A Preliminary Strain-Based Design Criterion for Pipeline Girth Welds

Author(s):  
Yong-Yi Wang ◽  
David Rudland ◽  
Rudi Denys ◽  
David Horsley

The strain capacity of girth welds containing surface-breaking welding defects is examined through numerical analysis and experimental verification under a PRCI (Pipeline Research Council International) funded project. Some important insights on the various factors affecting the girth weld strain capacity are generated. The defect size is identified as one of the most important factors in determining strain capacity of a girth weld. Other factors, such as the strain hardening rate of the pipe and weld metals, weld strength mismatch, fracture toughness, and weld cap height, can play a significant role if the defect size is within certain limits. It is discovered that the girth weld response to the remotely applied strain may be characterized by a three-region diagram. For a given set of defect size and weld strength mismatch conditions, the crack driving force may be bounded, unbounded, or gradually changing, with respect to the remotely applied strain. A set of parametric equations is developed that allow the computation of allowable strains with the input of defect depth, defect length, CTOD toughness, and weld strength mismatch. The comparison of the developed strain criteria with full-scale bend tests and tensile-loaded CWPs (curved wide plates) shows the criteria are almost always conservative if lower bound CTOD toughness for a given set of welds is used. However, the criteria can significantly underpredict strain capacity of girth welds with short defects. Although defect length correction factors were added to the strain criteria based on the comparison of axisymmetric finite element (FE) results and full-scale bend test results, a more thorough investigation of the effects of defect length on strain capacity is needed. Future investigation that incorporates the finite length defects is expected to greatly reduce the underprediction. The influence of other factors, such as strain hardening rate, should be further quantified.

Author(s):  
Yong-Yi Wang ◽  
Don West ◽  
Douglas Dewar ◽  
Alex McKenzie-Johnson ◽  
Millan Sen

Ground movements, such as landslides and subsidence/settlement, can pose serious threats to pipeline integrity. The consequence of these incidents can be severe. In the absence of systematic integrity management, preventing and predicting incidents related to ground movements can be difficult. A ground movement management program can reduce the potential of those incidents. Some basic concepts and terms relevant to the management of ground movement hazards are introduced first. A ground movement management program may involve a long segment of a pipeline that may have a threat of failure in unknown locations. Identifying such locations and understanding the potential magnitude of the ground movement is often the starting point of a management program. In other cases, management activities may start after an event is known to have occurred. A sample response process is shown to illustrate key considerations and decision points after the evidence of an event is discovered. Such a process can involve fitness-for-service (FFS) assessment when appropriate information is available. The framework and key elements of FFS assessment are explained, including safety factors on strain capacity. The use of FFS assessment is illustrated through the assessment of tensile failure mode. Assessment models are introduced, including key factors affecting the outcome of an assessment. The unique features of girth welds in vintage pipelines are highlighted because the management of such pipelines is a high priority in North America and perhaps in other parts of the worlds. Common practice and appropriate considerations in a pipeline replacement program in areas of potential ground movement are highlighted. It is advisable to replace pipes with pipes of similar strength and stiffness so the strains can be distributed as broadly as possible. The chemical composition of pipe steels and the mechanical properties of the pipes should be such that the possibility of HAZ softening and weld strength undermatching is minimized. In addition, the benefits and cost of using the workmanship flaw acceptance criteria of API 1104 or equivalent standards in making repair and cutout decisions of vintage pipelines should be evaluated against the possible use of FFS assessment procedures. FFS assessment provides a quantifiable performance target which is not available through the workmanship criteria. However, necessary inputs to perform FFS assessment may not be readily available. Ongoing work intended to address some of the gaps is briefly described.


