Die Design Optimization in Explosive Deep Drawing Process

2015 ◽  
Vol 3 (1) ◽  
pp. 28-32
Author(s):  
Peyman Karampour ◽  
Ali Jabbari
2014 ◽  
Vol 2 (3) ◽  
pp. 212-214
Author(s):  
Ali Jabbari ◽  
Sajjad Kiani ◽  
Mahdi Rasafchi

Metals ◽  
2020 ◽  
Vol 10 (7) ◽  
pp. 870 ◽  
Author(s):  
Wiriyakorn Phanitwong ◽  
Sutasn Thipprakmas

As a major sheet metal process for fabricating cup or box shapes, the deep drawing process is commonly applied in various industrial fields, such as those involving the manufacture of household utensils, medical equipment, electronics, and automobile parts. The limiting drawing ratio (LDR) is the main barrier to increasing the formability and production rate as well as to decrease production cost and time. In the present research, the multi draw radius (MDR) die was proposed to increase LDR. The finite element method (FEM) was used as a tool to illustrate the principle of MDR based on material flow. The results revealed that MDR die could reduce the non-axisymmetric material flow on flange and the asymmetry of the flange during the deep drawing process. Based on this material flow characteristic, the cup wall stretching and fracture could be delayed. Furthermore, the cup wall thicknesses of the deep drawn parts obtained by MDR die application were more uniform in each direction along the plane, at 45°, and at 90° to the rolling direction than those obtained by conventional die application. In the present research, a proper design for the MDR was suggested to achieve functionality of the MDR die as related to each direction along the plane, at 45°, and at 90° to the rolling direction. The larger draw radius positioned for at 45° to the rolling direction and the smaller draw radius positioned for along the plane and at 90° to the rolling direction were recommended. Therefore, by using proper MDR die application, the drawing ratio could be increased to be 2.75, an increase in LDR of approximately 22.22%.


2013 ◽  
Vol 1 (2) ◽  
pp. 20-29 ◽  
Author(s):  
H. Zein ◽  
M. El-Sherbiny ◽  
M. Abd-Rabou ◽  
M. El Shazly

Materials ◽  
2021 ◽  
Vol 14 (14) ◽  
pp. 3993
Author(s):  
Thanh Trung Do ◽  
Pham Son Minh ◽  
Nhan Le

The formability of the drawn part in the deep drawing process depends not only on the material properties, but also on the equipment used, metal flow control and tool parameters. The most common defects can be the thickening, stretching and splitting. However, the optimization of tools including the die and punch parameters leads to a reduction of the defects and improves the quality of the products. In this paper, the formability of the camera cover by aluminum alloy A1050 in the deep drawing process was examined relating to the tool geometry parameters based on numerical and experimental analyses. The results showed that the thickness was the smallest and the stress was the highest at one of the bottom corners where the biaxial stretching was the predominant mode of deformation. The problems of the thickening at the flange area, the stretching at the side wall and the splitting at the bottom corners could be prevented when the tool parameters were optimized that related to the thickness and stress. It was clear that the optimal thickness distribution of the camera cover was obtained by the design of tools with the best values—with the die edge radius 10 times, the pocket radius on the bottom of the die 5 times, and the punch nose radius 2.5 times the sheet thickness. Additionally, the quality of the camera cover was improved with a maximum thinning of 25% experimentally, and it was within the suggested maximum allowable thickness reduction of 45% for various industrial applications after optimizing the tool geometry parameters in the deep drawing process.


Author(s):  
Hamidreza Gharehchahi ◽  
Mohammad Javad Kazemzadeh-Parsi ◽  
Ahmad Afsari ◽  
Mehrdad Mohammadi

1993 ◽  
Vol 115 (2) ◽  
pp. 224-229 ◽  
Author(s):  
K. Yamaguchi ◽  
K. Kanayama ◽  
M. H. Parsa ◽  
N. Takakura

A new deep drawing process of sheet metals is developed to facilitate small-lot production of deep cups with large drawing ratio. In this process, unlike the conventional deep drawing method, a few drawn cups are always stacked on the punch and used as a part of punch for the subsequent deep drawing of a given blank. Before drawing a new blank, a drawn cup which is in contact with the punch is stripped off. The repetition of such stripping and drawing operations makes it possible to carry out both the first-stage drawing and the subsequent slight redrawings in one drawing operation using only one pair of punch and die. In this paper, this new deep drawing process is applied to the production of tapered cups and the main feature of the process is shown.