High-Temperature Flexural Strength and Thermal Stability of Near Zero Expanding doped Aluminum Titanate Ceramics for Diesel Particulate Filters Applications

2013 ◽  
Vol 11 (4) ◽  
pp. 773-782 ◽  
Author(s):  
Ramanathan Papitha ◽  
Madireddy Buchi Suresh ◽  
Das Dibakar ◽  
Roy Johnson
2016 ◽  
Vol 680 ◽  
pp. 137-140 ◽  
Author(s):  
Hai Jian Li ◽  
Xiao Shuang Shao ◽  
Kai Li ◽  
Zhen Hua Geng ◽  
Ping Wu

The thermal stability of aluminum titanate (AT) ceramics is the main problem that restricted its extensive applications in many fields. In this paper, AT ceramics doped with single or composite additives of MgO, SiO2, mullite were fabricated by solid phase synthesis method. The thermal stability was tested by heated for 50h at 1100°C, and the phases of the samples were tested by X-ray diffraction (XRD) , and the microstructure were tested by SEM. The mechanism of the thermal stability of AT with additive was discussed based on DSC/TGA and electron back scatter diffraction pattern (EBSP). The results show that the adding of composite additives can improve the thermal stability of AT ceramics.


2007 ◽  
Author(s):  
R. S. Ingram-Ogunwumi ◽  
Q. Dong ◽  
T. A. Murrin ◽  
R. Y. Bhargava ◽  
J. L. Warkins ◽  
...  

2005 ◽  
Author(s):  
S. B. Ogunwumi ◽  
P. D. Tepesch ◽  
T. Chapman ◽  
C. J. Warren ◽  
I. M. Melscoet-Chauvel ◽  
...  

Author(s):  
Shiro Fujishiro ◽  
Harold L. Gegel

Ordered-alpha titanium alloys having a DO19 type structure have good potential for high temperature (600°C) applications, due to the thermal stability of the ordered phase and the inherent resistance to recrystallization of these alloys. Five different Ti-Al-Ga alloys consisting of equal atomic percents of aluminum and gallium solute additions up to the stoichiometric composition, Ti3(Al, Ga), were used to study the growth kinetics of the ordered phase and the nature of its interface.The alloys were homogenized in the beta region in a vacuum of about 5×10-7 torr, furnace cooled; reheated in air to 50°C below the alpha transus for hot working. The alloys were subsequently acid cleaned, annealed in vacuo, and cold rolled to about. 050 inch prior to additional homogenization


1996 ◽  
Author(s):  
M A Janney ◽  
D P Stinton ◽  
T M Yonushonis ◽  
A C McDonald ◽  
P D Wiczynski ◽  
...  

2011 ◽  
Vol 45 (16) ◽  
pp. 2623-2629 ◽  
Author(s):  
H. Tente ◽  
P. Gomes ◽  
F. Ferreira ◽  
J.H. Amorim ◽  
P. Cascão ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document