Enhanced bonding property of cold-sprayed Zn-Al coating on interstitial-free steel substrate with a nanostructured surface layer

2016 ◽  
Vol 385 ◽  
pp. 341-348 ◽  
Author(s):  
Y.L. Liang ◽  
Z.B. Wang ◽  
J. Zhang ◽  
J.B. Zhang ◽  
K. Lu
Metals ◽  
2021 ◽  
Vol 11 (11) ◽  
pp. 1782
Author(s):  
Gui-Qiao Wang ◽  
Yu-Qian Wang ◽  
Rui-Hai Duan ◽  
Guang-Ming Xie

A pure Ni interlayer with a thickness of 0.1 mm was introduced between high-strength interstitial free steel and Al–Mg–Si alloy, which were friction stir lap welded, producing an excellent welded joint. The interface layer consisted of a γ-Ni solid solution, and the mixed stirring zone contained alternate lamellae of γ-Ni and α-Fe solid solutions. The addition of a Ni interlayer strongly suppressed the reaction between Al and Fe because of the atomic arrangement of Ni. Furthermore, the insertion depth of the stirring pin has a significant influence on the Al/steel interfacial reaction. Under shallow insertion depth, the intermetallic compounds of both FeAl and Fe2Al5 were observed at the interface layer. A maximum tensile-shear fracture load of 4.3 kN was achieved, with fractures being present in the steel substrate far away from the Al/steel weld.


Crystals ◽  
2019 ◽  
Vol 9 (11) ◽  
pp. 565 ◽  
Author(s):  
Pan ◽  
Wan ◽  
Wang ◽  
Shen ◽  
Fu ◽  
...  

A Ti bearing interstitial-free steel was finishing rolled in the ferrite region with and without lubrication and microstructures, mechanical properties and textures evolution during warm rolling and subsequent annealing were investigated by OM, SEM, tensile test and ODF. The results show that the surface microstructure of the as-rolled specimen without lubrication is composed of dense shear bands, while the microstructures of the central layer of the as-rolled specimen without lubrication and the whole cross section of the as-rolled specimen with lubrication are elongated ferrite. Short-time annealing can make the non-lubricated rolling sample recrystallize, but the lubricated rolling sample cannot. After complete recrystallization, the microstructure of the surface layer of the as-annealed specimen without lubrication is finer than that of the center layer of the as-annealed specimen without lubrication and the whole section of the as-annealed specimen with lubrication. The mechanical properties of as-annealed sample without lubrication change significantly in the initial annealing stage, while that of as-annealed sample with lubrication remain unchanged until the end stage of annealing. The surface layers of the as-rolled samples have strong Goss component and weak γ fibre components, while the central layers have strong γ fibre components and moderate rotated cubic components. As annealing proceeds, the Goss components of the surface layer decrease and the γ fibre components increase. The rotated cubic components in the central layer are gradually transformed into γ texture.


2021 ◽  
Vol 227 (2) ◽  
pp. 137-152
Author(s):  
S. K. Chandra ◽  
R. Sarkar ◽  
Sukalpa Choudhury ◽  
Mrinmoy Jana ◽  
P. S. De ◽  
...  