Test Methods for Chemical Analysis of Cast Iron--All Types

2018 ◽  
Author(s):  
2013 ◽  
Vol 13 (2) ◽  
pp. 53-58 ◽  
Author(s):  
A. Janus ◽  
A. Kurzawa

Abstract Determined was quantitative effect of nickel equivalent value on austenite decomposition degree during cooling-down castings of Ni-Mn- Cu cast iron. Chemical composition of the alloy was 1.8 to 5.0 % C, 1.3 to 3.0 % Si, 3.1 to 7.7 % Ni, 0.4 to 6.3 % Mn, 0.1 to 4.9 % Cu, 0.14 to 0.16 % P and 0.03 to 0.04 % S. Analysed were castings with representative wall thickness 10, 15 and 20 mm. Scope of the examination comprised chemical analysis (including WDS), microscopic observations (optical and scanning microscopy, image analyser), as well as Brinell hardness and HV microhardness measurements of structural components.