Tovar ◽  
R. M. Fernández-Domene ◽  
...  

In the present work, TiO2/ZnO hybrid nanosponges have been synthesized for the first time. First, TiO2 nanosponges were obtained by anodization under hydrodynamic conditions in a glycerol/water/NH4F electrolyte. Next, in order to achieve the anatase phase of TiO2 and improve its photocatalytic behaviour, the samples were annealed at 450 °C for 1 h. Once the TiO2 nanosponges were synthesized, TiO2/ZnO hybrid nanosponges were obtained by electrodeposition of ZnO on TiO2 nanosponges using different temperatures, times, and concentrations of zinc nitrate (Zn(NO3)2). TiO2/ZnO hybrid nanosponges were used as photoanodes in photoelectrochemical water splitting tests. The results indicate that the photoelectrochemical response improves, in the studied range, by increasing the temperature and the Zn(NO3)2 concentration during the electrodeposition process, obtaining an increase in the photoelectrochemical response of 141% for the TiO2/ZnO hybrid nanosponges electrodeposited at 75 °C with 10 mM Zn(NO3)2 for 15 min. Furthermore, morphological, chemical, and structural characterization was performed by Field Emission Scanning Electron Microscopy (FE-SEM) with Energy Dispersive X-ray spectroscopy (EDX), Raman Confocal Laser Spectroscopy, X-ray Photoelectron Spectroscopy (XPS), and Grazing Incidence X-ray Diffraction (GIXRD).


Separations ◽  
2021 ◽  
Vol 8 (3) ◽  
pp. 25
Author(s):  
Chukwuka Bethel Anucha ◽  
Ilknur Altin ◽  
Emin Bacaksız ◽  
Tayfur Kucukomeroglu ◽  
Masho Hilawie Belay ◽  
...  

Abatement of contaminants of emerging concerns (CECs) in water sources has been widely studied employing TiO2 based heterogeneous photocatalysis. However, low quantum energy yield among other limitations of titania has led to its modification with other semiconductor materials for improved photocatalytic activity. In this work, a 0.05 wt.% CuWO4 over TiO2 was prepared as a powder composite. Each component part synthesized via the sol-gel method for TiO2, and CuWO4 by co-precipitation assisted hydrothermal method from precursor salts, underwent gentle mechanical agitation. Homogenization of the nanopowder precursors was performed by zirconia ball milling for 2 h. The final material was obtained after annealing at 500 °C for 3.5 h. Structural and morphological characterization of the synthesized material has been achieved employing X-ray diffraction (XRD), Fourier transform infra-red (FTIR) spectroscopy, Brunauer–Emmett–Teller (BET) N2 adsorption–desorption analysis, Scanning electron microscopy-coupled Energy dispersive X-ray spectroscopy (SEM-EDS), Transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS), and UV-Vis diffuse reflectance spectroscopy (UV-vis DRS) for optical characterization. The 0.05 wt.% CuWO4-TiO2 catalyst was investigated for its photocatalytic activity over carbamazepine (CBZ), achieving a degradation of almost 100% after 2 h irradiation. A comparison with pure TiO2 prepared under those same conditions was made. The effect of pH, chemical scavengers, H2O2 as well as contaminant ion effects (anions, cations), and humic acid (HA) was investigated, and their related influences on the photocatalyst efficiency towards CBZ degradation highlighted accordingly.


2020 ◽  
Vol 2020 ◽  
pp. 1-9 ◽  
Author(s):  
N. Cruz-González ◽  
O. Calzadilla ◽  
J. Roque ◽  
F. Chalé-Lara ◽  
J. K. Olarte ◽  
...  

In the last decade, the urgent need to environmental protection has promoted the development of new materials with potential applications to remediate air and polluted water. In this work, the effect of the TiO2 thin layer over MoS2 material in photocatalytic activity is reported. We prepared different heterostructures, using a combination of electrospinning, solvothermal, and spin-coating techniques. The properties of the samples were analyzed by scanning electron microscopy (SEM), transmission electron microscopy (TEM), atomic force microscopy (AFM), X-ray diffraction (XRD), nitrogen adsorption-desorption isotherms, UV-Vis diffuse reflectance spectroscopy (UV-Vis-DRS), and X-ray photoelectron spectroscopy (XPS). The adsorption and photocatalytic activity were evaluated by discoloration of rhodamine B solution. The TiO2-MoS2/TiO2 heterostructure presented three optical absorption edges at 1.3 eV, 2.28 eV, and 3.23 eV. The high adsorption capacity of MoS2 was eliminated with the addition of TiO2 thin film. The samples show high photocatalytic activity in the visible-IR light spectrum.