Author(s):  
Yong-Yi Wang ◽  
David Rudland ◽  
David Horsley

An ECA procedure specifically tailored to pipeline girth welds is developed under a PRCI (Pipeline Research Council International) funded project. This procedure of FAD (Failure Assessment Diagram) format incorporates some of the most recent developments in crack driving force, plastic collapse, and effects of weld strength mismatch match. The theoretical framework of this procedure is given in a companion paper. This paper focuses on the experimental verification of the procedure. Some particular issues related to girth weld ECA are discussed first. The experimental database includes both full-scale and wide plate test results. Most of the full-scale data are from pipes of API Grade X70 (483 MPa); a few were X65 (448 MPa) and X60 (414 MPa) grades. The diameter of the pipes ranged from 20 inch (508 mm) to 42 inch (1067 mm). The wide plate test data are taken from a PRCI project performed at the University of Gent. The plates were cut from an X60 36-inch OD 11.6-mm pipe. Surface-breaking defects were artificially introduced from the root side of the girth welds. The plates were loaded to failure in tension after the defects were fatigue pre-cracked. The girth welds had a range of yield stress levels ranging from 20% undermatching to 24% overmatching. In almost all the cases, the newly developed procedure proved conservative as compared to the experimental data. The comparison with the wide plate tests was particularly interesting with its wide range of weld strength mismatch levels. It was demonstrated that the inclusion of the weld strength mismatch in the new procedure improves the consistency and the accuracy of the predictions. It also showed that non-conservative predictions might result if the undermatching welds are not properly accounted for.


Author(s):  
Banglin Liu ◽  
Yong-Yi Wang ◽  
Xiaotong Chen ◽  
David Warman

Abstract The ability to accurately estimate the tensile strain capacity (TSC) of a girth weld is critical to performing strain-based assessment (SBA). A wide range of geometry, material, and loading factors can affect the TSC of a girth weld. Among the influencing factors, an increase in the internal pressure level has been shown to have a detrimental effect on the TSC. The overall influence of internal pressure is usually quantified by a TSC reduction factor, defined as the ratio of the TSC at zero pressure to the lowest TSC typically attained at pressure factors around 0.5–0.6. Here the pressure factor is defined as the ratio of the nominal hoop stress induced by pressure to the yield strength (YS) of the pipe material. A number of numeric and experiment studies have reported a TSC reduction factor of 1.5–2.5. These studies generally focused on strain-based designed pipelines with evenmatching or overmatching welds, minimum heat affected zone (HAZ) softening, and a surface breaking flaw at the weld centerline or the fusion boundary. This paper examines the effects of pipe internal pressure on the TSC of girth welds under the premise of weld strength undermatching and HAZ softening. The interaction of biaxial loading and the local stress concentration at the girth weld region was quantified using full-pipe finite element analysis (FEA). The relationship between TSC and the internal pressure level was obtained under several combinations of weld strength mismatch and HAZ softening. Results from the FEA show that the effects of the internal pressure on the TSC are highly sensitive to the material attributes in the girth weld region. Under less favorable weld strength undermatching and HAZ softening conditions, the traditionally assumed reduction factor or 1.5–2.5 may not be applicable. Further, the location of tensile failure is found to depend on both the weld material attributes and the internal pressure. It is possible for the failure location to shift from pipe body at zero internal pressure to the girth weld at elevated internal pressure levels. The implications of the results for both girth weld qualification and integrity assessment are discussed.


2015 ◽  
Vol 137 (4) ◽  
Author(s):  
Stijn Hertelé ◽  
Rudi Denys ◽  
Anthony Horn ◽  
Koen Van Minnebruggen ◽  
Wim De Waele

A key influence factor in the strain-based assessment of pipeline girth weld flaws is weld strength mismatch. Recent research has led to a framework for tensile strain capacity as a function of weld flow stress (FS) overmatch. This framework is built around three parameters: the strain capacity of an evenmatching weldment, the sensitivity of strain capacity to weld FS overmatch, and the strain capacity at gross section collapse (GSC). A parametric finite element study of curved wide plate (CWP) tests has been performed to identify the influence of various characteristics on each of these three parameters. This paper focuses on flaw depth, tearing resistance of the weld, stress–strain behavior of the base metal, and weld geometry. Influences of these characteristics are mostly found to be limited to one or two of the three framework parameters. A preliminary structure is proposed for equations that further develop the strain capacity framework.


