Top-seeded solution growth and characterization of Raman crystal LiVMoO6
Keyword(s):
Single crystal LiVMoO6, with dimensions up to 20 mm × 15 mm × 12 mm, has been grown successfully for the first time from a high-temperature solution with MoO3 as a flux.