Effect of Molecular Weight on the Phase Diagram and Thermal Properties of Poly(styrene)/8CB Mixtures

2000 ◽  
Vol 33 (3) ◽  
pp. 960-967 ◽  
Author(s):  
Farida Benmouna ◽  
Abdelylah Daoudi ◽  
Frédérick Roussel ◽  
Laurent Leclercq ◽  
Jean-Marc Buisine ◽  
...  
2021 ◽  
Author(s):  
Carlos Alejandro Rodríguez-Ramírez ◽  
Alain Dufresne ◽  
Norma Beatriz D'Accorso ◽  
Nancy Garcia

Abstract In this work, from an endemic and non-significant value-added bamboo argentine, nanofibrils (CNFs) of 20 nm in width were obtained. These nanofibrils were chemical modified in surface with three simple steps using a noncommercial low molecular weight polylactic acid. The success of modification was confirmed by FTIR, TGA, DSC and XRD analysis. The modified nanofibrils were taken up for changing surface properties in films based on commercial PLA. The results show that dispersive (γ D/S) component of films increase of 34.7 mN/m to 36.1 mN/m after the addition of modified nanofibrils from 2 to 5% in formulation of the films, comparing with a physical blend. Interesting others result in physical, mechanical, and thermal properties of the nanocomposites, were reported.


2018 ◽  
Vol 775 ◽  
pp. 26-31
Author(s):  
Sukantika Manatsittipan ◽  
Kamonthip Kuttiyawong ◽  
Kazuo Ito ◽  
Sunan Tiptipakorn

In this study, the biodegradability and thermal properties the composites of polybutylene succinate (PBS) and chitosan of different molecular weights (Mn = 104,105, and 106 Da) were prepared at chitosan contents of 0-10 wt%. After 10 days of microbial degradation, the results show that the amount of holes from degradation was increased with either decreasing Mn or increasing chitosan contents. However, the size of holes was increased with increasing Mn and chitosan contents. The results from Differential Scanning Calorimeter (DSC) present that the melting temperature (Tm) of PBS was decreased with increasing chitosan contents. Moreover, there was no significant difference between Tm of the composites with different Mn of chitosan. From the TGA thermograms, the decomposition temperature at 10% weight loss (Td10) was decreased with increasing chitosan contents. Moreover, the water absorption of PBS/chitosan composites was increased with increasing Mn and content of chitosan.


2010 ◽  
Vol 147 (3-4) ◽  
pp. 172-179 ◽  
Author(s):  
Simon Bengtsson ◽  
Ana R. Pisco ◽  
Peter Johansson ◽  
Paulo C. Lemos ◽  
Maria A.M. Reis

e-Polymers ◽  
2003 ◽  
Vol 3 (1) ◽  
Author(s):  
Thomas Fey ◽  
Helmut Keul ◽  
Hartwig Höcker

Abstract Alternating poly(ester amide)s 6a - e were prepared by polycondensation of α-carboxyl-ω-hydroxyamides 3a - e which were obtained by aminolysis of glutaric anhydride (1) and α,ω-aminoalcohols, H2N-(CH2)x-OH (x = 2 - 6) 2a - e. The polycondensation was performed in dimethylformamide solution using a carbodiimide as activating agent, or in bulk with Bu2Sn(OMe)2, Ti(OBu)4 and Sn(octoate)2 as a catalyst. For the polycondensation in bulk, the influence of catalyst and of temperature on the number-average molecular weight was studied. 1H NMR analyses of the poly(ester amide)s clearly show the alternating microstructure. The poly(ester amide)s from glutaric anhydride and the homologous series of α,ω-aminoalcohols are semicrystalline materials; their melting points show the odd/even effect observed for other poly(ester amide)s.


Polymers ◽  
2019 ◽  
Vol 11 (3) ◽  
pp. 438 ◽  
Author(s):  
Yosra Chebbi ◽  
Nejib Kasmi ◽  
Mustapha Majdoub ◽  
George Papageorgiou ◽  
Dimitris Achilias ◽  
...  

In this study, the synthesis of poly(ethylene furanoate) (PEF), catalyzed by five different catalysts—antimony acetate (III) (Sb Ac), zirconium (IV) isopropoxide isopropanal (Zr Is Ip), antimony (III) oxide (Sb Ox), zirconium (IV) 2,4-pentanedionate (Zr Pe) and germanium (IV) oxide (Ge Ox)—via an industrially common combination of melt polymerization and subsequent solid-state polymerization (SSP) is presented. In all reactions, proper amounts of 2,5-dimethylfuran-dicarboxylate (DMFD) and ethylene glycol (EG) in a molar ratio of DMFD/EG= 1/2 and 400 ppm of catalyst were used. Polyester samples were subjected to SSP procedure, under vacuum application, at different reaction times (1, 2, 3.5, and 5 h) and temperatures of 190, 200, and 205 °C. Carboxyl end-groups concentration (–COOH), intrinsic viscosity (IV), and thermal properties, via differential scanning calorimetry (DSC), were measured for all resultant polymers to study the effect of the used catalysts on the molecular weight increase of PEF during SSP process. As was expected, it was found that with increasing the SSP time and temperature, the intrinsic viscosity and the average molecular weight of PEF steadily increased. In contrast, the number of carboxyl end-groups content showed the opposite trend as intrinsic viscosity, that is, gradually decreasing during SSP time and temperature increase. It is worthy to note that thanks to the SSP process an obvious and continuous enhancement in the thermal properties of the prepared PEF samples was attained, in which their melting temperatures (Tm) and degree of crystallinity (Xc) increase progressively with increasing of reaction time and temperature. To predict the time evolution of polymers IV, as well as the hydroxyl and carboxyl content of PEF polyesters during the SSP, a simple kinetic model was developed. From both the theoretical simulation results and the experimental measurements, it was demonstrated that surely the Zr Is Ip catalyst shows the best catalytic characteristics compared to all other used catalysts herein, that is, leading in reducing—in a spectacular way—the activation energy of the involved both transesterification and esterification reactions during SSP.


2020 ◽  
Vol 40 (2) ◽  
pp. 136-142 ◽  
Author(s):  
Homa Maleki ◽  
Hossein Barani

AbstractThe stereocomplex formation is a promising method to improve the properties of poly(lactide) (PLA)-based products due to the strong interaction of the side-by-side arrangement of the molecular chains. Recently, electrospinning method has been applied to prepare PLA stereocomplex, which is more convenient. The objective of the current study is to make stereocomplexed PLA nanofibers using electrospinning method and compare their properties and structures with pure poly(l-lactide) (PLLA) fibers. The stereocomplexed fibers were electrospun from a blend solution of high molecular weight PLLA and poly(d-lactide) (1:1 ratio). The morphology of the obtained electrospun fibers was examined by scanning electron microscopy (SEM) and atomic force microscopy (AFM). Differential scanning calorimetry was applied to study their thermal properties and crystallinity. Fourier transform infrared spectroscopy (FTIR) test was conducted on the samples to characterize their chemical properties. The SEM and AFM images indicated that smooth uniform fibers with a cylindrical structure were produced. Besides, the FTIR results and thermal properties confirmed that only stereocomplex crystallites formed in the resulting fibers via the electrospinning method.