Influence of etching mode and composite resin type on bond strength to dentin using universal adhesive system

Author(s):  
Stefan Dačić ◽  
Milan Miljković ◽  
Aleksandar Mitić ◽  
Goran Radenković ◽  
Marija Anđelković‐Apostolović ◽  
...  
Author(s):  
João Victor Gonçalves da SILVA ◽  
Jonathas José de PAULO ◽  
Rodolfo Scavuzzi Carneiro da CUNHA ◽  
Rodivan BRAZ ◽  
Márcia de Almeida DURÃO

ABSTRACT Objective: To evaluate the bond strength of repairs with the self-adhering flowable composite Vertise Flow (Kerr) and a conventional composite resin Filtek Z350 (3M ESPE) subjected to different surface treatments. Methods: Forty specimens were divided into four groups: ZV (Filtek Z350 + Vertise Flow, without prior treatment); ZAV (Z350 + Vertise Flow with prior treatment with Single Bond Universal Adhesive System (3M ESPE)); ZAZ (Filtek Z350 + Filtek Z350 with prior treatment with Single Bond Universal Adhesive System (3M ESPE)); VV (Vertise Flow + Vertise Flow, without prior treatment). After 15 days of storage, the specimens were subjected to microtensile tests (Kratos IKCL3-USB, SP, Brazil), with speed of 0.5 mm/min and 20kg load. For statistical analysis, ANOVA with Tukey tests were used (p < 5%). Results: The mean values of the bond strength were highest respectively in the groups: ZV (36.07 ± 37.63); ZAZ (24.04 ± 28.51); VV (19.39 ± 28.24) and ZAV (16.06 ± 15.66). The bond strength of the repairs between the groups presented satisfactory results. Conclusion: The self-adhesive composite resin Vertise Flow seems to be a viable and fast alternative for composite resins repairs.


2018 ◽  
Vol 32 (4) ◽  
pp. 163
Author(s):  
Fábio Herrmann Coelho-de-Souza ◽  
Guilherme Fossá ◽  
Flávia Ávila Pereira ◽  
Celso Afonso Klein-Júnior ◽  
Maria Carolina Guilherme Erhardt ◽  
...  

OBJECTIVE: This study evaluated in vitro the shear bond strength of experimentally fractured human tooth fragments reattached with different adhesive materials and retentive techniques.METHODS: Forty-eight sound mandibular incisors were randomly divided into 6 groups (n=8). Their incisal edges were cut off in 5 groups, representing an enamel-dentin fracture. Intact teeth were used as control (Group 1). The fragment edges were reattached with adhesive system (Scotch Bond Multipurpose – 3M ESPE) (Group 2), adhesive system and composite resin (ICE – SDI) (Group 3), adhesive system and composite resin with circumferential bevel (Group 4), adhesive system and composite resin with internal dentin groove (Group 5), and adhesive system and composite resin with the circumferential bevel and internal dentin groove (Group 6). Shear bond strength was determined in a universal testing machine. Fracture modes were identified by light microscope. Kruskal-Wallis was used to analysis resistance to fracture and fracture patterns.RESULTS: The results showed statistically significant differences (p<0.05) among groups. The intact teeth (Group 1) showed higher fracture resistance than the other groups. Groups 2 and 6 did not differ and were statistically superior to other techniques. Group 4 presented statistically higher than in Group 5, which in turn was more resistant than Group 3.CONCLUSIONS: None of the fragment reattachment techniques was able to achieve the strength of sound teeth. Fragments reattached only with adhesive system or with adhesive system and composite resin with the circumferential bevel and internal dentin groove showed the best performance for resistance to fracture.


2020 ◽  
Vol 2020 ◽  
pp. 1-7
Author(s):  
Mariana Almeida Mello Proença ◽  
Karime Tavares Lima da Silva ◽  
Alisson Costa e Silva ◽  
Edilausson Moreno Carvalho ◽  
José Bauer ◽  
...  

Objectives. The aim of this study was to evaluate the shear bond strength of metal brackets bonded with different universal adhesive systems containing 10-MDP and Transbond Plus Self Etching Primer after 20,000 thermal cycles. Materials and Methods. A total of 130 sound bovine teeth were used, which are divided into 5 groups (n = 26) according to the adhesive system used: All-Bond Universal (Bisco), Ambar Universal (FGM), Clearfil Universal Bond (Kuraray), Single Bond Universal (3M/ESPE), and Transbond Plus SEP (3M/ESPE) as control. The adhesives were applied for 20 seconds and bonded with a resin Transbond XT (3M/ESPE). After this, the teeth were submitted to 20,000 cycles at 5°C and 55°C. Afterwards, the shear bond strength test was performed in a universal test machine (Instron 3342). The adhesive remnant index (ARI) was evaluated under a stereomicroscope at 10x magnification and scanning electronic microscopy (SEM, Hitachi 3030). The shear bond strength data were submitted to One-Way ANOVA (α = 0.05) and the ARI to the Kruskal–Wallis test (α = 0.05). Results. Statistical analysis showed that the universal adhesive systems presented mean shear bond strength values similar to Transbond Plus SEP (p<0.05). The universal adhesive presented similar ARI values among them but differed from those of Transbond Plus SEP (p<0.001). Transbond Plus SEP presented a high ARI value when compared with the universal adhesive systems and high demineralization of enamel. Conclusions. The results show that universal adhesive systems may be used for bonding metal brackets if the orthodontist wants to maintain dental enamel health.


