Surface Carbon Hydrogenation on Precovered Fe(110) with Spectator-Coverage-Dependent Chain Initiation and Propagation

2019 ◽  
Vol 123 (42) ◽  
pp. 25657-25667 ◽  
Author(s):  
Teng Li ◽  
Xiaodong Wen ◽  
Yong-Wang Li ◽  
Haijun Jiao
Author(s):  
B. A. Dolgoplosk ◽  
K. L. Makovetskii ◽  
E. I. Tinyakova ◽  
T. G. Golenko ◽  
I. A. Oreshkin

1978 ◽  
Vol 20 (4) ◽  
pp. 913-918 ◽  
Author(s):  
V.M. Munikhes ◽  
S.I. Kuzina ◽  
D.P. Kiryukhin ◽  
A.I. Mikhailov ◽  
I.M. Barkalov

2002 ◽  
Vol 719 ◽  
Author(s):  
Myoung-Woon Moon ◽  
Kyang-Ryel Lee ◽  
Jin-Won Chung ◽  
Kyu Hwan Oh

AbstractThe role of imperfections on the initiation and propagation of interface delaminations in compressed thin films has been analyzed using experiments with diamond-like carbon (DLC) films deposited onto glass substrates. The surface topologies and interface separations have been characterized by using the Atomic Force Microscope (AFM) and the Focused Ion Beam (FIB) imaging system. The lengths and amplitudes of numerous imperfections have been measured by AFM and the interface separations characterized on cross sections made with the FIB. Chemical analysis of several sites, performed using Auger Electron Spectroscopy (AES), has revealed the origin of the imperfections. The incidence of buckles has been correlated with the imperfection length.