AbstractTungsten disulfide (WS2) nanotubes (NTs) are examined here as a filler for polylactide (PLA) for their ability to accelerate PLA crystallization and for their promising biocompatibility in relevant to biomedical applications of PLA-WS2 nanocomposites. In this work, we have studied the structural and thermal properties of PLA-WS2 nanocomposite films varying the concentration of WS2 NTs from 0 (neat PLA) to 0.6 wt%. The films were uniaxially drawn at 90 °C and annealed at the same temperature for 3 and 10 min. Using wide angle x-ray scattering, Raman spectroscopy and differential scanning calorimetry, we probed the effects of WS2 NT addition on the structure of the PLA films at various stages of processing (unstretched, stretching, annealing). We found that 0.6 wt% of WS2 induces the same level of crystallinity in as stretched PLA-WS2 as annealing in neat PLA for 10 min. These data provide useful insights into the role of WS2 NTs on the structural evolution of PLA-WS2 composites under uniaxial deformation, and extend their applicability to situations where fine tuning of PLA crystallinity is desirable.


2017 ◽  
Vol 155 ◽  
pp. 680-687 ◽  
Author(s):  
Ramez A. Al-Mansob ◽  
Amiruddin Ismail ◽  
Riza Atiq O.K. Rahmat ◽  
Muhamad Nazri Borhan ◽  
Jamal M.A. Alsharef ◽  
...  

RSC Advances ◽  
2015 ◽  
Vol 5 (42) ◽  
pp. 32909-32919 ◽  
Author(s):  
Siduo Wu ◽  
Guangsu Huang ◽  
Jinrong Wu ◽  
Feng Tian ◽  
Hui Li

A regulated morphology of multi-walled CNT bundles in an olefin block copolymer matrix is achieved via solution blending after sonication. We observed an unexpected inverse evolution trend of long period in nanocomposites compared to that in neat matrix.


2008 ◽  
Vol 81 (5) ◽  
pp. 753-766 ◽  
Author(s):  
Sureerut Amnuaypornsri ◽  
Jitladda Sakdapipanich ◽  
Shigeyuki Toki ◽  
Benjamin S. Hsiao ◽  
Naoya Ichikawa ◽  
...  

Abstract The effects of proteins and phospholipids in natural rubber (NR) on the strain-induced crystallization behavior during uniaxial deformation were studied by in-situ synchrotron wide-angle X-ray diffraction (WAXD) technique and simultaneous measurements of stress-strain relation. The influences of proteins and phospholipids in NR were evaluated separately by decomposition methods using deproteinization and lipase treatment, respectively. It was found that both components form a naturally occurring network, which is responsible for the strain-induced crystallizability of unvulcanized NR and the corresponding high mechanical property. This network also plays a significant role in strain-induced crystallization of vulcanized natural rubber.


2021 ◽  
pp. 179108
Author(s):  
Amin Raveshtian ◽  
Mohammad Fasihi ◽  
Reza Norouzbeigi ◽  
Sajad Rasouli

1987 ◽  
Vol 22 (10) ◽  
pp. 3470-3476 ◽  
Author(s):  
W. F. Reichert ◽  
M. K. Hopfenm�ller ◽  
D. G�ritz

Nanoscale ◽  
2020 ◽  
Vol 12 (48) ◽  
pp. 24527-24542
Author(s):  
Liang Chen ◽  
Lihui Wu ◽  
Lixian Song ◽  
Zhijie Xia ◽  
Yuanfei Lin ◽  
...  

The hierarchical structural evolution of natural rubber (NR) filled with different contents of nanoscale carbon black after first loading and recovering for different times.


Sign in / Sign up

Export Citation Format

Share Document