Reliable Methods for Calculation of Average Film Thickness in a Vertical Thin-film Evaporator

1979 ◽  
Vol 51 (9) ◽  
pp. 905-905
Author(s):  
Dominique A. Taeymans
Materials ◽  
2021 ◽  
Vol 14 (16) ◽  
pp. 4681
Author(s):  
Dorian Minkov ◽  
Emilio Marquez ◽  
George Angelov ◽  
Gavril Gavrilov ◽  
Susana Ruano ◽  
...  

Three means are investigated for further increasing the accuracy of the characterization of a thin film on a substrate, from the transmittance spectrum T(λ) of the specimen, based on the envelope method. Firstly, it is demonstrated that the accuracy of characterization, of the average film thickness d¯ and the thickness non-uniformity ∆d over the illuminated area, increases, employing a simple dual transformation utilizing the product T(λ)xs(λ), where Tsm(λ) is the smoothed spectrum of T(λ) and xs(λ) is the substrate absorbance. Secondly, an approach is proposed for selecting an interval of wavelengths, so that using envelope points only from this interval provides the most accurate characterization of d¯ and ∆d, as this approach is applicable no matter whether the substrate is transparent or non-transparent. Thirdly, the refractive index n(λ) and the extinction coefficient k(λ) are computed, employing curve fitting by polynomials of the optimized degree of 1/λ, instead of by previously used either polynomial of the optimized degree of λ or a two-term exponential of λ. An algorithm is developed, applying these three means, and implemented, to characterize a-Si and As98Te2 thin films. Record high accuracy within 0.1% is achieved in the computation of d¯ and n(λ) of these films.


1993 ◽  
Vol 115 (1) ◽  
pp. 185-190 ◽  
Author(s):  
T. Makino ◽  
S. Morohoshi ◽  
S. Taniguchi

The flow factors for the average Reynolds equation introduced by Patir and Cheng (1978, 1979) are extended to be valid for thin film gas lubrication. The effects of molecular mean free-path on the roughness-induced flow factors are included on the assumption that the local compressibility is small. The derivation of flow factors is carried out by means of the perturbation approach developed by Tripp (1983). The results are expressed in terms of Knudsen number, Peklenik parameter and nondimensional film thickness defined as the ratio of average film thickness and standard deviation of composite roughness. Two-dimensional roughness effects on the load-carrying capacity of a gas lubricated finite slider are also investigated.


Carbon ◽  
2021 ◽  
Vol 178 ◽  
pp. 506-514
Author(s):  
Meiyu He ◽  
Jiayue Han ◽  
Xingwei Han ◽  
Jun Gou ◽  
Ming Yang ◽  
...  

Coatings ◽  
2020 ◽  
Vol 11 (1) ◽  
pp. 23
Author(s):  
Weiguang Zhang ◽  
Jijun Li ◽  
Yongming Xing ◽  
Xiaomeng Nie ◽  
Fengchao Lang ◽  
...  

SiO2 thin films are widely used in micro-electro-mechanical systems, integrated circuits and optical thin film devices. Tremendous efforts have been devoted to studying the preparation technology and optical properties of SiO2 thin films, but little attention has been paid to their mechanical properties. Herein, the surface morphology of the 500-nm-thick, 1000-nm-thick and 2000-nm-thick SiO2 thin films on the Si substrates was observed by atomic force microscopy. The hardnesses of the three SiO2 thin films with different thicknesses were investigated by nanoindentation technique, and the dependence of the hardness of the SiO2 thin film with its thickness was analyzed. The results showed that the average grain size of SiO2 thin film increased with increasing film thickness. For the three SiO2 thin films with different thicknesses, the same relative penetration depth range of ~0.4–0.5 existed, above which the intrinsic hardness without substrate influence can be determined. The average intrinsic hardness of the SiO2 thin film decreased with the increasing film thickness and average grain size, which showed the similar trend with the Hall-Petch type relationship.


2020 ◽  
Vol 102 (21) ◽  
Author(s):  
Stephan Geprägs ◽  
Björn Erik Skovdal ◽  
Monika Scheufele ◽  
Matthias Opel ◽  
Didier Wermeille ◽  
...  

Sensors ◽  
2021 ◽  
Vol 21 (12) ◽  
pp. 4056
Author(s):  
José Javier Imas ◽  
Carlos R. Zamarreño ◽  
Ignacio del Villar ◽  
Ignacio R. Matías

A fiber Bragg grating patterned on a SnO2 thin film deposited on the flat surface of a D-shaped polished optical fiber is studied in this work. The fabrication parameters of this structure were optimized to achieve a trade-off among reflected power, full width half maximum (FWHM), sensitivity to the surrounding refractive index (SRI), and figure of merit (FOM). In the first place, the influence of the thin film thickness, the cladding thickness between the core and the flat surface of the D-shaped fiber (neck), and the length of the D-shaped zone over the reflected power and the FWHM were assessed. Reflected peak powers in the range from −2 dB to −10 dB can be easily achieved with FWHM below 100 pm. In the second place, the sensitivity to the SRI, the FWHM, and the FOM were analyzed for variations of the SRI in the 1.33–1.4 range, the neck, and the thin-film thickness. The best sensitivities theoretically achieved for this device are next to 40 nm/RIU, while the best FOM has a value of 114 RIU−1.


2019 ◽  
Vol 682 ◽  
pp. 109-120 ◽  
Author(s):  
Wjatscheslaw Sakiew ◽  
Stefan Schrameyer ◽  
Marco Jupé ◽  
Philippe Schwerdtner ◽  
Nick Erhart ◽  
...  

2005 ◽  
Vol 297-300 ◽  
pp. 1446-1451 ◽  
Author(s):  
Takeshi Kasuya ◽  
Hideto Suzuki

The fatigue strength of TiAl intermetallic alloy coated with TiAlN film was studied in vacuum at 1073K using a SEM-servo testing machine. In addition, three kinds of TiAlN films were given by physical vapor deposition (1, 3, and 10μ m). The fatigue strength of 3μ m was highest. Also, the fatigue strength of 1μ m was lowest. From this result, existence of optimum film thickness was suggested because the difference of fatigue strength arose in each film thickness. The justification for existence of optimum film thickness is competition of 45-degree crack and 90-degree crack. The 45-degree crack is phenomenon seen in the thin film (1μ m), and is caused by plastic deformation of TiAl substrate. The 45-degree crack is the factor of the fatigue strength fall by the side of thin film. In contrast, the 90-degree crack is phenomenon in the thick film (10μ m), and is caused as result of reaction against load to film. The 90-degree crack is the factor of the fatigue strength fall by the side of thick film. In conclusion, the optimum film thickness can perform meso fracture control, and improves fatigue strength.