Effect of deep drawing on the mechanical properties of VT1-0 titanium alloy

1979 ◽  
Vol 15 (10) ◽  
pp. 788-790
Author(s):  
V. S. Dokuchaev ◽  
A. A. Orinova
Alloy Digest ◽  
1999 ◽  
Vol 48 (9) ◽  

Abstract ALZ 305 is an austenitic stainless steel with excellent formability and good corrosion resistance, toughness, and mechanical properties. The higher amount of nickel in this grade enables high deep-drawing deformation without intermediate annealing. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-762. Producer or source: ALZ nv.


2021 ◽  
pp. 130476
Author(s):  
I.P. Mishin ◽  
E.V. Naydenkin ◽  
O.V. Zabudchenko ◽  
A.I. Manisheva ◽  
D.I. Bobrov ◽  
...  

2019 ◽  
Author(s):  
I. P. Mishin ◽  
E. V. Naydenkin ◽  
I. V. Ratochka ◽  
O. N. Lykova ◽  
A. I. Manisheva

2016 ◽  
Vol 849 ◽  
pp. 376-381
Author(s):  
Ming Long Li ◽  
Yu Jie Geng ◽  
Chen Chen ◽  
Shu Jie Pang ◽  
Tao Zhang

The effects of cold-rolling with different reduction ratios of 70%-90% on the microstructure and mechanical properties of Ti50Zr30Nb10Ta10 alloy were investigated. It was found that the β-Ti phase in this alloy was stable under cold-rolling. With the increase in reduction ratio from 70% to 90%, the microstructure of the alloys evolved from deformed dendrite structure to fiber-like structure. The alloy cold-rolled with the reduction ratio of 70% exhibited optimum mechanical properties of combined high fracture strength of 1012 MPa and plastic strain of 10.1%, which are closely correlated with the dendrite structure of the alloy. It is indicated that the proper cold-rolling is an effective way to improve the mechanical properties of the titanium alloy.


1974 ◽  
Vol 6 (6) ◽  
pp. 753-755
Author(s):  
I. I. Kornilov ◽  
A. T. Pronin ◽  
N. A. Vorob'ev ◽  
T. T. Nartova ◽  
L. P. Fatkullina