Author(s):  
Doug P. Fairchild ◽  
Svetlana Shafrova ◽  
Huang Tang ◽  
Justin M. Crapps ◽  
Wentao Cheng

There are generally two reasons for conducting full-scale tests (FSTs) for the measurement of pipe or weld strain capacity, (1) to generate data useful in verifying the accuracy of a strain capacity prediction model, or (2) to test materials being considered for use. The former case involves exploring variables important to the scope of the model, while the latter involves project specific materials and girth weld procedures often combined with upper bound cases of weld misalignment. Because the challenge of strain-based design is relatively new, FSTs should be used for both reasons cited above. This paper provides observations, lessons learned, and recommendations regarding full-scale pipe strain capacity tests. This information has been developed through the conduct, witness, or review of 159 FSTs. One of the most important aspects of full-scale testing is the preparation of welded pipe test specimens. It is imperative that the specimens be fabricated with materials of known properties and that all possible measures be taken to limit variations from the intended specimen design. It has been observed that unexpected results are often due to irregularities in pipe material strength, weld strength, weld toughness, or the presence of unintended weld defects in a specimen designed to contain just man-made defects. Post-test fractography and metallurgical examination are very useful in explaining the performance of a FST; therefore, failure analysis is discussed.


2013 ◽  
Vol 135 (6) ◽  
Author(s):  
Stijn Hertelé ◽  
Wim De Waele ◽  
Rudi Denys ◽  
Matthias Verstraete ◽  
Koen Van Minnebruggen ◽  
...  

Weld strength mismatch is a key factor in the strain based assessment of flawed girth welds under tension. A strength overmatching weld shields potential flaws within the weld itself from remotely applied deformations and consequently reduces crack driving force. Although this effect has been recognized for decades, different weld strength overmatch definitions exist, and it is not yet fully established which of those is most relevant to a strain based flaw assessment. In an effort to clarify this unsolved question, the authors have performed a large series of parametric finite element analyses of curved wide plate tests. This paper provides an experimental validation of the model and subsequently discusses representative results. It is found that crack driving force is influenced by the shape of the pipe metals' stress–strain curves, which influences the representativeness of two common mismatch definitions (based on yield strength and on ultimate tensile strength). Effects of strength mismatch on strain capacity of a flawed girth weld are best described on the basis of a flow stress, defined as the average of yield and ultimate tensile strength. Based on the observations, a framework for a new strain capacity equation is proposed.


Author(s):  
Yong-Yi Wang ◽  
Steve Rapp ◽  
David Horsley ◽  
David Warman ◽  
Jim Gianetto

There has been a number of unexpected girth weld failures in newly constructed pipelines. Girth weld failures have also been observed in pre-service hydrostatic testing. Post-incident investigations indicated that the pipes met the requirements of industry standards, such as API 5L. The welds were qualified per accepted industry standards, such as API 1104. The field girth welding was performed, inspected, and accepted per industry standards, such as API 1104. Some of the traditional causes of girth weld failures, such as hydrogen cracks and high-low misalignment, were not a factor in these incidents. This paper starts with a review of the recent girth weld incidents. A few key features of a failed weld and their implications are examined. The characteristics of the recent failures is summarized, and the major contributing factors known to date are given. Some of the options to prevent future failures include (1) changes to the tensile properties of the pipes and enhanced hardenability, (2) welding options aimed at increasing the weld strength and minimizing heat-affected zone (HAZ) softening, and (3) reduction of stresses on girth welds. This paper focuses on the first two options. The trends of chemical composition and tensile properties of linepipe are reviewed. The potential contribution of these trends to the girth weld incidents is examined. Possible changes to the linepipe properties and necessary updates in the testing and qualification requirements of the linepipes are provided. Welding options beneficial to enhanced girth weld strain capacity are discussed. Possible revisions to welding procedure qualification requirements, aimed at achieving a minimum level of strain tolerance/capacity, are proposed. The application of previously developed tools in estimating the propensity of HAZ softening is reviewed.


