scholarly journals 10,000 h molten salt corrosion testing on IN617, uncoated and aluminide ferritic steels at 580 °C

2020 ◽  
Author(s):  
Alina Agüero ◽  
Pauline Audigié ◽  
Sergio Rodríguez
Energies ◽  
2021 ◽  
Vol 14 (3) ◽  
pp. 543
Author(s):  
Ketan Kumar Sandhi ◽  
Jerzy Szpunar

Nickel superalloy Hastelloy-N, alloy X-750, stainless steel 316 (SS316), and stainless steel 304 (SS304) are among the alloys used in the construction of molten salt reactor (MSR). These alloys were analyzed for their corrosion resistance behavior in molten fluoride salt, a coolant used in MSR reactors with 46.5% LiF+ 11.5% NaF+ 42% KF. The corrosion tests were run at 700 °C for 100 h under the Ar cover gas. After corrosion, significant weight loss was observed in the alloy X750. Weight loss registered in SS316 and SS304 was also high. However, Hastelloy-N gained weight after exposure to molten salt corrosion. This could be attributed to electrochemical plating of corrosion products from other alloys on Hastelloy-N surface. SEM–energy-dispersive X-ray spectroscopy (EDXS) scans of cross-section of alloys revealed maximum corrosion damage to the depth of 250 µm in X750, in contrast to only 20 µm on Hastelloy-N. XPS wide survey scans revealed the presence of Fe, Cr, and Ni elements on the surface of all corroded alloys. In addition, Cr clusters were formed at the triple junctions of grains, as confirmed by SEM–EBSD (Electron Back Scattered Diffraction) analysis. The order of corrosion resistance in FLiNaK environment was X750 < SS316 < SS304 < Hastelloy-N.


2021 ◽  
Vol 1885 (3) ◽  
pp. 032005
Author(s):  
Dandan Men ◽  
Jian Xiong ◽  
Wenyi Peng ◽  
Lingyun Bai

CORROSION ◽  
2001 ◽  
Vol 57 (6) ◽  
pp. 489-496 ◽  
Author(s):  
M. Amaya ◽  
J. Porcayo-Calderon ◽  
L. Martinez

Abstract The performance of Fe-Si coatings and an iron aluminide (FeAl) intermetallic alloy (FeAl40at%+0.1at%B+10vol%Al2O3) in molten salts containing vanadium pentoxide (V2O5) and sodium sulfate (Na2SO4) is reported. Corrosion and fouling by ash deposits containing V2O5 and Na2SO4 are typical corrosion problems in fuel oil-fired electric power units. High-temperature corrosion tests were performed using both electrochemical polarization and immersion techniques. The temperature interval of this study was 600°C to 900°C, and the molten salts were 80wt%V2O5-20wt%Na2SO4. Curves of corrosion current density vs temperature obtained by the potentiodynamic studies are reported, as well as the weight loss vs temperature curves from molten salt immersion tests. Both Fe-Si coatings and FeAl40at%+0.1at%B+10vol%Al2O3 showed good behavior against molten salt corrosion. The final results show the potential of these coatings and alloys to solve the high-temperature corrosion in fuel oil-fired electric power units.


1970 ◽  
Vol 3 (2) ◽  
pp. 77-82 ◽  
Author(s):  
TS Sidhu ◽  
S Prakash ◽  
RD Agrawal

The present study aims to evaluate the hot corrosion behaviour of the Ni-based alloy Superni- 75 in the molten salt environment of Na2SO-60%V2O5 at 900°C under cyclic conditions. The thermogravimetric technique was used to establish the kinetics of corrosion. X-ray diffraction, scanning electron microscopy/energy-dispersive analysis and electron probe microanalysis techniques were used to analyse the corrosion products. Superni-75 has successfully provided the hot corrosion resistance to the given molten salt environment. The hot corrosion resistance of the Superni-75 has been attributed to the formation of uniform, homogeneous and adherent thick layer of the scale consisting mainly of oxides of nickel and chromium, and refractory Ni(VO3)2. These oxides and refractory nickel vanadates have blocked the penetration of oxygen and other corrosive species to the substrate. Keywords: Hot corrosion, nickel-based alloy, superalloy, molten salt environment   DOI: 10.3329/jname.v3i2.922 Journal of Naval Architecture and Marine Engineering 3(2006) 77-82


Author(s):  
Michael W. Usrey ◽  
Yiping Liu ◽  
Mark Anderson ◽  
Jon Lubbers ◽  
Brady Knowles ◽  
...  

Solar power is a sustainable resource which can reduce the power generated by fossil fuels, lowering greenhouse gas emissions and increasing energy independence. The U.S. Department of Energy’s SunShot Initiative has set goals to increase the efficiency of concentrating solar power (CSP) systems. One SunShot effort to help CSP systems exceed 50% efficiency is to make use of high-temperature heat transfer fluids (HTFs) and thermal energy storage (TES) fluids that can increase the temperature of the power cycle up to 1300°C. Sporian has successfully developed high-temperature operable pressure, temperature, thermal flux, strain, and flow sensors for gas path measurements in high-temperature turbine engines. These sensors are based on a combination of polymer derived ceramic (PDC) sensors, advanced high-temperature packaging, and integrated electronics. The overall objective is the beneficial application of these sensors to CSP systems. Through collaboration with CSP industry stakeholders, Sporian has established a full picture of operational, interface, and usage requirements for trough, tower, and dish CSP architectures. In general, sensors should have accurate measurement, good reliability, reasonable cost, and ease of replacement or repair. Sensors in contact with hot salt HTF and TES fluids will experience temperature cycling on a daily basis, and parts of the system may be drained routinely. Some of the major challenges to high-temperature CSP implementation include molten salt corrosion and flow erosion of the sensors. Potential high-temperature sensor types that have been identified as of interest for CSP HTF/TES applications include temperature, pressure, flow, and level sensors. Candidate solar salts include nitrate, carbonate, and chloride, with different application temperatures ranging from 550°C-900°C. Functional ceramics were soaked for 500 hours in molten nitrate, carbonate, and chloride salts, showing excellent corrosion resistance in chloride salts and good resistance in nitrate salts. The demonstration of functional ceramics in relevant HTFs laid the foundation for full prototype sensor and packaging demonstration. Sporian has developed a packaging approach for ceramic-based sensors in various harsh gaseous environments at temperatures up to 1400°C, but several aspects of that packaging are not compatible with corrosive and electrically conductive HTFs. In addition to consulting published literature, a 300 hour soak test in molten chloride salt allowed the authors to identify suitable structural metals and ceramics. Based on discussions with stakeholders, molten salt corrosion testing and room-temperature water flow testing, suitable for CSP sensor/packaging concepts were identified for future development, and initial prototypes have been built and tested.


2019 ◽  
Vol 159 ◽  
pp. 108087 ◽  
Author(s):  
O. Muránsky ◽  
C. Yang ◽  
H. Zhu ◽  
I. Karatchevtseva ◽  
P. Sláma ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document