scholarly journals In Situ Low-Temperature Chemical Bath Deposition of CdS Thin Films without Thickness Limitation: Structural and Optical Properties

2018 ◽  
Vol 2018 ◽  
pp. 1-12 ◽  
Author(s):  
Mouad Ouafi ◽  
Boujemaâ Jaber ◽  
Lahoucine Atourki ◽  
Najwa Zayyoun ◽  
Ahmed Ihlal ◽  
...  

In this work, thin CdS films have been deposited using the chemical bath deposition technique (CBD). Different synthesis parameters, such as number of runs, deposition time, and postannealing temperature, are studied and optimized in order to avoid the supersaturation phenomenon and to achieve a low-temperature growth. CdS thin films, of cubic structure, oriented along the (111) direction with homogenous and smooth surface, have been deposited by using the CBD growth process without any annealing treatment. Based on a set of experimental observations, we show that the solution saturation phenomenon can be avoided if the deposition is performed in several runs at a short deposition time. Throughout the CBD technique, it is then possible not only to overcome any film thickness limitation but also to grow the CdS films in a single technological step at a low temperature and without any postdeposition annealing treatment. CdS films with excellent structural quality and a controllable thickness are obtained when the deposition bath temperature is fixed at 65°C. In addition, deposited films exhibit an optical transmittance ranging from 70 to 95% depending on the synthesis parameters, with band gap energy around 2.42 eV. The process developed in this work might be useful for depositing CdS films on flexible substrates.

2009 ◽  
Vol 609 ◽  
pp. 243-247 ◽  
Author(s):  
H. Moualkia ◽  
S. Hariech ◽  
M.S. Aida

The present work deals with the preparation and characterization of cadmium sulfur (CdS) thin films. These films are prepared by chemical bath deposition on the well cleaned glass substrates. The thickness of the samples was measured by using profilometer DEKTAK, structural and optical properties were studied by X-ray diffraction analysis, and UV-visible spectrophotometry. The optical properties of the films have been investigated as a function of temperature. The band gap energy and Urbach energy were also investigated as a function of temperature. From the transmittance data analysis the direct band gap ranges from 2.21 eV to 2.34 eV. A dependence of band gap on temperature has been observed and the possible raisons are discussed. Transmission spectra indicates a high transmission coefficient (75 %). Structural analysis revealed that the films showed cubic structure, and the crystallite size decreased at a higher deposition temperature.


2017 ◽  
Vol 110 ◽  
pp. 202-209 ◽  
Author(s):  
Sachin Rondiya ◽  
Avinash Rokade ◽  
Bharat Gabhale ◽  
Subhash Pandharkar ◽  
Madhavi Chaudhari ◽  
...  

1996 ◽  
Vol 426 ◽  
Author(s):  
Yuming Zhu ◽  
Dull Mao ◽  
D. L. Williamson ◽  
J. U. Trefny

AbstractChemical-bath-deposited CdS thin films from an ammonia-thiourea solution have been studied by x-ray diffraction, surface profilometry, ellipsometry, and other techniques. The compactness of the CdS films, structural properties of the films, and the growth mechanism have been investigated. For the deposition conditions used, we found that the film compactness reaches its maximum at a deposition time of 35 minutes. Films grown at longer deposition times are less compact, consistent with the CdS duplex layer structure proposed previously. This transition from compact layer growth to porous layer growth is important for depositing CdS films in solar cell applications. Based on x-ray diffraction (XRD) studies, we were able to determine the crystal phase, lattice constant, and other structural properties.


Author(s):  
Fatma Salamon

CdS thin films were prepared by chemical bath deposition technique (CBD) onto the glass substrates at different conditions of preparation. The obtained samples are studied by X-Ray diffraction (XRD). The XRD patterns of CdS samples revealed the formation with a hexagonal crystal structure P36mc, and the clear effect of the concentration of thiourea, cadmium sulfide, NaOH, time and temperature deposition, and annealing temperature, on the structure of the prepared thin films. through the study, we found that the samples have preferred orientation along [002], also the thickness of thin films decrease with deposition time after certain value, with the appearance of free cadmium. It has been found that the 200°C is the best temperature for annealing to improve the other structural and physical properties of films.