Direct Selective Laser Sintering of WC-Co Cemented Carbide by Premixing of Additives

Author(s):  
Hideki Kyogoku ◽  
Takeshi Uemori ◽  
Akihiko Ikuta ◽  
Kenichi Yoshikawa ◽  
Hitoshi Ohmori

In this study, the fabrication conditions of WC cemented carbides by direct selective laser melting were investigated. The effects of additives, such as Co, Cu-20%Sn and Cu powders, and laser scanning conditions on laser sintering process were examined to fabricate a sound laser-scanned body of WC cemented carbides. The optimum laser power, scan speed and scan pitch were found out by experiments. It was found that the continuously smooth single-scan track can be obtained at a lower laser power and a higher scan speed by the addition of 30% Cu powder. The smooth surface of the laser-scanned body could be fabricated at a laser power of 9 W, a scan speed of 20 mm/s and a scan pitch of 0.05 mm.

Author(s):  
M M Savalani ◽  
L Hao ◽  
Y Zhang ◽  
K E Tanner ◽  
R A Harris

Hydroxyapatite, a ceramic with which natural bone inherently bonds, has been incorporated into a polymer matrix to enhance the bioactivity of implant materials. In order to manufacture custom-made bioactive implants rapidly, selective laser sintering has been investigated to fabricate hydroxyapatite and polyamide composites and their properties investigated. One objective of this research was to identify the maximum hydroxyapatite content that could be incorporated into the matrix, which was sintered at various parameters. The study focused on investigating the control of porosity and pore size of the matrix by manipulating the selective laser sintering parameters of the laser power and laser scan speed. The interception method was used to analyse the internal porous morphology of the matrices which were cross-sectioned through the vertical plane. Most notably, all structures built demonstrated interconnection and penetration throughout the matrix. Liquid displacement was also used to analyse the porosity of the matrices. The laser power showed a negative relationship between porosity and variation in parameter values until a critical power value was reached. However, the same relationship for laser scan speed matrices was inconsistent. The effects of the laser power and laser scanning speed on the features of porous structures that could influence cell spreading, proliferation, and bone regeneration are presented.


Author(s):  
Diego Augusto de Moraes ◽  
Aleksander Czekanski

Selective Laser Melting (SLM) process is a Powder Bed Fusion (PBF) technique, which has shown significantly growth in the recent years. The demand for this process is justified by the versatility and ease in manufacturing the parts from 3D models as well for the increased complexity of engineered parts generated from topology or shape optimization. Automotive, aerospace, medical and aviation industries are taking great advantage of this process due the unique geometry characteristics found in the components. To enhance the benefits of SLM, a vital task is to analyze the laser power input impact on the temperature distribution through the powder bed, important for posterior residual stresses analysis. The Finite Element Method proposed in this study is a transient thermal model, able to predict temperature distribution through different sections of the powder bed when performing a single track of the laser scanning. Furthermore, the impact of the laser power input is carried out utilizing SS 304L, a low cost Stainless Steel alloy that can be employed in the SLM process, in order to determine the influence on the temperature distribution along the different cross sections.


2019 ◽  
Vol 31 (2) ◽  
pp. 022306 ◽  
Author(s):  
Wei Lin ◽  
Denise Albertazzi Gonçalves ◽  
Adriano de Souza Pinto Pereira ◽  
Milton Pereira ◽  
Walter Lindolfo Weingaertner

2020 ◽  
Vol 861 ◽  
pp. 77-82
Author(s):  
Gan Li ◽  
Cheng Guo ◽  
Wen Feng Guo ◽  
Hong Xing Lu ◽  
Lin Ju Wen ◽  
...  

This study investigated the effect of laser power (P), scan speed (v) and hatch space (h) on densification behavior, surface quality and hardness of 18Ni300 maraging steel fabricated by selective laser melting (SLM). The results indicated that the relative density of the SLMed samples has a shape increase from 73% to 97% with the laser energy density increasing from 0.5 to 2.2 J/mm2. The relative density ≥ 99% was achieved at the energy density in the range of 2.2~5.9 J/mm2. The optimum process parameters were found to be laser power of 150~200 W, scan speed of 600mm/s and hatch space of 0.105mm. In addition, it was found that the hardness increased initially with the increasing relative density up to relative density of 90% and then little relationship, but finally increase again significantly. This work provides reference for determining process parameters for SLMed maraging steel and the development of 3D printing of die steels.


