Yang Ju

Through-hole anodic aluminum oxide (AAO) was fabricated by two steps anodization method. The pore diameter of the AAO was 40 nm. Cu nanowire array was prepared using the fabricated AAO as a template by electrochemical deposition. The mechanical and electrical performances of Cu nanowire surface fastener (NSF) were realized by the interconnection of Cu nanowire arrays. The shear and normal bonding strengths for the Cu NSF with 40 nm diameter nanowires were 3.38 × 10−3 and 2.46 × 10−3 N/cm2, respectively, and the parasitic resistance of it was approximately 22.5 Ω · cm2.