Fatigue crack propagation behavior in AISI 304 steel welded joints for cold‐stretched liquefied natural gas (LNG) storage tank at cryogenic temperatures

2019 ◽  
Vol 50 (5) ◽  
pp. 580-587
Author(s):  
I.K. Heo ◽  
D.H. Yoon ◽  
J.H. Kim ◽  
H.C. Kim ◽  
K.D. Kim