2014 ◽  
Vol 30 ◽  
pp. e144
Author(s):  
C.P. Gré ◽  
M.A.C. Andrada ◽  
S. Monteiro Júnior ◽  
D.P. Lise ◽  
C. Deucher ◽  
...  

2005 ◽  
Vol 16 (2) ◽  
pp. 107-111 ◽  
Author(s):  
Eduardo Batista Franco ◽  
Lawrence Gonzaga Lopes ◽  
Paulo Henrique Perlatti D'Alpino ◽  
José Carlos Pereira

The purpose of this study was to investigate the effect of pH of different adhesive systems on the polymerization of a chemically cured composite resin (Adaptic - AD), by means of tensile bond strength testing. The adhesive systems tested were: ARM, Prime & Bond 2.1 (PB), Scotchbond Multi Purpose (SMP) and Single Bond (SB). Bond strength at the resin/adhesive system/resin interface was assessed. Five groups (n=5) were formed, according to following configuration: G1: AD/ARM/AD; G2: AD/PB/AD; G3: AD/SMP/AD; G4: AD/SB/AD; G5: AD/AD (no adhesive). A two-mold stainless steel matrix with a cone-shaped opening (1-mm-thick; 4 mm in diameter) was used to obtain resin discs. AD resin was inserted into the first mold, left-self curing and an adhesive layer was applied onto resin surface and light-cured. The second mold was assembled over the first and was filled with the resin. After 10 min, this setting was loaded in tension in a universal testing machine running at a crosshead speed of 0.5 mm/min. Data were submitted to one-way ANOVA and Tukey's test (p<0.05). Bond strength means (kgf) were: G1: 15.23 ± 4.1; G2: 0.00 ± 0.0; G3: 16.96 ± 2.4; G4: 10.08 ± 2.7; G5: 15.44 ± 0.9. There were statistically significant differences (p<0.05) between G2-G1; G2-G3; G2-G4; G4-G1; G4-G3. The systems with the lowest pHs (PB and SB) yielded the lowest bond strength. The findings of this in vitro study demostrates that the pH of adhesive systems influences the polymerization and bond strength of chemically cured resin materials. The low pH simplified adhesive systems showed distinct degrees of incompatibility with the chemically cured resin, when compared to the conventional adhesive systems.


2020 ◽  
Vol 11 (2) ◽  
pp. 37-40
Author(s):  
Gina Deborah Maia de Carvalho ◽  
Marianny Flexa Feitosa ◽  
Bruna Dantas Muniz ◽  
Lara Rabelo Aragão ◽  
Taira Endi de Flaviano Albuquerque ◽  
...  

2014 ◽  
Vol 13 (1) ◽  
pp. 7
Author(s):  
Dewi Puspitasari ◽  
Andi Soufyan ◽  
Ellyza Herda

Composite resin is a widely used aesthetic restoration. The restoration can fail due to secondary caries. Chlorhexidinegluconate 2% is used as a cavity disinfectant to eliminate microorganisms on the prepared cavity and to prevent thesecondary caries. The purpose of this study was to analyze the effect of chlorhexidine gluconate 2% to the bondstrength of composite resin with self etch system adhesive on dentine. Sixteen specimens of buccal dentine of premolarscrown are divided into 2 different groups. Group I: Clearfil SE Bond self-etch primer was applied for 20 seconds,Clearfil SE Bond bonding was applied for 5 seconds and polymerized for 10 seconds. Composite resin was constructedincrementally and polymerized for 20 seconds. Group II: prior to self etch primer application as in group I,chlorhexidine gluconate 2% was applied for 15 seconds. Shear bond strength was tested using Testing machine andanalyzed with unpaired T test. The highest shear bond strength was obtained by applying chlorhexidine gluconate 2%.The study concludes that chlorhexidine gluconate 2% application to dentine did not affect significantly to the bondstrength composite resin using self etch adhesive systems.


Sign in / Sign up

Export Citation Format

Share Document