Phase behavior in thin films of weakly segregated block copolymer/homopolymer blends
Keyword(s):
For P(S-b-MMA)/PS mixtures with ϕPS = 64%, PL exists in thin films annealed at 230–270 °C. For thick films, thermal annealing at 245–270 °C produces both PL and DG of various fractions. PL becomes the only discernible phase in thick films annealed at 230 °C.