scholarly journals Effect of magnesium aluminum silicate glass on the thermal shock resistance of BN matrix composite ceramics

2017 ◽  
Vol 100 (6) ◽  
pp. 2669-2678 ◽  
Author(s):  
Delong Cai ◽  
Dechang Jia ◽  
Zhihua Yang ◽  
Qishuai Zhu ◽  
Vaclav Ocelik ◽  
...  
1978 ◽  
Vol 100 (1) ◽  
pp. 136-139
Author(s):  
J. J. Cleveland ◽  
C. W. Fritsch ◽  
R. N. Kleiner

Thin-wall regenerator cores offer the potential for higher effectiveness than comparable thick-wall cores. The fracture strength of magnesium-aluminum-silicate (MAS) ceramic heat-exchanger cores with wall thickness of 0.083 mm (0.003 in.) and 0.160 mm (0.006 in.) are compared. Thermal shock resistance calculations for these cores are also presented.


2012 ◽  
Vol 455-456 ◽  
pp. 650-654 ◽  
Author(s):  
He Yi Ge ◽  
Jian Ye Liu ◽  
Xian Qin Hou ◽  
Dong Zhi Wang

The physical and mechanical properties of nanometer ZrO2-ZrO2fiber composite ceramics were studied by introduction of ZrO2fiber. ZrO2composite ceramics at different sintering temperature was investigated by porosity and water absorption measurements, flexual strength and thermal shock resistance analysis. Results showed that ZrO2composite ceramics containing 15 wt% ZrO2fiber with sintering temperature of 1650°C exhibited good mechanical properties and thermal shock resistance. The porosity and the water absorption were 8.84% and 1.62%, respectively. The flexual strength was 975 MPa and the thermal shock times reached 31 times. Scanning electron microscope (SEM) was used to analyze the microstructure of ZrO2composite ceramics.


2018 ◽  
Vol 922 ◽  
pp. 62-67
Author(s):  
Ke Zheng Sang ◽  
Fan Wang ◽  
De Jun Zeng ◽  
Hong Wei Li

To reinforce the mullite/Al2O3 composite ceramics through formation of mullite whiskers, the composite ceramics were prepared by pressureless sintering using different AlF3 content. The microstructure, porosity, fracture toughness and thermal shock resistance of the composite ceramics were investigated. The results show that the addition of AlF3 can promote the mullite whisker formations, and the whiskers with the size of 3~10μm in diameter and a length-diameter ratio of 10~15 are obtained by sintering at 1600°C with the AlF3 content of 5wt%. Fracture toughness and thermal shock resistance of the composite ceramics are improved by the formation of mullite whisker. The fracture toughness of 4.79MPa•m1/2 can be obtained, and the 95.18% flexural strength remained after thermal shock.


2017 ◽  
Vol 43 (2) ◽  
pp. 1762-1767 ◽  
Author(s):  
Xiaohong Xu ◽  
Jingwen Li ◽  
Jianfeng Wu ◽  
Zhaohui Tang ◽  
Linlin Chen ◽  
...  

2015 ◽  
Vol 3 (5) ◽  
pp. 2199-2206 ◽  
Author(s):  
Baoxi Zhang ◽  
Xinghong Zhang ◽  
Yunfeng Qiu ◽  
Jiecai Han ◽  
PingAn Hu ◽  
...  

The manipulation of the heat flow in a ceramic matrix composite is of great importance in industrial and academic fields.