Author(s):  
Miranda Fateri ◽  
Andreas Gebhardt ◽  
Maziar Khosravi

Selective Laser Melting (SLM) is a powder based Additive manufacturing (AM) technology which builds an object layer wise using a laser beam to melt the powder on an elevated platform. Thus far numerous studies have investigated lunar manufacturing methods and construction but little is known about applicability of SLM of lunar regolith. As most lunar construction proposals require transportation of essential materials from Earth, using an in-situ manufacturing method with indigenous material would be considerably more economical. Fabrication of parts with SLM using various metals and ceramics has already been presented. As such, the feasibility of using lunar regolith mixture to create functional parts with SLM process is investigated. Variation of process parameters such as laser power, scan speed, and scan strategies is investigated and multiple 3D objects are successfully created and presented.


2010 ◽  
Vol 43 ◽  
pp. 430-433
Author(s):  
Nai Fei Ren ◽  
Pan Wang ◽  
Yan Luo ◽  
Hui Juan Wu

The dimensional accuracy and mechanics properties of parts made by Selective Laser Sintering depend greatly on the sintering process parameters. The influence of process parameters on warping weight of parts sintered by blends of polyamide (PA12) and high density polyethylene (HDPE) was studied. The relationship between the process parameters and the warping height was presented. The surface morphology of the part and uniformity of powder mixed were analyzed by SEM. The optimum parameters of minimum warping height were obtained: preheat temperature 110°C, scan speed 300mm/s, laser power 21W, thickness of single layer 0.2mm.


2020 ◽  
Vol 26 (5) ◽  
pp. 871-879 ◽  
Author(s):  
Haihua Wu ◽  
Junfeng Li ◽  
Zhengying Wei ◽  
Pei Wei

Purpose To fabricate a selective laser melting (SLM)-processed AlSi10Mg part with almost full density and free of any apparent pores, this study aims to investigate the effect of ambient argon pressure and laser scanning speed on the particles splash during the AlSi10Mg powder bed laser melting. Design/methodology/approach Based on the discrete element method (DEM), a 3D model of random distribution of powder particles was established, and the 3D free surface of SLM forming process was dynamically tracked by the volume of fluid, where a Gaussian laser beam acts as the energy source melting the powder bed. Through the numerical simulation and process experimental research, the effect of the applied laser power and scanning speed on the operating laser melting temperature was studied. Findings The process stability has a fundamental role in the porosity formation, which is process-dependent. The effect of the processing conditions on the process stability and the resultant forming defects were clarified. Research limitations/implications The results shows that the pores were the main defects present in the SLM-processed AlSi10Mg sample, which decreases the densification level of the sample. Practical implications The optimal processing parameters (argon pressure of 1,000 Pa, laser power of 180 W, scan speed of 1,000 mm/s, powder layer thickness of 35 µm and hatch spacing of 50 µm ) applied during laser melting can improve the quality of selective laser melting of AlSi10Mg, Social implications It can provide a technological support for 3D printing. Originality/value Based on the analysis of the pore and balling formation mechanisms, the optimal processing parameters have been obtained, which were argon pressure of 1,000 Pa, laser power of 180 W, scan speed of 1,000 mm/s, powder layer thickness of 35 µm and hatch spacing of 50 µm. Then, a near-fully dense sample free of any apparent pores on the cross-sectional microstructure was produced by SLM, wherein the relative density of the as-built samples is larger than 97.5%.


Materials ◽  
2020 ◽  
Vol 13 (17) ◽  
pp. 3720 ◽  
Author(s):  
Tatevik Minasyan ◽  
Sofiya Aydinyan ◽  
Ehsan Toyserkani ◽  
Irina Hussainova

The laser power bed fusion approach has been successfully employed to manufacture Mo(Si,Al)2-based composites through the selective laser melting of a MoSi2-30 wt.% AlSi10Mg mixture for high-temperature structural applications. Composites were manufactured by leveraging the in situ reaction of the components during printing at 150–300 W laser power, 500–1000 mm·s−1 laser scanning speed, and 100–134 J·mm−3 volumetric energy density. Microcomputed tomography scans indicated a negligible induced porosity throughout the specimens. The fully dense Mo(Si1-x,Alx)2-based composites, with hardness exceeding 545 HV1 and low roughness for both the top (horizontal) and side (vertical) surfaces, demonstrated that laser-based additive manufacturing can be exploited to create unique structures containing hexagonal Mo(Si0.67Al0.33)2.