Communication—Monitoring the Average Molecular Weight of Polyethylene Glycol in an Acidic Cu Plating Bath

2016 ◽  
Vol 163 (14) ◽  
pp. D747-D749 ◽  
Author(s):  
Seunghoe Choe ◽  
Myung Jun Kim ◽  
Taeho Lim ◽  
Yu Seok Ham ◽  
Soo-Kil Kim ◽  
...  
2016 ◽  
Vol 19 (4) ◽  
pp. 58-65
Author(s):  
Ha Thi Thai La

In this research, the PLA-diol were synthesized from lactic acid (LA) and 1.4 butanediols (BD) with a tin octoate Sn(Oct)2 catalyst at a temperature of 180 °C and the pressure 5 mmHg. The structure and properties of PLA-diol are analyzed by the following methods: GPC, 1H-NMR and DSC. As a result, with the change in the content of Sn (Oct)2 from 0.1 to 1.0%, the molecular weight Mn of PLA - diol increased gradually from 4.119,2 to 7.359,6 g / mol . In addition, the BD content increased from 2.0% to 5.0%, the average molecular weight of the product decreased gradually from 7.536,9 g / mol to 4.735 g / mol, respectively. This change will affect the ability to use PLA-diol in the next denaturation research to apply in the field of biodegradable polymer such as copolymer with polyurethane, copolymer with polyethylene glycol diacid, or chain extension with other polymer in a chain reaction,...


Author(s):  
C. E. Cluthe ◽  
G. G. Cocks

Aqueous solutions of a 1 weight-per cent poly (ethylene oxide) (PEO) were degassed under vacuum, transferred to a parallel plate viscometer under a nitrogen gas blanket, and exposed to Co60 gamma radiation. The Co60 source was rated at 4000 curies, and the dose ratewas 3.8x105 rads/hr. The poly (ethylene oxide) employed in the irradiations had an initial viscosity average molecular weight of 2.1 x 106.The solutions were gelled by a free radical reaction with dosages ranging from 5x104 rads to 4.8x106 rads.


Sign in / Sign up

Export Citation Format

Share Document