2016 ◽  
Vol 2016 ◽  
pp. 1-10 ◽  
Author(s):  
Huang Liu ◽  
Yanhua Zhang ◽  
Hongtao Yang ◽  
Wei Xiao ◽  
Lanlan Sun

Using the common natural cellulose substance (filter paper) and triblock copolymer (Pluronic P123) micelles as dual templates, porous titania nanotubes with enhanced photocatalytic activity have been successfully synthesized through sol-gel methods. Firstly, P123 micelles were adsorbed onto the surfaces of cellulose nanofibers of filter paper, followed by hydrolysis and condensation of tetrabutyl titanate around these micelles to form titania layer. After calcination to remove the organic templates, hierarchical titania nanotubes with pores in the walls were obtained. The sample was characterized by X-ray diffraction pattern (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), nitrogen adsorption/desorption, Fourier Transform Infrared Spectroscopy (FT-IR), Ultraviolet-Visible Diffuse Reflectance Spectroscopy (UV-Vis DRS), and X-ray photoelectron spectroscopy (XPS). As compared with commercial P25 catalyst, the porous titania nanotubes prepared by this method displayed significantly enhanced photocatalytic activity for degrading methyl orange under UV irradiation. Within 10 minutes, the porous titania nanotubes are able to degrade over 70% of the original MO, while the value for the commercial Degussa P25 is only about 33%.


2011 ◽  
Vol 268-270 ◽  
pp. 356-359 ◽  
Author(s):  
Wen Song Lin ◽  
C. H. Wen ◽  
Liang He

Mn, Fe doped ZnO powders (Zn0.95-xMnxFe0.05O2, x≤0.05) were synthesized by an ameliorated sol-gel method, using Zn(CH3COO)2, Mn(CH3COO)2and FeCl2as the raw materials, with the addition of vitamin C as a kind of chemical reducer. The resulting powder was subsequently compacted under pressure of 10 MPa at the temperature of 873K in vacuum. The crystal structure and magnetic properties of Zn0.95-xMnxFe0.05O2powder and bulk samples have been investigated by X-ray diffraction (XRD) and vibrating sample magnetometer (VSM). X-ray photoelectron spectroscopy (XPS) was used to study chemical valence of manganese, iron and zinc in the samples. The x-ray diffraction (XRD) results showed that Zn0.95-xMnxFe0.05O (x≤0.05) samples were single phase with the ZnO-like wurtzite structure. No secondary phase was found in the XRD spectrum. X-ray photoelectron spectroscopy (XPS) showed that Fe and Mn existed in Zn0.95-xMnxFe0.05O2samples in Fe2+and Mn2+states. The results of VSM experiment proved the room temperature ferromagnetic properties (RTFP) of Mn, Fe co-doped ZnO samples.


2012 ◽  
Vol 2012 ◽  
pp. 1-12 ◽  
Author(s):  
Jiang Zhang ◽  
Zheng-Hong Huang ◽  
Yong Xu ◽  
Feiyu Kang

The iodine-doped Bi2WO6(I-BWO) photocatalyst was prepared via a hydrothermal method using potassium iodide as the source of iodine. The samples were characterized by X-ray diffraction (XRD), scanning electron microscope (SEM), transmission electron microscopy (TEM) and selected area electron diffraction (SAED), X-ray photoelectron spectroscopy (XPS), UV-vis diffuse reflectance spectroscopy (DRS), and photoluminescence (PL) spectroscopy. The photocatalytic activity of I-BWO for the degradation of rhodamine B (RhB) was higher than that of pure BWO and I2-BWO regardless of visible light (>420 nm) or ultraviolet light (<400 nm) irradiation. The results of DRS analysis showed that the I-BWO and I2-BWO catalysts had narrower band gaps. XPS analysis proved that the multivalent iodine species including I0and were coadsorbed on the defect surface of Bi2WO6in I-BWO. The enhanced PL intensity revealed that a large number of defects of oxygen vacancies were formed by the doping of iodine. The enhanced photocatalytic activity of I-BWO for degradation of RhB was caused by the synergetic effect of a small crystalline size, a narrow band gap, and plenty of oxygen vacancies.


Materials ◽  
2019 ◽  
Vol 12 (8) ◽  
pp. 1282 ◽  
Author(s):  
Zhao ◽  
Li ◽  
Ai ◽  
Wen

A kind of devices Pt/Ag/ZnO:Li/Pt/Ti with high resistive switching behaviors were prepared on a SiO2/Si substrate by using magnetron sputtering method and mask technology, composed of a bottom electrode (BE) of Pt/Ti, a resistive switching layer of ZnO:Li thin film and a top electrode (TE) of Pt/Ag. To determine the crystal lattice structure and the Li-doped concentration in the resulted ZnO thin films, X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) tests were carried out. Resistive switching behaviors of the devices with different thicknesses of Li-doped ZnO thin films were studied at different set and reset voltages based on analog and digital resistive switching characteristics. At room temperature, the fabricated devices represent stable bipolar resistive switching behaviors with a low set voltage, a high switching current ratio and a long retention up to 104 s. In addition, the device can sustain an excellent endurance more than 103 cycles at an applied pulse voltage. The mechanism on how the thicknesses of the Li-doped ZnO thin films affect the resistive switching behaviors was investigated by installing conduction mechanism models. This study provides a new strategy for fabricating the resistive random access memory (ReRAM) device used in practice.