Author(s):  
Stijn Hertelé ◽  
Wim De Waele ◽  
Rudi Denys ◽  
Matthias Verstraete ◽  
Koen Van Minnebruggen ◽  
...  

Weld strength mismatch is a key factor in the strain based assessment of flawed girth welds under tension. A strength overmatching weld shields potential flaws within the weld itself from remotely applied deformations and consequently reduces crack driving force. Although this effect has been recognized for decades, different weld strength overmatch definitions exist and it is not yet fully established which of those is most relevant to a strain based flaw assessment. In an effort to clarify this unsolved question, the authors have performed a large series of parametric finite element analyses of curved wide plate tests. This paper provides an experimental validation of the model and subsequently discusses representative results. It is found that crack driving force is influenced by the shape of the pipe metals’ stress-strain curves, which influences the representativeness of two common mismatch definitions (based on yield strength and on ultimate tensile strength). It can be concluded from further observations that effects of strength mismatch on strain capacity of a flawed girth weld are best described on the basis of a flow stress, defined as the average of yield and ultimate tensile strength. Based on the observations, a framework for a new strain capacity equation is proposed.


Author(s):  
Stijn Hertelé ◽  
Rudi Denys ◽  
Anthony Horn ◽  
Koen Van Minnebruggen ◽  
Wim De Waele

A key influence factor in the strain-based assessment of pipeline girth weld flaws is weld strength mismatch. Recent research has led to a framework for tensile strain capacity as a function of weld flow stress overmatch. This framework is built around three parameters: the strain capacity of an evenmatching weldment, the sensitivity of strain capacity to weld flow stress overmatch and the strain capacity at gross section collapse. A parametric finite element study of curved wide plate tests has been performed to identify the influence of various characteristics on each of these three parameters. This paper focuses on flaw depth, tearing resistance of the weld, stress-strain behaviour of the base metal, and weld geometry. Influences of these characteristics are mostly found to be limited to one or two of the three framework parameters. A preliminary structure is proposed for equations that further develop the strain capacity framework.


Author(s):  
Fredrick F. Noecker ◽  
Doug Fairchild ◽  
Mike Cook ◽  
Mario Macia ◽  
Wan Kan

The onshore pipeline portion of the Papua New Guinea Liquefied Natural Gas (PNG LNG) project traverses terrain with seismically active faults with potential ground displacements up to four meters. The resulting longitudinal strain demand exceeds 0.5% strain, thereby requiring use of strain-based pipeline design (SBD) technology. This paper discusses the application of previously developed strain-based design methodologies to successfully qualify the PNG LNG pipeline system for a design tensile strain demand up to 3%, and flexibility to increase the design strain demand with additional restrictions on key variables impacting strain capacity at select locations. Key SBD pipeline qualification activities are discussed along with the required project timeline. The first activity is specifying, evaluating and procuring line pipe suitable for strain-based design. SBD line pipe must be strain-age resistant, have excellent longitudinal uniform elongation, and have tightly controlled ultimate tensile strength (UTS) limits to ensure robust girth weld overmatch. The girth welds must exhibit upper shelf fracture toughness, excellent tearing resistance, and have sufficient tensile strength to ensure adequate girth weld strength overmatch. The pipeline qualification effort culminates in full scale pipe strain testing as proof of performance. The specimens for these tests are fabricated with project-specific pipe, girth welds, and pipe fit-up (hi-lo misalignment). The girth welds contain machined flaws in both weld metals and heat affected zones, these flaws being sized consistent with acceptable flaw sizes predicted from analytical models and prior experience. The results of these tests and their significance are described. Efforts to reduce capacity through lowering strain demand are outlined, along with examples of construction challenges the project has successfully faced. Key engineering and project decisions, and lessons learned from this qualification effort are also detailed.


Sign in / Sign up

Export Citation Format

Share Document